Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Ahmed Nabil Elalem has a total of 7 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Application and Adaptation of Arc-Based Welding Processes to Wire Arc Additive Manufacturing: A Review

    by Ahmed Nabil Elalem, Husam Alrehaili, Mohammad Azad Alam, Sufian Raja, Azim Uddin

    Wire Arc Additive Manufacturing (WAAM) has emerged as one of the most industrially scalable arc-based metal additive manufacturing (AM) technologies, using established Gas Metal Arc Welding (GMAW), Gas Tungsten Arc Welding (GTAW), and Plasma Arc Welding (PAW) processes to deposit metallic material layer-by-layer into near-net-shape components. This review presents a physics-based examination of the adaptation of traditional welding processes for AM applications, with emphasis on: (i) the thermodynamic and metallurgical principles governing melt pool formation, solidification, and solid-state transformations; (ii) the thermal and solidification features that WAAM shares with multi-pass welding and those that are distinctive to WAAM, with particular attention to the temperature gradient-to-solidification-rate ratio (G/R) and its role in controlling grain morphology; (iii) deposition path strategies and their influence on heat distribution and microstructural homogeneity; (iv) arc metal transfer modes and their thermal implications for AM; and (v) mechanisms of defect formation including porosity, solidification cracking, residual stress, and geometric deviation. Unlike general WAAM reviews, this article specifically positions conventional arc welding processes as the metallurgical and thermal foundation of WAAM and critically examines how their operating principles are transformed under repeated layer-by-layer deposition. Key governing equations linking process parameters to microstructure and properties are presented. Among GMAW variants, Cold Metal Transfer (CMT) provides low heat input, controlled droplet transfer, and low spatter, whereas GTAW and PAW allow wire feed and arc power to be set independently; the preferred process therefore depends on the alloy, required deposition rate, geometry, and surface quality. A synthesis of findings across ferrous and non-ferrous alloy systems is presented, together with knowledge gaps and future directions toward closed-loop adaptive WAAM systems.

  • Open Access

    Hot Deformation Behavior of AA6061-T6 Aluminum Alloy: Flow Stress, Constitutive Modeling, and Microstructural Evolution

    by Ahmed Nabil Elalem, Husam Alrehaili, Xin Wu

    AA6061-T6 undergoes work hardening, dynamic recovery, and progressive flow softening during hot torsion, yet a systematic single-campaign dataset with quantified experimental uncertainty is absent from the literature. Gleeble hot torsion tests were conducted at eleven conditions from 250 to 450 °C and 0.91 to 9.07 s−1. With the stress multiplier fixed a priori at α = 0.045 MPa−1 from compression literature on this alloy, a two-stage calibration determined the remaining Garofalo–Arrhenius constants: the temperature-slope stage anchors Q = 151.1 kJ mol−1 (consistent with Al lattice self-diffusion), and a global Zener–Hollomon regression conditional on Q yields n = 1.371 and A = 3.51 × 1010 s−1; a fully simultaneous three-parameter fit is shown to be practically unidentifiable on the three-level matrix. Training AARE = 15.5% (R = 0.908); leave-one-out cross-validation gives AARE = 23.0%, bounding the predictive uncertainty. The Prasad instability map identifies 400–450 °C at 0.91–2.72 s−1 as the optimal hot-forming window; flow instability is predicted at 350 °C (outright at 2.72 and 9.07 s−1, with the 0.91 s−1 condition at the map boundary), and macroscopic fracture was observed in all three specimens tested there. Optical microscopy in specimen T1 (εeq = 3.69) shows elongated subgrains at the gauge center and fine-grained zones near the fracture surface consistent with localized geometric dynamic recrystallization. The activation energy, smooth post-peak softening, and subgrain wall morphology identify dynamic recovery as the likely dominant restoration mechanism. Adiabatic heating and a 24% peak-stress repeatability scatter at the single repeated condition (450 °C, 9.07 s−1) are quantified and propagated into the constitutive model uncertainty bounds. Because the training-to-cross-validation error gap (15.5% versus 23.0% AARE) reflects the limited three-level strain-rate matrix, the calibrated equation is recommended for interpolation within the tested window of 300 to 450 °C and 0.91 to 9.07 s−1 (noting that 300 °C was tested only at 0.91 s−1, so higher-rate predictions at that temperature are extrapolations) and for forming-window identification, not for extrapolation beyond this domain without additional validation data.


