Mechanism Characterization and Nondestructive Inspection Method of Thermal Degradation Faults in EPDM Cable Termination
- 25 April 2022
- journal article
- research article
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Instrumentation and Measurement
- Vol. 71 (00189456) , 1-12
Abstract
There is a significant positive proportional correlation between the condition of ethylene propylene diene monomer (EPDM) insulation and partial discharge (PD) characteristics in electric multiple units (EMUs) cable termination. Especially for the cable terminations with long service life, the aging effect of EPDM insulation material is significant due to long-term high-current load. In this article, electrical deterioration and PD development of EPDM insulation under long-term thermal degradation is conducted. During the test process, the phase-resolved PD (PRPD) analysis, PD inception voltage (PDIV), physicochemical properties, and flashover voltage of EPDM samples with different thermal degradation are measured. The relationship between the thermal degradation extent of EPDM insulation and PD characteristics is also proposed. The results show that electrical deterioration of the aged sample can be divided into four gradations by PD amplitude and pulse repetition rate. In the four gradations, the shape of the PRPD spectrum in every gradation changes significantly with different thermal degradations. Surface morphologies of EPDM insulation show different features such as gully areas and white particles. The results of the Fourier transform infrared (FTIR) spectroscopy test indicate that the increase of oxygen-containing groups and free radicals are the key reasons for the rapid PD development process of cable insulation under different electrical gradations and thermal-oxygen degradations.Keywords
Funding Information
- National Key Research and Development Program Project of Ministry of Science and Technology (2018YFC309005)
This publication has 24 references indexed in Scilit:
- DC electrical breakdown dependence on the radial position of specimens within HVDc XLPE cable insulationIEEE Transactions on Dielectrics and Electrical Insulation, 2017
- Basic aspects of partial discharge on-site testing of long length transmission power cablesIEEE Transactions on Dielectrics and Electrical Insulation, 2017
- Thermal Analysis of Power Cables Installed in Solid Bottom Trays Using an Equivalent CircuitIEEE Transactions on Power Delivery, 2016
- Partial discharge phenomena within an artificial void in cable insulation geometry: experimental validation and simulationIEEE Transactions on Dielectrics and Electrical Insulation, 2016
- Aging Characteristics on Epoxy Resin Surface Under Repetitive Microsecond Pulses in Air at Atmospheric PressurePlasma Science and Technology, 2016
- Influence of temperature on dielectric properties of EPR and partial discharge behavior of spherical cavity in EPR insulationIEEE Transactions on Dielectrics and Electrical Insulation, 2015
- Physico-chemical study of thermally aged EPDM used in power cables insulationIEEE Transactions on Dielectrics and Electrical Insulation, 2015
- Investigation on insulation material morphological structure of 110 and 220 kV XLPE retired cables for reusingIEEE Transactions on Dielectrics and Electrical Insulation, 2014
- Thermal ageing behavior of styrene–butadiene random copolymer: A study on the ageing mechanism and relaxation propertiesPolymer Degradation and Stability, 2012
- Surface flashover of insulatorsIEEE Transactions on Electrical Insulation, 1989