Tihao Cao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Tihao Cao has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Qing Huang
YongJiang Laboratory
2 shared publications - Quanxing Ren
Zhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications, Ningbo Key Laboratory of Special Energy Materials and Chemistry, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China
2 shared publications - Yinsheng Li
Zhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications, Ningbo Key Laboratory of Special Energy Materials and Chemistry, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China
2 shared publications - Zhengren Huang
Zhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications, Ningbo Key Laboratory of Special Energy Materials and Chemistry, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China
2 shared publications - Haifeng Nie
College of Materials Science and Engineering, China Jiliang University, Hangzhou 310018, China
1 shared publication - Haifeng Nie
Zhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications, Ningbo Key Laboratory of Special Energy Materials and Chemistry, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China
1 shared publication
Latest Publications
- Open Access
Hydrothermal Corrosion Resistance of Reaction-Bonded SiC Ceramic: Synergistic Enhancement by Homogeneous MoSi2 Distribution and Residual Silicon Reduction
Reaction-bonded SiC (RBSC) ceramics exhibit limited hydrothermal corrosion resistance due to the presence of residual silicon. This study presents a strategy to enhance the corrosion resistance of RBSC through homogeneous incorporation of MoSi2 and concurrent reduction in residual silicon content. Three material systems were fabricated via reactive melt infiltration: conventional RBSC with a SiC/C preform (SC), a SiC–MoSi2 composite incorporating commercial Mo2C powder via physical mixing (MC), and a SiC–MoSi2 composite derived from a Mo2C/C precursor synthesized by a molten salt method (MS). The Mo2C/C composite synthesized at 1150 °C exhibited fine, uniformly distributed Mo2C particles coated on carbon black, contrasting with the agglomerated distribution in commercial Mo2C mixtures. During reactive sintering at 1600 °C, Mo2C reacted with molten Si to form MoSi2, reducing residual Si content. Sample MS achieved the lowest residual Si (8.77 ± 0.45 vol.%), followed by MC (12.43 ± 0.86 vol.%) and SC (19.17 ± 1.01 vol.%). All samples achieved near-full densification (open porosity < 0.1%), with bulk densities of 2.96 ± 0.05, 3.03 ± 0.03, and 3.07 ± 0.03 g/cm3 for SC, MC, and MS, respectively. Microstructurally, MS displayed homogeneous MoSi2 dispersion, while MC showed partial MoSi2 aggregation, and SC contained continuous residual Si regions. Hydrothermal corrosion tests at 345 °C and 15 MPa for 9 days demonstrated that corrosion resistance followed the order MS > MC > SC. After 9 days, weight loss was 22.3970 ± 1.2059 mg/cm2 (SC), 17.6370 ± 0.8266 mg/cm2 (MC), and 15.4347 ± 0.7807 mg/cm2 (MS), with corrosion depths of 393.17 ± 27.46, 267.40 ± 24.44, and 224.60 ± 25.13 μm, respectively. The enhanced performance of MS arises from two synergistic factors: reduced residual Si minimizes large corrosion pores, while uniform distribution of MoSi2 facilitates the formation of a stable, dissolution-resistant composite oxide layer composed of MoO3 and SiO2, in which MoO3 restrains excessive dissolution of SiO2 through a pinning effect. These findings demonstrate that combining residual Si reduction with homogeneous MoSi2 incorporation via molten salt-synthesized precursors offers an effective strategy for improving hydrothermal corrosion resistance of reaction-bonded SiC-based materials for applications in high-temperature and high-pressure aqueous environments such as nuclear water reactors.
