Abstract
Heat-set threaded inserts provide a practical solution for reusable, load-bearing joints in FDM-printed polymer parts; however, their pull-out performance is governed not only by the insert itself, but also by the surrounding printed architecture. This study examines the pull-out behavior of heat-set M3 inserts embedded in FDM-printed PLA specimens across three wall thicknesses (1.28 mm, 1.6 mm, and 1.92 mm) and three infill patterns (adaptive cubic, cross-zag, and gyroid) using a repeatable drill-stand-based insertion fixture and a two-stage embedding protocol at 190 °C. Across 27 specimens, mean peak pull-out force ranged from 1353.6 ± 7.5 N to 1551.5 ± 20.4 N. Two-way ANOVA showed that both wall thickness and infill pattern significantly affected peak force, although the wall-thickness effect was practically modest—a 20% increase in material yielded only a 4.6% increase in mean force. Cross-zag specimens failed at significantly lower loads than adaptive cubic and gyroid, which performed comparably. Two specimens (7.4%) failed prematurely because of defective insert threads rather than the printed structure, underlining the importance of fastener quality control.

This publication has 13 references indexed in Scilit: