Xinpeng Cui
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Xinpeng Cui has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Haocheng Yang
MOE Key Laboratory of High Performance Polymer Materials and Technology, School of Chemistry and Chemical Engineering, Nanjing University, Nanjing 210023, China
4 shared publications - Hongfeng Xie
MOE Key Laboratory of High Performance Polymer Materials and Technology, School of Chemistry and Chemical Engineering, Nanjing University, Nanjing 210023, China
4 shared publications - Jun Cai
Public Instrument Center, School of Chemistry and Chemical Engineering, Nanjing University, Nanjing 210023, China
4 shared publications - Junsheng Zhang
MOE Key Laboratory of High Performance Polymer Materials and Technology, School of Chemistry and Chemical Engineering, Nanjing University, Nanjing 210023, China
4 shared publications - Zhonghua Xi
Experimental Chemistry Teaching Center, School of Chemistry and Chemical Engineering, Nanjing University, Nanjing 210023, China
3 shared publications - Chengwei Wu
MOE Key Laboratory of High Performance Polymer Materials and Technology, School of Chemistry and Chemical Engineering, Nanjing University, Nanjing 210023, China
2 shared publications
Latest Publications
- Open Access
Dispersed and Co-Continuous Morphologies of Epoxy Asphalt Bond Coats and Their Effects on Mechanical Performance
The co-continuous microstructure represents an ideal configuration for polymer-modified asphalts. Consequently, determining the optimum polymer content hinges on establishing this critical network between polymer and bitumen. In this study, epoxy asphalt bond coats (EABCs) exhibiting three distinct morphologies (epoxy-dispersed, co-continuous, and bitumen-dispersed) were prepared. Phase structure evolution and the final cured morphology were analyzed using a laser scanning confocal microscope (LSCM). Rotational viscosity–time characteristics, tensile properties, single-lap shear strength, and pull-off adhesion strength were characterized using various techniques. Results indicated that the viscosity of EABCs at the late stage of the curing reaction increased with increasing epoxy resin (ER) concentration, whereas the time required for EABCs to reach a viscosity of 5 Pa·s decreased. LSCM analysis revealed that EABCs exhibited three distinct morphologies dependent on ER concentration: (1) a bitumen-continuous morphology with dispersed epoxy domains (41–42 vol.% ER) formed via a nucleation and growth mechanism; (2) a co-continuous structure (43–45 vol.% ER); and (3) an epoxy-continuous structure with dispersed bitumen domains (46 vol.% ER). Furthermore, the EABC with 42 vol.% exhibited a transitional morphology between bitumen-continuous and co-continuous structures. A significant improvement in mechanical properties occurred during the transition from the bitumen-continuous (41 vol.% ER) to the co-continuous morphology (43 vol.% ER): tensile strength, elongation at break, and toughness increased by 524%, 1298%, and 2732%, respectively. Simultaneously, pull-off adhesion strength and single-lap shear strength rose by 61% and 99%, respectively. In contrast, mechanical properties increased only gradually during the co-continuous phase and the subsequent transition to an epoxy-continuous morphology (45–46 vol.% ER). Considering cost, rotational viscosity–time dependence, and mechanical performance, an ER concentration of 43 vol.% (within the co-continuous region) is optimal for EABC production.
Open AccessDispersed and Co-Continuous Morphologies of Epoxy Asphalt Bond Coats and Their Effects on Mechanical Performance
The co-continuous microstructure represents an ideal configuration for polymer-modified asphalts. Consequently, determining the optimum polymer content hinges on establishing this critical network between polymer and bitumen. In this study, epoxy asphalt bond coats (EABCs) exhibiting three distinct morphologies (epoxy-dispersed, co-continuous, and bitumen-dispersed) were prepared. Phase structure evolution and the final cured morphology were analyzed using a laser scanning confocal microscope (LSCM). Rotational viscosity–time characteristics, tensile properties, single-lap shear strength, and pull-off adhesion strength were characterized using various techniques. Results indicated that the viscosity of EABCs at the late stage of the curing reaction increased with increasing epoxy resin (ER) concentration, whereas the time required for EABCs to reach a viscosity of 5 Pa·s decreased. LSCM analysis revealed that EABCs exhibited three distinct morphologies dependent on ER concentration: (1) a bitumen-continuous morphology with dispersed epoxy domains (41–42 vol.% ER) formed via a nucleation and growth mechanism; (2) a co-continuous structure (43–45 vol.% ER); and (3) an epoxy-continuous structure with dispersed bitumen domains (46 vol.% ER). Furthermore, the EABC with 42 vol.% exhibited a transitional morphology between bitumen-continuous and co-continuous structures. A significant improvement in mechanical properties occurred during the transition from the bitumen-continuous (41 vol.% ER) to the co-continuous morphology (43 vol.% ER): tensile strength, elongation at break, and toughness increased by 524%, 1298%, and 2732%, respectively. Simultaneously, pull-off adhesion strength and single-lap shear strength rose by 61% and 99%, respectively. In contrast, mechanical properties increased only gradually during the co-continuous phase and the subsequent transition to an epoxy-continuous morphology (45–46 vol.% ER). Considering cost, rotational viscosity–time dependence, and mechanical performance, an ER concentration of 43 vol.% (within the co-continuous region) is optimal for EABC production.
