Takehiko Nagai
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Takehiko Nagai has a total of 86 co-authors. Here are the top co-authors by number of shared publications:
- Hitoshi Tampo
National Institute of Advanced Industrial Science and Technology (AIST)
11 shared publications - Shinho Kim
Department of Materials Science and Engineering, Pusan National University, Busan 46742, Republic of Korea
8 shared publications Michio Kondo
6 shared publicationsHajime Shibata
Research Institute for Energy Conservation, National Institute of Advanced Industrial Science and Technology (AIST), Central 2, 1-1-1 Umezono, Tsukuba, Ibaraki 305-8568, Japan
5 shared publicationsNorio Terada
Graduate School of Science and Engineering, Kagoshima University, 1-21-40 Korimoto, Kagoshima 890-0065, Japan
5 shared publicationsZhengxin Liu
5 shared publications
Latest Publications
- 26 November 2024
- Published by Wiley in Physica Status Solidi (RRL) – Rapid Research Letters
- Vol. 19 (2)
Characterizing ZnMgO/Sb2Se3 Interface for Solar Cell Applications
This study investigates the band alignment of the Zn0.8Mg0.2O/Sb2Se3 interface structure to improve solar cell performance. Sb2Se3 is a promising absorber material. However, Sb2Se3 solar cells exhibit a lower conversion efficiency than CuInGaSe2 and CdTe solar cells. The lower efficiency of Sb2Se3 solar cells is attributed to the severe open‐circuit voltage loss caused by the band structure at the buffer/Sb2Se3 interface. Sb2Se3 solar cells typically employ CdS as the buffer layer, and the CdS/Sb2Se3 interface exhibits a cliff structure, which results in interfacial recombination. By contrast, a ZnMgO buffer layer can form a spike structure with Sb2Se3 at their interface, which reduces recombination and, as a result, enhances conversion efficiency. Therefore, this study employs the ZnMgO buffer layer and analyzes their material properties with various Mg contents and band structure at buffer/absorber layer interface. A ZnMgO buffer layer is sputter‐deposited on Sb2Se3. The optical bandgap of ZnMgO is 3.3–3.72 eV, corresponding to an Mg content of 0–0.35 at%. The carrier concentration indicates an appropriate doping level ranging from 1014 to 1016 cm−3. The Zn0.8Mg0.2O/Sb2Se3 interface is characterized via interface‐induced band bending. The Zn0.8Mg0.2O/Sb2Se3 interface exhibits a spike structure with a positive delta conduction band offset of +0.193 eV.
- 26 November 2024
- Published by Wiley in Physica Status Solidi (RRL) – Rapid Research Letters
- Vol. 19 (2)
Characterizing ZnMgO/Sb2Se3 Interface for Solar Cell Applications
This study investigates the band alignment of the Zn0.8Mg0.2O/Sb2Se3 interface structure to improve solar cell performance. Sb2Se3 is a promising absorber material. However, Sb2Se3 solar cells exhibit a lower conversion efficiency than CuInGaSe2 and CdTe solar cells. The lower efficiency of Sb2Se3 solar cells is attributed to the severe open‐circuit voltage loss caused by the band structure at the buffer/Sb2Se3 interface. Sb2Se3 solar cells typically employ CdS as the buffer layer, and the CdS/Sb2Se3 interface exhibits a cliff structure, which results in interfacial recombination. By contrast, a ZnMgO buffer layer can form a spike structure with Sb2Se3 at their interface, which reduces recombination and, as a result, enhances conversion efficiency. Therefore, this study employs the ZnMgO buffer layer and analyzes their material properties with various Mg contents and band structure at buffer/absorber layer interface. A ZnMgO buffer layer is sputter‐deposited on Sb2Se3. The optical bandgap of ZnMgO is 3.3–3.72 eV, corresponding to an Mg content of 0–0.35 at%. The carrier concentration indicates an appropriate doping level ranging from 1014 to 1016 cm−3. The Zn0.8Mg0.2O/Sb2Se3 interface is characterized via interface‐induced band bending. The Zn0.8Mg0.2O/Sb2Se3 interface exhibits a spike structure with a positive delta conduction band offset of +0.193 eV.
