Santosh Kumar Sahoo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Santosh Kumar Sahoo has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- S. Narayana Jammalamadaka
Magnetic Materials and Device Physics Laboratory, Department of Physics, Indian Institute of Technology Hyderabad, Hyderabad, India
3 shared publications Akash Mohapatra
2 shared publications- Apoorva Kaul
Nanomaterials Research Laboratory, Surface Engineering Division, CSIR - National Aerospace Laboratories, Bangalore 560 017, India
1 shared publication - Arup Biswas
Atomic and Molecular Physics Division, Bhabha Atomic Research Centre 4 , Mumbai 400085
1 shared publication Asghar Husain
1 shared publication- Asghar Husain
IIT Hyderabad
1 shared publication
Latest Publications
- 20 November 2026
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1087
Disorder-induced stripe domains ‐ Coupled magnetic and charge transport in Fe2CoAl thin film
- 20 November 2026
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1087
Disorder-induced stripe domains ‐ Coupled magnetic and charge transport in Fe2CoAl thin film
- 25 August 2026
- Published by IOP Publishing in Journal of Physics D: Applied Physics
- Vol. 59 (34) , 345001
Annealing-driven perpendicular magnetic anisotropy in Fe 2 CoSi thin films: correlating domain imaging, FORC, and minor loops
Achieving strong perpendicular magnetic anisotropy (PMA) in Heusler alloys is highly beneficial for developing efficient and scalable spintronic devices. Here, we demonstrate the onset of PMA and its enhancement in Fe 2 CoSi thin films through post-deposition annealing. X-ray diffraction confirms the A2 disordered phase. Williamson–Hall analysis reveals an increase in average crystallite size from ∼1.7–10.7 nm with annealing. Indeed, there is a reduction in lattice strain from 28.8 × 10 −3 (room temperature (RT)) to 4.6 × 10 −3 (film annealed at 550 °C), which indicates improved structural order. Enhanced structural order is confirmed with selective area electron diffraction. Magnetic measurements demonstrate an increase in coercivity (from ∼23 to ∼137 Oe) and saturation magnetization (from ∼1185 to ∼1407 emu cc −1 ) with annealing from RT to 550 °C, respectively. First-order reversal curve analysis shows a clear evolution from a compact single-domain state to a broadened multi-domain state. The enhanced full width at half maximum of switching-field distribution, minor-loop parameters ( W F 0 , W R 0 ), and appearance of stripe-like domains in magnetic force microscopy images further confirm the onset of PMA and its development. These findings infer that thermal annealing is an effective route to engineer anisotropy in Fe 2 CoSi thin films for spintronic applications.
- 25 August 2026
- Published by IOP Publishing in Journal of Physics D: Applied Physics
- Vol. 59 (34) , 345001
Annealing-driven perpendicular magnetic anisotropy in Fe 2 CoSi thin films: correlating domain imaging, FORC, and minor loops
Achieving strong perpendicular magnetic anisotropy (PMA) in Heusler alloys is highly beneficial for developing efficient and scalable spintronic devices. Here, we demonstrate the onset of PMA and its enhancement in Fe 2 CoSi thin films through post-deposition annealing. X-ray diffraction confirms the A2 disordered phase. Williamson–Hall analysis reveals an increase in average crystallite size from ∼1.7–10.7 nm with annealing. Indeed, there is a reduction in lattice strain from 28.8 × 10 −3 (room temperature (RT)) to 4.6 × 10 −3 (film annealed at 550 °C), which indicates improved structural order. Enhanced structural order is confirmed with selective area electron diffraction. Magnetic measurements demonstrate an increase in coercivity (from ∼23 to ∼137 Oe) and saturation magnetization (from ∼1185 to ∼1407 emu cc −1 ) with annealing from RT to 550 °C, respectively. First-order reversal curve analysis shows a clear evolution from a compact single-domain state to a broadened multi-domain state. The enhanced full width at half maximum of switching-field distribution, minor-loop parameters ( W F 0 , W R 0 ), and appearance of stripe-like domains in magnetic force microscopy images further confirm the onset of PMA and its development. These findings infer that thermal annealing is an effective route to engineer anisotropy in Fe 2 CoSi thin films for spintronic applications.
- Open Access
- 12 August 2025
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 138 (6)
Ultra-soft magnetic properties in Ta/NiFe laminated system
An integrated magnetic flux concentrator (MFC) has become a choice for enhancing the sensitivity of a magnetic field sensor. However, the flux concentrator’s geometry and its ultra-soft magnetic properties are the key ingredients for successful implementation to improve the detectability of a magnetic sensor. In this report, the laminated stack of Ta/Ru/[NiFe(tNiFe)/Ta(tTa)]N/Ta of thickness 0.5 μm was investigated, where tNiFe, tTa, and N were varied to optimize ultra-soft magnetic properties of the film and compared them with the bulk NiFe film. Structural investigations revealed that incorporating an ultra-thin layer of Ta in the laminated stack suppresses the grain growth of the NiFe phase and improves the textured growth of the fcc(111) phase of the NiFe alloy. This results in dramatic improvement of the measured magnetic hysteresis loop of the laminated stack with a reduced coercivity field in the range of 0.4 ± 0.1 Oe, high linearity, and low saturation field (<10 Oe) while comparing them with the bulk film of NiFe of equivalent thicknesses. The laminated stack thickness of up to 4 μm was further investigated, and the bilinear M(H) loop was explained through antiferromagnetic (AFM) interlayer coupling between successive NiFe layers.
- 12 August 2025
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 138 (6)
Open AccessUltra-soft magnetic properties in Ta/NiFe laminated system
An integrated magnetic flux concentrator (MFC) has become a choice for enhancing the sensitivity of a magnetic field sensor. However, the flux concentrator’s geometry and its ultra-soft magnetic properties are the key ingredients for successful implementation to improve the detectability of a magnetic sensor. In this report, the laminated stack of Ta/Ru/[NiFe(tNiFe)/Ta(tTa)]N/Ta of thickness 0.5 μm was investigated, where tNiFe, tTa, and N were varied to optimize ultra-soft magnetic properties of the film and compared them with the bulk NiFe film. Structural investigations revealed that incorporating an ultra-thin layer of Ta in the laminated stack suppresses the grain growth of the NiFe phase and improves the textured growth of the fcc(111) phase of the NiFe alloy. This results in dramatic improvement of the measured magnetic hysteresis loop of the laminated stack with a reduced coercivity field in the range of 0.4 ± 0.1 Oe, high linearity, and low saturation field (<10 Oe) while comparing them with the bulk film of NiFe of equivalent thicknesses. The laminated stack thickness of up to 4 μm was further investigated, and the bilinear M(H) loop was explained through antiferromagnetic (AFM) interlayer coupling between successive NiFe layers.