  • Open Access

    Effect of Active Air-Cooling Configuration During Interlayer Friction Stir Processing on Grain Morphology and Within-Wall Homogeneity in UAMFSP-Fabricated Aluminum 4043 Walls: A Single-Replicate Exploratory Study

    by Ahmed Nabil Elalem, Husam Alrehaili, Xin Wu

    The Unified Additive-Deformation Manufacturing Process (UAMFSP) integrates MIG-based Wire Arc Additive Manufacturing (WAAM) with interlayer Friction Stir Processing (FSP) on a single CNC platform, applying severe plastic deformation to each deposited layer. The novelty of this work is the first controlled comparison, to the authors’ knowledge, of the spatial position of forced-air cooling applied concurrently with the FSP traverse in such an integrated platform: cooling was directed at the top bead surface (TC), at the bottom substrate (BC), or at both surfaces simultaneously (DC), with a MIG-only wall serving as the baseline. Single-layer, four-bead ER4043 aluminum walls were deposited on AA6061 substrates, and optical micrographs from three within-bead locations per condition were quantified with ImageJ, yielding 2038 to 2723 grains per condition. A lumped-parameter thermal model calibrated to infrared thermography ranked the comparative cooling rates as NC < TC < BC < DC. The principal finding is grain homogenization: every FSP condition reduced the grain area scatter by 55 to 71 percent relative to MIG-only, eliminating the coarse-grain tail of the as-deposited distribution regardless of cooling position. Mean equivalent diameters of all four conditions lie within 0.5 µm of one another, at the resolution limit of the optical measurement, so the mean-size ordering (DC finest, 2.76 µm) is reported as a ranking rather than as net refinement. Vickers microhardness on the MIG-only and uncooled FSP walls revealed a 27 HV within-wall gradient (86 ± 7 HV at the stir-zone center versus 59 ± 2 HV at the bead edge), which motivates bilateral cooling for thermal-field homogenization. Because the design is single-replicate, between-condition differences are presented as hypotheses for replicate study with EBSD and spatially resolved hardness mapping.

  • Open Access

    Post-Peak Cooling Rate Is Strongly Associated with Layer-Resolved Porosity Evolution in Hybrid WAAM–FSP Al 4043 Multi-Layer Walls