- 6 April 2024
- Published by Elsevier in Materials Letters
- Vol. 365
Cu2O single crystal growth using CuCl flux and bandgap evaluation
- 6 April 2024
- Published by Elsevier in Materials Letters
- Vol. 365
Cu2O single crystal growth using CuCl flux and bandgap evaluation
- Open Access
- 6 May 2022
- Published by Springer Nature in Scientific Reports
- Vol. 12 (1) , 1-9
Tunability of the bandgap of SnS by variation of the cell volume by alloying with A.E. elements
We clarified that the bandgap of inorganic materials is strongly correlated with their effective coordination number (ECoN) via first-principles calculations and experimental confirmations. Tin mono-sulphide (Pnma) and germanium mono-sulphide (Pnma) were selected as model cases since these materials successively alter the ECoN as the cell volume changes and show an uncommon relationship between cell volume and bandgap. Contrary to the common semiconductors, the bandgaps of SnS (Pnma) and GeS (Pnma) have a positive relationship with respect to cell volume. This unique phenomenon was explained by incorporating the concept of ECoN into the theoretical studies. The theory proposed in this study is widely applicable to semiconductors with low-symmetry structures. Further, we experimentally demonstrated that the bandgap of SnS (Pnma) can be broadly tuned by changing the unit cell volume via alloying with alkali-earth (A.E.) metals, which could allow SnS to be applied to Si-based tandem photovoltaics. Alloying with A.E. elements also stabilised Cl as an n-type donor, which enabled n-type conduction in the bandgap-widened SnS film in the SnS-based semiconductors.
- 6 May 2022
- Published by Springer Nature in Scientific Reports
- Vol. 12 (1) , 1-9
Open AccessTunability of the bandgap of SnS by variation of the cell volume by alloying with A.E. elements
We clarified that the bandgap of inorganic materials is strongly correlated with their effective coordination number (ECoN) via first-principles calculations and experimental confirmations. Tin mono-sulphide (Pnma) and germanium mono-sulphide (Pnma) were selected as model cases since these materials successively alter the ECoN as the cell volume changes and show an uncommon relationship between cell volume and bandgap. Contrary to the common semiconductors, the bandgaps of SnS (Pnma) and GeS (Pnma) have a positive relationship with respect to cell volume. This unique phenomenon was explained by incorporating the concept of ECoN into the theoretical studies. The theory proposed in this study is widely applicable to semiconductors with low-symmetry structures. Further, we experimentally demonstrated that the bandgap of SnS (Pnma) can be broadly tuned by changing the unit cell volume via alloying with alkali-earth (A.E.) metals, which could allow SnS to be applied to Si-based tandem photovoltaics. Alloying with A.E. elements also stabilised Cl as an n-type donor, which enabled n-type conduction in the bandgap-widened SnS film in the SnS-based semiconductors.
- 5 April 2022
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 14 (14) , 16780-16790
Impacts of KF Post-Deposition Treatment on the Band Alignment of Epitaxial Cu(In,Ga)Se2 Heterojunctions
In this study, we investigated band alignments at CdS/epitaxial CuInxGa1–xSe2 (epi-CIGSe) and epi-CIGSe/GaAs heterointerfaces for solar cell applications using ultraviolet, inverse, and X-ray photoemission spectroscopy (UPS, IPES, and XPS) techniques. We clarified the impacts of KF postdeposition treatment (KF-PDT) at the CdS/epi-CIGSe front heterointerfaces. We found that KF-PDT changed the conduction band alignment at the CdS/epi-CIGSe heterointerface from a cliff to flat configuration, attributed to an increase in the electron affinity (EA) and ionization potential (IP) of the epi-CIGSe surface because of a decrease in Cu and Ga contents. Herein, we discuss the correlation between the impacts of KF-PDT and the solar cell performance. Furthermore, we also investigated the band alignment at the epi-CIGSe/GaAs rear heterointerface. Electron barriers were formed at the epi-CIGSe/GaAs interface, suppressing carrier recombination as the back surface field. Contrarily, a hole accumulation layer is formed by the valence band bending, which is like Ohmic contact.
