Effect of Surface Treatments on the Repair Bond Strength Between Aged Glass Ceramics and Composite Resin: An In Vitro Study
Open Access
- 24 August 2026
- journal article
- Published by Selcuk Dental Journal in Selcuk Dental Journal
- Vol. 13 (2) , 184-190
Abstract
Background: This study aimed to investigate the effects of glass bead particle abrasion and different primer systems on the repair bond strength of two types of aged glass ceramics and composite resins. Methods: Eighty specimens were prepared from leucite-reinforced (G-Ceram) and lithium disilicate (IPS e.max CAD) glass-ceramic materials. After thermocycling (5–55 °C, 30 s dwell time, 5000 cycles), each ceramic specimen was divided into five test groups (n=8): control (C), air abrasion with 50-µm glass beads (GB), 37% phosphoric acid etching, Clearfil Ceramic Primer Plus application (CP), Monobond Etch&Prime (MEP) application, 4.8% hydrofluoric acid etching, and Monobond N (MN) application. All specimens were coated with a universal adhesive (Nova Compo B Plus) following treatment. Clearfil Majesty Esthetic, a nanohybrid composite resin, was applied. The specimens were kept in distilled water at 37 °C for 24 h and evaluated for the shear bond strength (1 mm/min). Data were statistically analyzed using two-way ANOVA, Tukey HSD and Bonferroni post-hoc tests (α=0.05).Results: Surface treatment and its interaction with the ceramic material exhibited a statistically significant effect on the repair bond strength (P < 0.05), whereas the main effect of the ceramic type was not significant (P > 0.05). The C and GB groups demonstrated significantly lower mean bond strength values than the CP, MEP, and MN groups (P < 0.05). For the lithium disilicate ceramics, both the CP and MN groups produced the highest bond strengths, with no significant difference between them (P > 0.05). In the leucite-reinforced ceramics, the MN group showed significantly higher bond strength than the CP (P < 0.05). Although the overall effect of surface treatment was consistent across ceramic types, in the CP group, lithium disilicate specimens exhibited a higher bond strength than leucite-reinforced ceramics (P < 0.05).Conclusions: Both phosphoric acid and hydrofluoric acid etching followed by different primer applications achieved the highest bond strength for lithium disilicate ceramics, whereas silane-based treatment after hydrofluoric acid etching was the most effective for leucite-reinforced ceramics. Overall, the tested primers significantly enhanced the bonding to aged glass-ceramics, supporting their use in repair procedures.Keywords
This publication has 38 references indexed in Scilit:
- Repair bond strength of resin composite to CAD/CAM glass-ceramic: Influence of cleaning methods, surface treatments, and agingJournal of Dentistry, 2025
- The effects of different silicatization and silanization protocols on the bond durability of resin cements to new high-translucent zirconiaClinical Oral Investigations, 2021
- Repair bond strength and surface topography of resin‐ceramic and ceramic restorative blocks treated by laser and conventional surface treatmentsMicroscopy Research and Technique, 2020
- Physicochemical and morphological characterization of a glass ceramic treated with different ceramic primers and post-silanization protocolsDental Materials, 2019
- Effectiveness of pre-silanization in improving bond performance of universal adhesives or self-adhesive resin cements to silica-based ceramics: Chemical and in vitro evidencesDental Materials, 2019
- Self-etching ceramic primer versus hydrofluoric acid etching: Etching efficacy and bonding performanceJournal of Prosthodontic Research, 2018
- Effectiveness and stability of silane coupling agent incorporated in ‘universal’ adhesivesDental Materials, 2016
- An in vitro comparison of four intra-oral ceramic repair systemsJournal of Dentistry, 2012
- Possible hazardous effects of hydrofluoric acid and recommendations for treatment approach: a reviewClinical Oral Investigations, 2011
- Effect of sandblasting, grinding, polishing and glazing on the flexural strength of two pressable all-ceramic dental materialsJournal of Dentistry, 2004