Pierre Schutz
Pierre Schutz has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Edgar Fernand Rauch
Univ. Grenoble Alpes, CNRS, Grenoble INP, SIMAP, 38000 Grenoble, France
1 shared publication - Frantz Martin
Université Paris-Saclay, CEA, Service de recherche en Corrosion et Comportement des Matériaux, 91191 Gif Sur Yvette, France
1 shared publication - Jamila Adem
Swiss Steel Group, Centre de Recherche d’Ugitech, 73400 Ugine, France
1 shared publication - Laurence Latu-Romain
SIMaP, Université Grenoble Alpes, Grenoble, France
1 shared publication - Quentin Auzoux
Université Paris-Saclay, CEA, Service de recherche en Corrosion et Comportement des Matériaux, 91191 Gif Sur Yvette, France
1 shared publication - Yves Wouters
Univ. Grenoble Alpes, CNRS, Grenoble INP, SIMAP, 38000 Grenoble, France
1 shared publication
Latest Publications
- Open Access
Hydrogen Embrittlement Characterization of 1.4614 and 1.4543 Martensitic Precipitation Hardened Stainless Steels
Hydrogen embrittlement (HE) of 1.4614 and 1.4543 maraging stainless steels is characterized with fine structural TEM-ASTAR, hydrogen electrochemical permeation, thermodesorption and tensile testing (with slow strain rate during H cathodic charging) experiments. Both solutions annealed and 550 °C aged states are studied. When aged, 1.4614 grade contains nanometric hexagonal Ni3Ti precipitates whereas 1.4543 grade contains three families of nanometric precipitates, namely, hexagonal Ni3Ti, non fcc-rich Cu and G-phase rich in Si, Ti and Ni with cube-cube relations with martensite. From the permeation and thermodesorption results, it appears that austenite and nanometric precipitates seem to constitute deep traps for hydrogen in both grades. From tensile tests with in situ H charging, 1.4614 and 1.4543 maraging grades show a high susceptibility to HE with relative reduction of area (RRA) strictly superior to 80% for both metallurgical states. The presence of retained austenite does not seem to bring any HE resistance because of its transformation into martensite during deformation.
Open AccessHydrogen Embrittlement Characterization of 1.4614 and 1.4543 Martensitic Precipitation Hardened Stainless Steels
Hydrogen embrittlement (HE) of 1.4614 and 1.4543 maraging stainless steels is characterized with fine structural TEM-ASTAR, hydrogen electrochemical permeation, thermodesorption and tensile testing (with slow strain rate during H cathodic charging) experiments. Both solutions annealed and 550 °C aged states are studied. When aged, 1.4614 grade contains nanometric hexagonal Ni3Ti precipitates whereas 1.4543 grade contains three families of nanometric precipitates, namely, hexagonal Ni3Ti, non fcc-rich Cu and G-phase rich in Si, Ti and Ni with cube-cube relations with martensite. From the permeation and thermodesorption results, it appears that austenite and nanometric precipitates seem to constitute deep traps for hydrogen in both grades. From tensile tests with in situ H charging, 1.4614 and 1.4543 maraging grades show a high susceptibility to HE with relative reduction of area (RRA) strictly superior to 80% for both metallurgical states. The presence of retained austenite does not seem to bring any HE resistance because of its transformation into martensite during deformation.