    by Ahmed Nabil Elalem, Mahmood Razzaghi, Xin Wu

    In hybrid wire arc additive manufacturing with interlayer friction stir processing (UAMFSP), refined microstructures are produced in aluminum alloy builds; however, the thermal parameters governing layer-resolved defect evolution remain poorly understood. In this study, a correlative mechanistic framework is presented in which post-peak cooling rate is identified as a plausible controlling factor for porosity evolution in UAMFSP Al 4043 three-layer walls. A multi-scale characterization is performed by employing infrared thermography, quantitative optical grain morphology analysis (N = 10,346 grains, Layers 1–3), scanning electron microscopy from 250× to 35,000×, and image-based porosity quantification from calibrated SEM fields. This primary quantitative comparison is established between L1 and L3 only; Layer 2 is excluded from the 250× quantitative analysis owing to its thermally distinct cooling regime and is treated separately. A counterintuitive layer-dependent porosity gradient is reported, wherein the upper layer (L3) exhibited 80% higher porosity (2.90 ± 1.18%) and 107% higher pore density (4283 ± 900 pores/mm2) than the bottom layer (L1), despite recording a 26% lower peak FSP surface temperature (195.1 vs. 263.2 °C) (n = three fields per layer; Cohen’s d ≈ 1.7). Based on these results, the post-peak cooling rate, rather than peak temperature, is identified as a plausible controlling factor for void consolidation quality, as evidenced by the observation that L3 cools at −12.3 °C/s versus −16.2 °C/s for L1, which is consistent with prolonged high-temperature dwell and reduced plastic-flow-assisted pore closure in the upper layer. The anomalously rapid cooling of L2 (−46.9 °C/s), attributed to a bilateral thermal gradient between the substrate and the air-cooled free surface, places it in a thermally distinct regime; accordingly, L2 is utilized exclusively for high-magnification SEM characterization in this study. High-magnification SEM imaging (12,000×–35,000×) revealed a frequent spatial co-location of sub-micron pores with fragmented Al–Si eutectic particles, which is consistent with preferential void persistence near particle–matrix interfaces. Grain morphology also exhibits non-monotonic evolution with build height, with mean circularity following the order L3 (0.645) > L1 (0.621) > L2 (0.569), and the equiaxed grain fraction ranging from 25.5% (L2) to 36.1% (L3) (ANOVA: F = 56.2, p = 5.15 × 10−25), while the mean equivalent grain diameter remained below 3.4 μm across all layers. Overall, the outcomes of this study establish post-peak cooling rate, rather than peak temperature, as a plausible controlling factor for void consolidation quality in UAMFSP builds, with the caveat that complete causal isolation requires controlled single-variable experiments. These outcomes are presented as a first mechanistic framework for this class of hybrid process and are intended to motivate targeted controlled experiments, subsurface thermal characterization, and expanded porosity sampling in future investigations of multi-layer additive–deformation manufacturing of Al-based alloys.

  • Open Access

    Layer-Resolved Grain Morphology and Recrystallized Crystal Evolution in FSP-Assisted Wire Arc Additive Manufacturing of Aluminum Alloy 4043

    by Ahmed Nabil Elalem, Xin Wu

    Wire arc additive manufacturing of aluminum generates coarse, anisotropic solidification microstructures that limit mechanical performance, and interlayer friction stir processing (FSP) is increasingly applied to refine them. This study reports the layer-resolved grain morphology and the recrystallized crystal evolution in MIG + FSP-fabricated aluminum alloy 4043 walls, pairing the FSP spindle torque recorded from the CNC controller with multi-descriptor grain morphology in a coupling that, to the authors’ knowledge, has not been previously reported in the WAAM + FSP literature. Methodologically, two four-bead, three-layer walls were co-fabricated under identical deposition conditions on a HAAS VF-3 CNC platform, one by MIG deposition alone and one by the complete MIG + FSP route; the FSP spindle torque was measured at three positions per layer (118 ± 6 N·m at 600 RPM for L1, and 19.1 ± 1.0 and 26.6 ± 1.3 N·m at 1200 RPM for L2 and L3), and quantitative image analysis of 10,091 grains provided the layer-resolved mean grain area, equivalent diameter, aspect ratio, perimeter-to-area ratio, and circularity. The results show that the mean grain area increased from 8.55 μm2 (L1) to 12.96 μm2 (L3) while the aspect ratio decreased monotonically (1.389 to 1.323), indicating progressive grain equiaxiality with build height; the P/A ratio followed a non-monotonic layer dependence (2.54 to 2.11 to 2.50 μm−1), with the L2 minimum consistent with reduced boundary line density under the combined thermal influence of two adjacent FSP events. The MIG + FSP route produced grain areas 29–48× smaller per layer than the MIG wall and a 45.8% higher hardness (75.8 ± 7.7 versus 52.0 ± 1.3 HV; n = 6; p = 0.0027). In conclusion, the L3 torque exceeds the L2 torque at equal 1200 RPM, qualitatively consistent with the d−p term in the grain-size-explicit creep framework γ. = C·(τn/dp)·exp(−Q/RT), although temperature, strain rate, and grain size cannot be fully decoupled from the present three-layer dataset. The morphology and the distributional evidence are consistent with dynamic recrystallization (DRX); discrimination between continuous and discontinuous DRX requires EBSD.