- 5 April 2022
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 14 (14) , 16780-16790
Impacts of KF Post-Deposition Treatment on the Band Alignment of Epitaxial Cu(In,Ga)Se2 Heterojunctions
In this study, we investigated band alignments at CdS/epitaxial CuInxGa1–xSe2 (epi-CIGSe) and epi-CIGSe/GaAs heterointerfaces for solar cell applications using ultraviolet, inverse, and X-ray photoemission spectroscopy (UPS, IPES, and XPS) techniques. We clarified the impacts of KF postdeposition treatment (KF-PDT) at the CdS/epi-CIGSe front heterointerfaces. We found that KF-PDT changed the conduction band alignment at the CdS/epi-CIGSe heterointerface from a cliff to flat configuration, attributed to an increase in the electron affinity (EA) and ionization potential (IP) of the epi-CIGSe surface because of a decrease in Cu and Ga contents. Herein, we discuss the correlation between the impacts of KF-PDT and the solar cell performance. Furthermore, we also investigated the band alignment at the epi-CIGSe/GaAs rear heterointerface. Electron barriers were formed at the epi-CIGSe/GaAs interface, suppressing carrier recombination as the back surface field. Contrarily, a hole accumulation layer is formed by the valence band bending, which is like Ohmic contact.
- 3 March 2021
- Published by Wiley in Physica Status Solidi (a)
- Vol. 218 (10) , 2000658
Examination of Suitable Bandgap Grading of Cu(InGa)Se2 Bottom Absorber Layers for Tandem Cell Application
A high‐efficiency tandem solar cell comprises of top and bottom solar cells. The bottom cell has a bandgap of ≈1.1 eV and is designed to absorb longer wavelengths of photons. A Cu(InGa)Se2 (CIGS) is one of the candidates for a bottom solar cell, but its bandgap is not constant and is graded with depth. This study discusses suitable bandgap grading of CIGS cells for bottom cell applications. Three CIGS devices with different bandgap gradings are prepared for bottom cell evaluation. One device has a single‐back‐graded bandgap type whereas the others have double‐graded bandgap types, which have been used for high‐efficiency CIGS devices. The three CIGS devices exhibit similar conversion efficiencies of ≈20% but different solar cell parameters, due to their different shapes of bandgap grading. For the bottom cell evaluations, current–voltage measurements are performed using 720 nm (≈1.72 eV) and 800 nm (≈1.55 eV) long‐pass filters. It is found that a CIGS device with a double‐graded bandgap is unsuitable and/or shows reduced performance with a decreased top cell bandgap. By contrast, CIGS devices with a single‐back‐graded bandgap can be adopted as a bottom cell under top cell bandgaps of both ≈1.55 and ≈1.72 eV.
- 3 March 2021
- Published by Wiley in Physica Status Solidi (a)
- Vol. 218 (10) , 2000658
Examination of Suitable Bandgap Grading of Cu(InGa)Se2 Bottom Absorber Layers for Tandem Cell Application
A high‐efficiency tandem solar cell comprises of top and bottom solar cells. The bottom cell has a bandgap of ≈1.1 eV and is designed to absorb longer wavelengths of photons. A Cu(InGa)Se2 (CIGS) is one of the candidates for a bottom solar cell, but its bandgap is not constant and is graded with depth. This study discusses suitable bandgap grading of CIGS cells for bottom cell applications. Three CIGS devices with different bandgap gradings are prepared for bottom cell evaluation. One device has a single‐back‐graded bandgap type whereas the others have double‐graded bandgap types, which have been used for high‐efficiency CIGS devices. The three CIGS devices exhibit similar conversion efficiencies of ≈20% but different solar cell parameters, due to their different shapes of bandgap grading. For the bottom cell evaluations, current–voltage measurements are performed using 720 nm (≈1.72 eV) and 800 nm (≈1.55 eV) long‐pass filters. It is found that a CIGS device with a double‐graded bandgap is unsuitable and/or shows reduced performance with a decreased top cell bandgap. By contrast, CIGS devices with a single‐back‐graded bandgap can be adopted as a bottom cell under top cell bandgaps of both ≈1.55 and ≈1.72 eV.
