    Origin of Silicon-Rich Phases in Uranium Oxycarbide (UCO) Tri Structural ISOtropic (TRISO) Fuel Kernels: Fabrication-Driven Formation and Implications for Fuel Performance

    by Soroosh Hakimian, Shamim Pourrahimi, Samantha Michelle Gateman

    Prior post-irradiation studies reporting Si within UCO kernels in Tri-Structural Isotropic (TRISO) fuel have attributed its presence to migration from the SiC layer. However, TRISO kernel fabrication involves internal gelation in hot silicone oil followed by carbothermic reduction. Despite this, detailed chemical characterization of as-fabricated kernels remains limited. This work provides chemical characterization of as-fabricated UCO kernels, where Si-rich phases were identified in both bare kernels and coated TRISO kernels. This study outlines the significance of identifying Si-rich phases in as-fabricated kernels for understanding production-related contamination, quality control, and interpretation of post-discharge microstructural analyses.

  • Open Access

    Assessing the Potential for Galvanic Corrosion of TRISO Fuel

    by Sebastian A. Skaanvik, S. Pourrahimi, S. Hakimian, E. S. Alaei, S. M. Gateman, J. J. Noël

    TRi-structural ISOtropic (TRISO) particle fuel is an attractive advanced fuel type due to its improved fissionproduct retention and mechanical and thermal stability. Several investigations have confirmed the high performance of TRISO fuel under reactor operation and safety-testing conditions; however, the fuel’s degradation mechanisms and pathways under disposal repository conditions are poorly understood. Particularly underexplored is the possibility of galvanic corrosion of the uranium ceramic fuel kernel coupled to the significant amounts of graphite within the fuel layers and matrices. Herein, we report the first approach to evaluating galvanic corrosion of TRISO fuel by studying the macroscale electrochemical behaviour of UO2 and nuclear-grade graphite. The macroscale electrochemistry of nuclear-grade graphite was found to be somewhat complex, complicating electrochemical analysis; however, we show that glassy carbon is a reasonable proxy. Of the relevant radiolysis oxidants explored—O2, H2O2, NaClO, NaNO3, and NaNO2—only O2, H2O2, and NaClO may drive galvanic corrosion.

  • Open Access

    Investigating Size-Dependent Inclusion-Assisted Pitting Susceptibility using Scanning Electrochemical Cell Microscopy–Chronoamperometry

    by Liudmila Strelnikova, Emmanuel Mena-Morcillo, Soroosh Hakimian, Samantha Michelle Gateman

    Scanning electrochemical cell microscopy (SECCM) was employed to systematically investigate inclusion-induced localized corrosion with statistically meaningful spatial sampling. Using stainless steel 316-L (SS 316-L) as a model material, SECCM measurements were performed over both passive matrix regions and MnS inclusions, as identified by post-measurement microscopy. Analysis of potentiodynamic polarization curves acquired at inclusion sites with Tafel analysis yielded inconsistent results, highlighting limitations of conventional macroscale methods applied at the microscale for the passive system. Instead, a distinct breakdown potential feature, observed exclusively at inclusion sites, proved to be a more informative parameter extracted from the polarization data. To evaluate the stability of localized anodic activity at varying sizes of inclusions (~0.2 – 3 µm2), chronoamperometric measurements were conducted. The magnitude of anodic currents was directly correlated to the probed inclusion areas (areas of inclusions or inclusion parts enclosed in an SECCM footprint), showing a linear direct relationship. This study provides statistically grounded new insight into how inclusion size governs the persistence of localized anodic activity of passive metals, advancing prior macroscale observations and limited single-inclusion analyses into a robust microscale understanding. Furthermore, the presented SECCM – chronoamperometry workflow enabled high-resolution electrochemical investigations without limitations of Tafel theory at the microscale and could potentially be extended to study other passive materials with high inclusion densities.

  • Open Access

    Effect of gap size on flange face corrosion

    by Soroosh Hakimian, Abdel‐Hakim Bouzid, Lucas A. Hof

    Bolted flanged joints play a critical role in offshore wind turbine tower structures, serving as integral components that connect various sections of the tower. This research study employs electrochemical techniques to investigate the effect of gap dimensions, which determine the crevice gap thickness and crevice depth, on corrosion behavior of 321 stainless steel flange sample plates in a 3.5 wt% NaCl solution at 50°C. Gaskets are used in this study to create gaps between two flange surfaces. A novel fixture is utilized to simulate the applied stress on the gasket, fluid flow within the fixture, and the geometric aspects of the gasket and flange. The findings reveal that increasing the gap thickness from 1.58 to 6.35 mm results in a rise in the general corrosion rate of the flange surface from 0.09 to 1.03 mm y−1, and crevice corrosion initiation time increases from 0.23 to 3.12 h. Furthermore, reducing the crevice depth (d) from 7.49 to 0 mm leads to a decrease in the general corrosion rate from 0.09 mm y−1 to 0.04 µm y−1, and cases with d = 3.81 and d = 0 mm show no observable crevice corrosion after potentiostatic tests.