  • Open Access

    Hybrid Additive Manufacturing via Wire Arc Metal Deposition and Deformation for Microstructure Refinement and Performance Enhancement: A Review

    by Ahmed Nabil Elalem, Xin Wu

    Wire Arc Additive Manufacturing (WAAM) is a cost-effective and scalable technique for producing large metallic components; however, coarse columnar microstructures, strong crystallographic texture, and significant residual stresses limit its widespread adoption. Hybrid WAAM processes that integrate deformation-based techniques have been developed to address these limitations. This review provides an analysis of deformation-assisted WAAM, covering interlayer rolling, friction stir processing (FSP), machine hammer peening, laser shock peening, and ultrasonic-vibration-assisted techniques. These hybrid techniques introduce additional thermomechanical parameters (strain, strain rate, and applied stress) that significantly influence microstructure evolution. The governing physical metallurgy mechanisms are discussed in detail, including dislocation accumulation, recovery, static and dynamic recrystallization, and severe plastic deformation. Studies from 2022 to 2025 are critically reviewed, highlighting the effectiveness of hybrid WAAM in promoting columnar-to-equiaxed grain transformation, reducing anisotropy, mitigating defects, and improving mechanical properties across aluminum, titanium, steels, and nickel-based alloys. The integration of auxiliary processes such as in situ machining and heat treatment is also discussed. This review establishes a process–structure–property framework for hybrid WAAM and provides guidance for the development of advanced additive manufacturing systems for the production of near-net-shape components, with reported yield-strength gains of 20–40%, elongation gains of 10–30%, and fatigue-life improvements of up to 60% relative to as-built WAAM.


  • Open Access

    Post-Peak Cooling Rate Controls Porosity Evolution in Hybrid WAAM–FSP Al 4043 Multi-Layer Walls

    by Ahmed Nabil Elalem, Mahmood Razzaghi, Xin Wu

    In hybrid Wire Arc Additive Manufacturing with interlayer Friction Stir Processing (UAMFSP), refined microstructures are produced in aluminum alloy builds; however, the thermal parameters governing layer-resolved defect evolution remain poorly understood. In this study, a first mechanistic framework is presented, identifying post-peak cooling rate as a governing parameter for porosity evolution in UAMFSP Al 4043 three-layer walls. In this study, a comprehensive multi-scale characterization of three-layer Al 4043 UAMFSP walls is presented, employing infrared thermography, quantitative optical grain morphology analysis (N = 10,346 grains, Layers 1–3), scanning electron microscopy from 250× to 35,000×, and image-based porosity quantification from calibrated SEM fields. A counterintuitive layer-dependent porosity gradient is reported, wherein the upper layer (L3) exhibited 80% higher porosity (2.90 ± 1.18%) and 107% higher pore density (4,283 ± 900 pores/mm²) than the bottom layer (L1), despite recording a 26% lower peak FSP surface temperature (195.1 vs. 263.2°C) (n = 3 fields per layer; Cohen’s d ≈1.7). Based on these results, the post-peak cooling rate, rather than peak temperature, is identified as a dominant controlling parameter for void consolidation quality, as evidenced by the observation that L3 cools at −12.3 °C/s versus −16.2 °C/s for L1, which is consistent with prolonged high-temperature dwell and reduced plastic-flow-assisted pore closure in the upper layer. It should be noted that the anomalously rapid cooling of L2 (−46.9 °C/s), attributed to a bilateral thermal gradient between the substrate and the air-cooled free surface, places it in a thermally distinct regime; accordingly, L2 is utilized exclusively for high-magnification SEM characterization in this study. High-magnification SEM imaging (12,000×–35,000×) revealed a frequent spatial co-location of sub-micron pores with fragmented Al–Si eutectic particles, which is consistent with preferential void persistence near particle–matrix interfaces. Furthermore, grain morphology exhibited evolve non-monotonically with build height, with mean circularity following the order L3 (0.645) > L1 (0.621) > L2 (0.569), and the equiaxed grain fraction ranging from 25.5% (L2) to 36.1% (L3) (ANOVA: F = 56.2, p = 5.15 × 10⁻²⁵), while the mean equivalent grain diameter remained below 3.4 μm across all layers. In summary, the outcomes of this study establish post-peak cooling rate, rather than peak temperature, as a governing parameter for void consolidation quality in UAMFSP builds. These outcomes are presented as a first mechanistic framework for this class of hybrid process, and are intended to motivate targeted controlled experiments, subsurface thermal characterization, and expanded porosity sampling in future investigations of multi-layer additive–deformation manufacturing of Al-based alloys.