- 3 May 2020
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 28 (8) , 816-822
Large open‐circuit voltage boosting of pure sulfide chalcopyrite Cu(In,Ga)S2 prepared using Cu‐deficient metal precursors
We performed a comparative study to find out the reasons why it is necessary to prepare the pure sulfide chalcopyrite, Cu(InGa)S2 (CIGS) under a Cu‐deficient condition to improve solar cell performance. It has been shown that CIGS that was grown under Cu‐deficient condition exhibits large open‐circuit voltage (VOC) boosting compared with that the one grown under Cu‐excess condition. Thus, CIGS were prepared from Cu‐excess and Cu‐deficient metal precursor (MP) and characterized concerning the origins of the different VOC. We observed that CIGS prepared using Cu‐excess MP suffered large recombination at buffer/CIGS interface and in bulk, which resulted in serious limitation of the VOC. On the other hand, CIGS prepared from Cu‐deficient MP exhibited largely improved VOC with reduced recombination. We conducted defect analysis using the photoluminescence (PL) method, and CIGS prepared using Cu‐excess MP exhibited strong deep emissions. However, CIGS prepared from Cu‐deficient MP exhibited PL emission characteristics without deep level transition. This implies that a large number of deep level defects exist in the CIGS prepared using Cu‐excess MP, and this might be the reason for the large recombination limiting VOC of the device. Finally, we also present the reason for deep levels in the CIGS prepared using Cu‐excess MP.
- 3 May 2020
- Published by Wiley in Progress in Photovoltaics: Research and Applications
- Vol. 28 (8) , 816-822
Large open‐circuit voltage boosting of pure sulfide chalcopyrite Cu(In,Ga)S2 prepared using Cu‐deficient metal precursors
We performed a comparative study to find out the reasons why it is necessary to prepare the pure sulfide chalcopyrite, Cu(InGa)S2 (CIGS) under a Cu‐deficient condition to improve solar cell performance. It has been shown that CIGS that was grown under Cu‐deficient condition exhibits large open‐circuit voltage (VOC) boosting compared with that the one grown under Cu‐excess condition. Thus, CIGS were prepared from Cu‐excess and Cu‐deficient metal precursor (MP) and characterized concerning the origins of the different VOC. We observed that CIGS prepared using Cu‐excess MP suffered large recombination at buffer/CIGS interface and in bulk, which resulted in serious limitation of the VOC. On the other hand, CIGS prepared from Cu‐deficient MP exhibited largely improved VOC with reduced recombination. We conducted defect analysis using the photoluminescence (PL) method, and CIGS prepared using Cu‐excess MP exhibited strong deep emissions. However, CIGS prepared from Cu‐deficient MP exhibited PL emission characteristics without deep level transition. This implies that a large number of deep level defects exist in the CIGS prepared using Cu‐excess MP, and this might be the reason for the large recombination limiting VOC of the device. Finally, we also present the reason for deep levels in the CIGS prepared using Cu‐excess MP.
- 23 January 2020
- Published by Wiley in Physica Status Solidi (RRL) – Rapid Research Letters
- Vol. 14 (4)
Characterization of Surface and Heterointerface of Cu2ZnSn1–xGexSe4 for Solar Cell Applications
This study analyzes the electronic structure of Cu2ZnSn1–xGexSe4 (CZTGSe) surface and band alignments of CdS and CZTGSe using the Ge/(Sn + Ge) composition ratios of x = 0–1 based on inversed, ultraviolet, and X‐ray photoemission spectroscopy. The conduction band offsets of the CdS/CZTGSe interface linearly decrease with increasing x, which are so‐called spike conduction band connections, whereas the valence band offsets are observed to be independent of x. Moreover, the hole density near the CZTGSe surface increases with an increase in x; this corresponds to the increase in the measured built‐in‐potential with x. However, the open circuit voltage (VOC) saturates to ≈0.5 V for x over 0.2 in spite of the favorable band alignment and larger built‐in‐potential of x at the interface. External‐quantum‐efficiency spectral analysis shows that the carrier recombination in CZTGSe bulk is suppressed with an increase in x, whereas the recombination near the CZTGSe surface is enhanced. The relationship between these recombination centers, electronic structure, and saturation of VOC is discussed.
