SZSa Zhao

Sa Zhao

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Sa Zhao has a total of 7 co-authors. Here are the top co-authors by number of shared publications:

  • Chi Zhang

    Key Laboratory for Advanced Materials of Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing, China

    1 shared publication
  • Guang Li

    Metals and Chemistry Research Institute, China Academy of Railway Sciences Corporation Limited, Beijing 100081, China

    1 shared publication
  • Guanzhen Zhang

    Metals and Chemistry Research Institute, China Academy of Railway Sciences Corporation Limited, Beijing 100081, China

    1 shared publication
  • Mingzhe Fan

    Metals and Chemistry Research Institute, China Academy of Railway Sciences Corporation Limited, Beijing 100081, China

    1 shared publication
  • Xiang Li

    Metals and Chemistry Research Institute, China Academy of Railway Sciences Corporation Limited, Beijing 100081, China

    1 shared publication
  • Yuming Fu

    Key Laboratory of Advanced Materials of Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing 100084, China

    1 shared publication

Latest Publications

  • Open Access

    Microstructural Evolution of Pearlitic Wheel Steel Under Thermal–Mechanical Fatigue

    by Mingzhe Fan, Yuming Fu, Guang Li, Xiang Li, Sa Zhao, Zhifeng Li, Guanzhen Zhang, Chi Zhang

    Pearlitic wheel steel subjected to thermal–mechanical fatigue (TMF) during braking can undergo catastrophic fracture. This study clarifies the microstructural evolution governing the macroscopic cyclic hardening/softening behavior of pearlitic wheel steel under thermal–mechanical fatigue (TMF) with a constant mechanical strain range of −0.4% to +0.2%. At lower temperature amplitudes (200–500 °C), the geometrically necessary dislocation (GND) density reaches 20.4 × 1014/m2 during initial cycles, corresponding to cyclic hardening due to dislocation pile-ups at cementite lamellae interfaces. With increasing cycles, the GND density decreases to 12.3 × 1014/m2, concurrent with softening arising from lamellar bending/fracture, partial spheroidization, and dynamic recrystallization of ferrite. At higher temperature amplitudes (200–730 °C), the GND density decreases from 8.8 × 1014/m2 to 3.5 × 1014/m2, reflecting sustained cyclic softening dominated by thermally activated mechanisms, including cementite spheroidization and dislocation annihilation. The resulting softened microstructure consists of ferrite grains, intragranular dispersed cementite, and chain-like coarse cementite at boundaries. Unlike previous studies that focused on single loading conditions (e.g., thermal fatigue, rolling contact fatigue, or wear), the present work addresses the more complex TMF scenario and quantitatively elucidates the interplay between mechanical response and microstructural evolution in pearlitic steel. This work provides theoretical guidance for the development of a fatigue life prediction model for pearlitic wheels under braking.