Y.K. Jee
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Y.K. Jee has a total of 2 co-authors. Here are the top co-authors by number of shared publications:
Jin Yu
Department of Material Science and Engineering, Korea Advanced Institute of Science and Engineering, Yuseong-gu, Daejeon 305-701, Korea
2 shared publicationsY.H. Ko
Samsung Electronics, Hwasung-city, Gyeongii-do 445-701, Korea
2 shared publications
Latest Publications
- 1 October 2007
- Published by Springer Nature in Journal of Materials Research
- Vol. 22 (10) , 2776-2784
Effects of Zn addition on the drop reliability of Sn–3.5Ag–xZn/Ni(P) solder joints
Varying amounts of Zn (1, 3, 7 wt%) were added to Sn–3.5Ag solder on the electroless Ni(P)/immersion Au metallization, and solder joint microstructures after reflow and isothermal aging (500 h at 150 °C) were investigated using scanning electron microscopy, energy dispersive x-ray spectroscopy, transmission electron microscopy, and x-ray diffraction, which were subsequently correlated to the microhardness and drop test results. Zinc in the solder affected the solder joint intermetallic compounds profoundly, which improved the drop reliability significantly. The effect of Zn was to nucleate Ni5Zn21and to suppress the formation of Ni3P, Ni3SnP, and Ni3Sn4, which were known to increase the propensity for brittle cracking. Drop test results showed an inverse correlation between the number of drops-to-failure (Nf) and the thickness of Ni3P layer. As the growth of the Ni3P layer was suppressed by Zn, drop reliability increased substantially.
- 1 October 2007
- Published by Springer Nature in Journal of Materials Research
- Vol. 22 (10) , 2776-2784
Effects of Zn addition on the drop reliability of Sn–3.5Ag–xZn/Ni(P) solder joints
Varying amounts of Zn (1, 3, 7 wt%) were added to Sn–3.5Ag solder on the electroless Ni(P)/immersion Au metallization, and solder joint microstructures after reflow and isothermal aging (500 h at 150 °C) were investigated using scanning electron microscopy, energy dispersive x-ray spectroscopy, transmission electron microscopy, and x-ray diffraction, which were subsequently correlated to the microhardness and drop test results. Zinc in the solder affected the solder joint intermetallic compounds profoundly, which improved the drop reliability significantly. The effect of Zn was to nucleate Ni5Zn21and to suppress the formation of Ni3P, Ni3SnP, and Ni3Sn4, which were known to increase the propensity for brittle cracking. Drop test results showed an inverse correlation between the number of drops-to-failure (Nf) and the thickness of Ni3P layer. As the growth of the Ni3P layer was suppressed by Zn, drop reliability increased substantially.
- 1 July 2007
- Published by Springer Nature in Journal of Materials Research
- Vol. 22 (7) , 1879-1887
Effect of Zn on the intermetallics formation and reliability of Sn-3.5Ag solder on a Cu pad
Varying amounts of Zn (1, 3, and 7 wt%) were added to Sn–3.5Ag solder on a Cu pad, and the resultant solder joint microstructures after a reflow and isothermal aging (150 °C, up to 500 h) were investigated using scanning electron microscopy, energy dispersive x-ray, and x-ray diffraction, which were subsequently correlated to the results of microhardness and drop tests. Zinc was effective in improving the drop resistance of Sn–3.5Ag solder on the Cu pad, and an addition of 3 wt% Zn nearly doubled the number of drops-to-failure (Nf). The beneficial role of Zn was ascribed to suppression of Cu6Sn5and precipitation of Zn-containing intermetallic compounds (IMCs). However, the Zn effect was reduced as Cu6Sn5and Ag3Sn precipitated in a joint IMC layer after prolonged aging. The interface between Ag5Zn8and Cu5Zn8was resistant to drop impact, but two other layered IMC structures of Cu6Sn5/Cu3Sn and Cu5Zn8/Cu6Sn5were not.
- 1 July 2007
- Published by Springer Nature in Journal of Materials Research
- Vol. 22 (7) , 1879-1887
Effect of Zn on the intermetallics formation and reliability of Sn-3.5Ag solder on a Cu pad
Varying amounts of Zn (1, 3, and 7 wt%) were added to Sn–3.5Ag solder on a Cu pad, and the resultant solder joint microstructures after a reflow and isothermal aging (150 °C, up to 500 h) were investigated using scanning electron microscopy, energy dispersive x-ray, and x-ray diffraction, which were subsequently correlated to the results of microhardness and drop tests. Zinc was effective in improving the drop resistance of Sn–3.5Ag solder on the Cu pad, and an addition of 3 wt% Zn nearly doubled the number of drops-to-failure (Nf). The beneficial role of Zn was ascribed to suppression of Cu6Sn5and precipitation of Zn-containing intermetallic compounds (IMCs). However, the Zn effect was reduced as Cu6Sn5and Ag3Sn precipitated in a joint IMC layer after prolonged aging. The interface between Ag5Zn8and Cu5Zn8was resistant to drop impact, but two other layered IMC structures of Cu6Sn5/Cu3Sn and Cu5Zn8/Cu6Sn5were not.