- 23 January 2020
- Published by Wiley in Physica Status Solidi (RRL) – Rapid Research Letters
- Vol. 14 (4)
Characterization of Surface and Heterointerface of Cu2ZnSn1–xGexSe4 for Solar Cell Applications
This study analyzes the electronic structure of Cu2ZnSn1–xGexSe4 (CZTGSe) surface and band alignments of CdS and CZTGSe using the Ge/(Sn + Ge) composition ratios of x = 0–1 based on inversed, ultraviolet, and X‐ray photoemission spectroscopy. The conduction band offsets of the CdS/CZTGSe interface linearly decrease with increasing x, which are so‐called spike conduction band connections, whereas the valence band offsets are observed to be independent of x. Moreover, the hole density near the CZTGSe surface increases with an increase in x; this corresponds to the increase in the measured built‐in‐potential with x. However, the open circuit voltage (VOC) saturates to ≈0.5 V for x over 0.2 in spite of the favorable band alignment and larger built‐in‐potential of x at the interface. External‐quantum‐efficiency spectral analysis shows that the carrier recombination in CZTGSe bulk is suppressed with an increase in x, whereas the recombination near the CZTGSe surface is enhanced. The relationship between these recombination centers, electronic structure, and saturation of VOC is discussed.
- 22 March 2019
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 11 (14) , 13319-13325
Improving the Open Circuit Voltage through Surface Oxygen Plasma Treatment and 11.7% Efficient Cu2ZnSnSe4 Solar Cell
The photovoltaic performance of Cu2ZnSnSe4 (CZTSe) solar cells subject to surface oxygen plasma treatments is investigated. The observed improvements are related to an enhancement of the open circuit voltage VOC, that is, the suppression of the VOC deficit. The VOC monotonically increases with treatment time up to 0.460 V. The origin of this improvement is discussed, and it is concluded that the effectiveness of the surface treatment is due not to oxygen-related alloying, but instead to the homogeneous oxidization and removal of the oxidized CZTSe surface layer. The surface oxygen content increases with surface treatment time, although surface oxides are fully removed after ammonia treatment, which is conducted in a similar manner to CdS buffer deposition. The reduction of surface recombination is confirmed by time-resolved photoluminescence measurements and the minority carrier lifetime deduced using the fast decay component increases with increasing treatment time. The relationship between photovoltaic properties and lifetime is clearly demonstrated. The best-performing CZTSe solar cell obtained using surface oxygen treatment demonstrates a conversion efficiency of 11.7%, which is higher than that of previous reports on CZTSe cells.
- 22 March 2019
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 11 (14) , 13319-13325
Improving the Open Circuit Voltage through Surface Oxygen Plasma Treatment and 11.7% Efficient Cu2ZnSnSe4 Solar Cell
The photovoltaic performance of Cu2ZnSnSe4 (CZTSe) solar cells subject to surface oxygen plasma treatments is investigated. The observed improvements are related to an enhancement of the open circuit voltage VOC, that is, the suppression of the VOC deficit. The VOC monotonically increases with treatment time up to 0.460 V. The origin of this improvement is discussed, and it is concluded that the effectiveness of the surface treatment is due not to oxygen-related alloying, but instead to the homogeneous oxidization and removal of the oxidized CZTSe surface layer. The surface oxygen content increases with surface treatment time, although surface oxides are fully removed after ammonia treatment, which is conducted in a similar manner to CdS buffer deposition. The reduction of surface recombination is confirmed by time-resolved photoluminescence measurements and the minority carrier lifetime deduced using the fast decay component increases with increasing treatment time. The relationship between photovoltaic properties and lifetime is clearly demonstrated. The best-performing CZTSe solar cell obtained using surface oxygen treatment demonstrates a conversion efficiency of 11.7%, which is higher than that of previous reports on CZTSe cells.