Open AccessHydrothermal Corrosion Resistance of Reaction-Bonded SiC Ceramic: Synergistic Enhancement by Homogeneous MoSi2 Distribution and Residual Silicon Reduction
Reaction-bonded SiC (RBSC) ceramics exhibit limited hydrothermal corrosion resistance due to the presence of residual silicon. This study presents a strategy to enhance the corrosion resistance of RBSC through homogeneous incorporation of MoSi2 and concurrent reduction in residual silicon content. Three material systems were fabricated via reactive melt infiltration: conventional RBSC with a SiC/C preform (SC), a SiC–MoSi2 composite incorporating commercial Mo2C powder via physical mixing (MC), and a SiC–MoSi2 composite derived from a Mo2C/C precursor synthesized by a molten salt method (MS). The Mo2C/C composite synthesized at 1150 °C exhibited fine, uniformly distributed Mo2C particles coated on carbon black, contrasting with the agglomerated distribution in commercial Mo2C mixtures. During reactive sintering at 1600 °C, Mo2C reacted with molten Si to form MoSi2, reducing residual Si content. Sample MS achieved the lowest residual Si (8.77 ± 0.45 vol.%), followed by MC (12.43 ± 0.86 vol.%) and SC (19.17 ± 1.01 vol.%). All samples achieved near-full densification (open porosity < 0.1%), with bulk densities of 2.96 ± 0.05, 3.03 ± 0.03, and 3.07 ± 0.03 g/cm3 for SC, MC, and MS, respectively. Microstructurally, MS displayed homogeneous MoSi2 dispersion, while MC showed partial MoSi2 aggregation, and SC contained continuous residual Si regions. Hydrothermal corrosion tests at 345 °C and 15 MPa for 9 days demonstrated that corrosion resistance followed the order MS > MC > SC. After 9 days, weight loss was 22.3970 ± 1.2059 mg/cm2 (SC), 17.6370 ± 0.8266 mg/cm2 (MC), and 15.4347 ± 0.7807 mg/cm2 (MS), with corrosion depths of 393.17 ± 27.46, 267.40 ± 24.44, and 224.60 ± 25.13 μm, respectively. The enhanced performance of MS arises from two synergistic factors: reduced residual Si minimizes large corrosion pores, while uniform distribution of MoSi2 facilitates the formation of a stable, dissolution-resistant composite oxide layer composed of MoO3 and SiO2, in which MoO3 restrains excessive dissolution of SiO2 through a pinning effect. These findings demonstrate that combining residual Si reduction with homogeneous MoSi2 incorporation via molten salt-synthesized precursors offers an effective strategy for improving hydrothermal corrosion resistance of reaction-bonded SiC-based materials for applications in high-temperature and high-pressure aqueous environments such as nuclear water reactors.
- Open Access
Effects of Preformed Composition and Pore Size on Microstructure and Properties of SiCf/SiC Composites via Reactive Melt Infiltration
This study investigated the influence of preformed composition and pore size on the microstructure and properties of SiCf/SiC composites fabricated via reactive melt infiltration (RMI). The process began with the impregnation of SiC fiber cloth with phenolic resin, followed by lamination and pyrolysis. Subsequent steps included further impregnations with phenolic resin, SiC slurry, and carbon black slurry, each followed by additional pyrolysis. This process resulted in three types of preforms, designated as PP, PS, and PC. These preforms exhibited a multimodal distribution of pore size, with peak pore diameters around 5 μm for PP, ranging from 200 nm to 4 μm for PS, and approximately 150 nm for PC. The preforms were then subjected to molten silicon infiltration at 1600 °C under vacuum for 1 h to create SiCf/SiC composites. The PP preform contained only pyrolytic carbon, leading to a composite with high closed porosity and unreacted carbon, resulting in poor mechanical properties. The PS preform, which was impregnated with SiC particles, displayed an optimized pore size distribution but retained significant amounts of residual silicon and carbon in the final composite. In contrast, the PC preform featured both an ideal pore size distribution and an adequate amount of carbon, achieving high density and low porosity with reduced residual phases in the final composite. This optimization led to a flexural strength of 152.4 ± 15.4 MPa, an elastic modulus of about 181.1 ± 0.1 GPa, and a thermal conductivity of 27.7 W/mK in the SiCf/SiC composites product. These findings underscore the importance of preform optimization in enhancing the performance of SiCf/SiC composites, potentially paving the way for more reliable nuclear fuel cladding solutions.
Open AccessEffects of Preformed Composition and Pore Size on Microstructure and Properties of SiCf/SiC Composites via Reactive Melt Infiltration
This study investigated the influence of preformed composition and pore size on the microstructure and properties of SiCf/SiC composites fabricated via reactive melt infiltration (RMI). The process began with the impregnation of SiC fiber cloth with phenolic resin, followed by lamination and pyrolysis. Subsequent steps included further impregnations with phenolic resin, SiC slurry, and carbon black slurry, each followed by additional pyrolysis. This process resulted in three types of preforms, designated as PP, PS, and PC. These preforms exhibited a multimodal distribution of pore size, with peak pore diameters around 5 μm for PP, ranging from 200 nm to 4 μm for PS, and approximately 150 nm for PC. The preforms were then subjected to molten silicon infiltration at 1600 °C under vacuum for 1 h to create SiCf/SiC composites. The PP preform contained only pyrolytic carbon, leading to a composite with high closed porosity and unreacted carbon, resulting in poor mechanical properties. The PS preform, which was impregnated with SiC particles, displayed an optimized pore size distribution but retained significant amounts of residual silicon and carbon in the final composite. In contrast, the PC preform featured both an ideal pore size distribution and an adequate amount of carbon, achieving high density and low porosity with reduced residual phases in the final composite. This optimization led to a flexural strength of 152.4 ± 15.4 MPa, an elastic modulus of about 181.1 ± 0.1 GPa, and a thermal conductivity of 27.7 W/mK in the SiCf/SiC composites product. These findings underscore the importance of preform optimization in enhancing the performance of SiCf/SiC composites, potentially paving the way for more reliable nuclear fuel cladding solutions.