  • Open Access

    Hybrid Additive Manufacturing via Wire Arc Metal Deposition and Deformation for Microstructure Refinement and Performance Enhancement

    by Ahmed Nabil Elalem, Xin Wu

    Wire Arc Additive Manufacturing (WAAM) is a cost-effective and scalable technique for producing large metallic components; however, coarse columnar microstructures, strong crystallographic texture, and significant residual stresses limit its widespread adoption. In recent years, hybrid WAAM processes integrating deformation-based techniques have been developed to address these limitations. This review provides a comprehensive analysis of deformation-assisted WAAM, encompassing interlayer rolling, friction stir processing (FSP), hammer peening, laser shock peening, and ultrasonic vibration-assisted approaches. These hybrid techniques introduce additional thermomechanical parameters—strain, strain rate, and applied stress—that significantly influence microstructure evolution. The governing physical metallurgy mechanisms are discussed in detail, including dislocation accumulation, recovery, static and dynamic recrystallization, and severe plastic deformation. Studies from 2022 to 2025 are critically reviewed, highlighting the effectiveness of hybrid WAAM in promoting columnar-to-equiaxed grain transformation, reducing anisotropy, mitigating defects, and improving mechanical properties across aluminum, titanium, steels, and nickel-based alloys. The integration of auxiliary processes such as in-situ machining and heat treatment is also discussed. This review establishes a process-structure-property framework for hybrid WAAM and provides guidance for the development of advanced additive manufacturing systems capable of delivering near-net-shape components with microstructures and properties approaching those of wrought or forged counterparts.


  • Open Access

    Process–Microstructure–Property Characteristics of Aluminum Walls Fabricated by Hybrid Wire Arc Additive Manufacturing with Friction Stir Processing

    by Ahmed Nabil Elalem, Xin Wu

    Wire Arc Additive Manufacturing (WAAM) is a cost-effective method for fabricating large aluminum components; however, it tends to suffer from heat accumulation and coarse anisotropic microstructures, which can limit the part’s performance. In this study, a wall is fabricated using a hybrid unified additive deformation manufacturing process (UAMFSP) method, which integrates friction stir processing (FSP) into WAAM, and is compared with a Metal Inert Gas (MIG)-based WAAM wall. Infrared (IR) thermography revealed progressive heat buildup in MIG walls, with peak layer temperatures of about 870 to 1000 °C. In contrast, in the UAMFSP process, heat was redistributed through mechanical stirring, maintaining more uniform sub-solidus profiles below approximately 400 °C. Also, optical microscopy and quantitative image analysis showed that MIG walls developed coarse, dendritic grains with a mean grain area of about 314 µm2, whereas the UAMFSP produced refined, equiaxed grains with a mean grain area of about 10.9 µm2. Microhardness measurement (Vickers HV0.2, 200 gf) confirmed that the UAMFSP process can improve the hardness by 45.8% compared to the MIG process (75.8 ± 7.7 HV vs. 52.0 ± 1.3 HV; p = 0.0027). In summary, the outcomes of this study introduce the UAMFSP process as a method for addressing the thermal and microstructural limitations of WAAM. These findings provide a framework for further extending hybrid additive–deformation strategies to thicker builds, alternative alloys, and service-relevant mechanical evaluations.