- Open Access
Viscosity, Morphology, and Thermomechanical Performance of Attapulgite-Reinforced Bio-Based Polyurethane Asphalt Composites
Bio-based polyurethane asphalt binder (PUAB) derived from castor oil (CO) is environmentally friendly and exhibits extended allowable construction time. However, CO imparts inherently poor mechanical performance to bio-based PUAB. To address this limitation, attapulgite (ATT) with fibrous nanostructures was incorporated. The effects of ATT on bio-based PUAB were systematically investigated, including cure kinetics, rotational viscosity (RV) evolution, phase-separation microstructures, dynamic mechanical properties, thermal stability, and mechanical performance. Experimental characterization employed Fourier transform infrared spectroscopy, Brookfield viscometry, laser scanning confocal microscopy, dynamic mechanical analysis, thermogravimetry, and tensile testing. ATT incorporation accelerated the polyaddition reaction conversion between isocyanate groups in polyurethane (PU) and hydroxyl groups in ATT. Paradoxically, it reduced RV during curing, prolonging allowable construction time proportionally with clay content. Additionally, ATT’s compatibilizing effect decreased bitumen particle size in PUAB, with scaling proportionally with clay loading. While enhancing thermal stability, ATT lowered the glass transition temperature and damping properties. Crucially, 1 wt% ATT increased tensile strength by 71% and toughness by 62%, while maintaining high elongation at break (>400%). The cost-effectiveness and significant reinforcement capability of ATT make it a promising candidate for producing high-performance bio-based PUAB composites.
Open AccessViscosity, Morphology, and Thermomechanical Performance of Attapulgite-Reinforced Bio-Based Polyurethane Asphalt Composites
Bio-based polyurethane asphalt binder (PUAB) derived from castor oil (CO) is environmentally friendly and exhibits extended allowable construction time. However, CO imparts inherently poor mechanical performance to bio-based PUAB. To address this limitation, attapulgite (ATT) with fibrous nanostructures was incorporated. The effects of ATT on bio-based PUAB were systematically investigated, including cure kinetics, rotational viscosity (RV) evolution, phase-separation microstructures, dynamic mechanical properties, thermal stability, and mechanical performance. Experimental characterization employed Fourier transform infrared spectroscopy, Brookfield viscometry, laser scanning confocal microscopy, dynamic mechanical analysis, thermogravimetry, and tensile testing. ATT incorporation accelerated the polyaddition reaction conversion between isocyanate groups in polyurethane (PU) and hydroxyl groups in ATT. Paradoxically, it reduced RV during curing, prolonging allowable construction time proportionally with clay content. Additionally, ATT’s compatibilizing effect decreased bitumen particle size in PUAB, with scaling proportionally with clay loading. While enhancing thermal stability, ATT lowered the glass transition temperature and damping properties. Crucially, 1 wt% ATT increased tensile strength by 71% and toughness by 62%, while maintaining high elongation at break (>400%). The cost-effectiveness and significant reinforcement capability of ATT make it a promising candidate for producing high-performance bio-based PUAB composites.
- Open Access
Thermo-Mechanical Properties and Phase-Separated Morphology of Warm-Mix Epoxy Asphalt Binders with Different Epoxy Resin Concentrations
The performance and phase-separated microstructures of epoxy asphalt binders greatly depend on the concentration of epoxy resin or bitumen. In this paper, the effect of the epoxy resin (ER) concentration (10–90%) on the viscosity, thermo-mechanical properties, and phase-separated morphology of warm-mix epoxy asphalt binders (WEABs) was investigated using the Brookfield rotational viscometer, differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA) and laser scanning confocal microscopy (LSCM). Due to the high reactivity of epoxy resin, the viscosity of WEABs increases with time. Furthermore, the initial viscosity of WEABs decreases with the ER concentration. Depending on the ER concentration, the viscosity–time behavior of WEABs is divided into three stages: slow (10–40%), fast (50–80%), and extremely slow (90%). In the slow stage, the viscosity slightly increases with the ER concentration, while the fast stage shows an opposite trend. DSC and DMA results reveal that WEABs with 10–80% ER exhibit two glass transition temperatures (Tgs) for cured epoxy resin and bitumen. Moreover, the Tgs of epoxy resin and bitumen increase with the ER concentration. However, WEAB with 90 % ER has only one Tg. LSCM observation shows that phase separation occurs in all WEABs. For WEABs containing 10–40% ER, spherical epoxy particles act as the discontinuous phase and disperse in the continuous bitumen phase. However, in WEABs with 50–90% ER, phase inversion takes place. Contrarily, bitumen particles disperse in the continuous epoxy phase. The damping properties of WEABs with the continuous epoxy phases increase with the ER concentration, while the crosslinking density shows an opposite trend. The occurrence of phase inversion results in a sharp increase in the tensile strength of WEABs. For WEABs with the continuous epoxy phases, the elongation at break increases with the ER concentration. The toughness first increases and then decreases with the ER concentration. A maximum toughness value shows at 70% ER.
