  • Joint Metallothermic Reduction of Titanium and Rare Refractory Metals of Group V

    by V. F. Balakirev, T. V. Osinkina, S. A. Krasikov, E. M. Zhilina, L. B. Vedmid’, S. V. Zhidovinova

    The features of phase formation during the joint aluminothermic reduction of titanium, niobium, tantalum, and vanadium from their oxides are studied using


  • Effect of Yttrium on the Structural-Phase State of the In Situ Mo–15.3 V–10.5 Si Composite

    by A. V. Larionov, K. V. Pikulin, S. V. Zhidovinova, L. Yu. Udoeva

    By means of X-ray phase analysis and energy-dispersive X-ray analysis, the effect of yttrium on the structural-phase state of the hypoeutectic Mo–15.3 V–10.5 Si alloy is investigated. It is established that the main phases of the Мо–(15.4–14.3) V–(10.6–9.8) Si–(0.3–5.3) Y alloys obtained under the conditions of nonequilibrium solidification are the (Mo1 – xVx)ss metal solid solution (matrix), (Mo1 – xVx)3Si silicide solid solution, and Y5Si3 silicide. In alloys doped with yttrium up to 1.0 at %, the space between dendrites of the (Mo1 – xVx)ss metal phase is filled with the (Mo1 – xVx)3Si solid solution, and at the boundaries of the metal solid solution, Y5Si3 is located. At the yttrium concentration of alloys higher than 3.0 at %, space between the (Mo1 – xVx)ss dendrites is filled with Y5Si3 silicide, inside which (Mo1 – xVx)3Si grains are formed. No ternary and quaternary yttrium-containing compounds are detected. The elemental composition of phases of the Мо–(15.4–14.3) V–(10.6–9.8) Si–(0.3–5.3) Y alloys is almost identical and is characterized by silicon nonstoichiometry. The silicon content of the (Mo1 – xVx)ss and (Mo1 – xVx)3Si phases lies within the accepted limits of the homogeneity region, and the silicon concentration of Y5Si3 (≈35.4 at %) goes beyond the defined limits. Doping the Мо–15.3 V–10.5 Si alloy with yttrium increases the degree of dispersion of the structure. Particles of the main structural constituents become close in size. At the same time, the volumetric ratio of the metal phase to the silicide phase increases as the yttrium content of the alloys is raised. The density of the alloys varies within 8.7 and 9.0 g/cm3.