Open AccessThermo-Mechanical Properties and Phase-Separated Morphology of Warm-Mix Epoxy Asphalt Binders with Different Epoxy Resin Concentrations
The performance and phase-separated microstructures of epoxy asphalt binders greatly depend on the concentration of epoxy resin or bitumen. In this paper, the effect of the epoxy resin (ER) concentration (10–90%) on the viscosity, thermo-mechanical properties, and phase-separated morphology of warm-mix epoxy asphalt binders (WEABs) was investigated using the Brookfield rotational viscometer, differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA) and laser scanning confocal microscopy (LSCM). Due to the high reactivity of epoxy resin, the viscosity of WEABs increases with time. Furthermore, the initial viscosity of WEABs decreases with the ER concentration. Depending on the ER concentration, the viscosity–time behavior of WEABs is divided into three stages: slow (10–40%), fast (50–80%), and extremely slow (90%). In the slow stage, the viscosity slightly increases with the ER concentration, while the fast stage shows an opposite trend. DSC and DMA results reveal that WEABs with 10–80% ER exhibit two glass transition temperatures (Tgs) for cured epoxy resin and bitumen. Moreover, the Tgs of epoxy resin and bitumen increase with the ER concentration. However, WEAB with 90 % ER has only one Tg. LSCM observation shows that phase separation occurs in all WEABs. For WEABs containing 10–40% ER, spherical epoxy particles act as the discontinuous phase and disperse in the continuous bitumen phase. However, in WEABs with 50–90% ER, phase inversion takes place. Contrarily, bitumen particles disperse in the continuous epoxy phase. The damping properties of WEABs with the continuous epoxy phases increase with the ER concentration, while the crosslinking density shows an opposite trend. The occurrence of phase inversion results in a sharp increase in the tensile strength of WEABs. For WEABs with the continuous epoxy phases, the elongation at break increases with the ER concentration. The toughness first increases and then decreases with the ER concentration. A maximum toughness value shows at 70% ER.
- Open Access
Performance and Morphology of Waterborne Polyurethane Asphalt in the Vicinity of Phase Inversion
Waterborne polyurethane asphalt emulsion (WPUA) is an environmentally friendly bituminous material, whose performance is highly dependent on the phase structure of the continuous phase. In this paper, WPUAs in the vicinity of phase inversion were prepared using waterborne polyurethane (WPU) and asphalt emulsion. The chemical structures, thermal stability, dynamic mechanical properties, phase-separated morphology and mechanical performance of WPUAs were studied. Fourier-transform infrared (FTIR) spectra revealed that there are no –NCO bonds in either the pure WPU or WPUAs. Moreover, the preparation of WPUA is a physical process. The addition of WPU weakens the thermal stability of asphalt emulsion. WPU improves the storage modulus of asphalt emulsion at lower and higher temperatures. The glass transition temperatures of the WPUA films are higher than that of the pure WPU film. When the WPU concentration increases from 30 wt% to 40 wt%, phase inversion occurs; that is, the continuous phase shifts from asphalt to WPU. The WPUA films have lower tensile strength and toughness than the pure WPU film. However, the elongations at break of the WPUA films are higher than that of the pure WPU film. Both the tensile strength and toughness of the WPUA films increase with the WPU concentration. Due to the occurrence of phase inversion, the elongation at break, tensile strength and toughness of the WPUA film containing 30 wt% WPU are increased by 29%, 250% and 369%, respectively, compared to the film with 40 wt% WPU.
Open AccessPerformance and Morphology of Waterborne Polyurethane Asphalt in the Vicinity of Phase Inversion
Waterborne polyurethane asphalt emulsion (WPUA) is an environmentally friendly bituminous material, whose performance is highly dependent on the phase structure of the continuous phase. In this paper, WPUAs in the vicinity of phase inversion were prepared using waterborne polyurethane (WPU) and asphalt emulsion. The chemical structures, thermal stability, dynamic mechanical properties, phase-separated morphology and mechanical performance of WPUAs were studied. Fourier-transform infrared (FTIR) spectra revealed that there are no –NCO bonds in either the pure WPU or WPUAs. Moreover, the preparation of WPUA is a physical process. The addition of WPU weakens the thermal stability of asphalt emulsion. WPU improves the storage modulus of asphalt emulsion at lower and higher temperatures. The glass transition temperatures of the WPUA films are higher than that of the pure WPU film. When the WPU concentration increases from 30 wt% to 40 wt%, phase inversion occurs; that is, the continuous phase shifts from asphalt to WPU. The WPUA films have lower tensile strength and toughness than the pure WPU film. However, the elongations at break of the WPUA films are higher than that of the pure WPU film. Both the tensile strength and toughness of the WPUA films increase with the WPU concentration. Due to the occurrence of phase inversion, the elongation at break, tensile strength and toughness of the WPUA film containing 30 wt% WPU are increased by 29%, 250% and 369%, respectively, compared to the film with 40 wt% WPU.