- 9 January 2019
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 11 (4) , 4637-4648
Band Alignment of the CdS/Cu2Zn(Sn1–xGex)Se4 Heterointerface and Electronic Properties at the Cu2Zn(Sn1–xGex)Se4 Surface: x = 0, 0.2, and 0.4
The surface electronic properties of the light absorber and band alignment at the p/n heterointerface are key issues for high-performance heterojunction solar cells. We investigated the band alignment of the heterointerface between cadmium sulfide (CdS) and Ge-incorporated Cu2ZnSnSe4 (CZTGSe), with Ge/(Ge + Sn) ratios ( x) between 0 and 0.4, by X-ray photoelectron, ultraviolet, and inversed photoemission spectroscopies (XPS, UPS, and IPES, respectively). In particular, we used interface-induced band bending in order to determine the conduction band offset (CBO) and valence-band offset (VBO), which were calculated from the core-level shifts of each element in both the CdS overlayer and the CZTGSe bottom layer. Moreover, the surface electronic properties of CZTGSe were also investigated by laser-irradiated XPS. The CBO at the CdS/CZTGSe heterointerface decreased linearly, from +0.36 to +0.20 eV, as x was increased from 0 to 0.4; in contrast, the VBO at the CdS/CZTGSe heterointerface was independent of Ge content. Both UPS and IPES revealed that the Fermi level at the CZTGSe surface is located near the center of the band gap. The hole concentration at the CZTGSe surface was on the order of 1011 cm-3, which is much smaller than that of the bulk (∼1016 cm-3). We discuss the differences in hole deficiencies near the surface and in the bulk on the basis of laser-irradiated XPS and conclude that hole deficiencies are due to defects distributed near the surface with densities that are lower than in the bulk, and the Fermi level is not pinned at the CZTGSe surface.
- 9 January 2019
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 11 (4) , 4637-4648
Band Alignment of the CdS/Cu2Zn(Sn1–xGex)Se4 Heterointerface and Electronic Properties at the Cu2Zn(Sn1–xGex)Se4 Surface: x = 0, 0.2, and 0.4
The surface electronic properties of the light absorber and band alignment at the p/n heterointerface are key issues for high-performance heterojunction solar cells. We investigated the band alignment of the heterointerface between cadmium sulfide (CdS) and Ge-incorporated Cu2ZnSnSe4 (CZTGSe), with Ge/(Ge + Sn) ratios ( x) between 0 and 0.4, by X-ray photoelectron, ultraviolet, and inversed photoemission spectroscopies (XPS, UPS, and IPES, respectively). In particular, we used interface-induced band bending in order to determine the conduction band offset (CBO) and valence-band offset (VBO), which were calculated from the core-level shifts of each element in both the CdS overlayer and the CZTGSe bottom layer. Moreover, the surface electronic properties of CZTGSe were also investigated by laser-irradiated XPS. The CBO at the CdS/CZTGSe heterointerface decreased linearly, from +0.36 to +0.20 eV, as x was increased from 0 to 0.4; in contrast, the VBO at the CdS/CZTGSe heterointerface was independent of Ge content. Both UPS and IPES revealed that the Fermi level at the CZTGSe surface is located near the center of the band gap. The hole concentration at the CZTGSe surface was on the order of 1011 cm-3, which is much smaller than that of the bulk (∼1016 cm-3). We discuss the differences in hole deficiencies near the surface and in the bulk on the basis of laser-irradiated XPS and conclude that hole deficiencies are due to defects distributed near the surface with densities that are lower than in the bulk, and the Fermi level is not pinned at the CZTGSe surface.
- 29 March 2018
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 57 (5)
Reduced recombination in a surface-sulfurized Cu(InGa)Se 2 thin-film solar cell
This study demonstrates surface sulfurization effects on Cu(InGa)Se 2 (CIGSe) thin-film solar cells with a single back-graded band gap. Single back-graded CIGSe thin films were prepared via a three-stage process in a high-vacuum molecular beam epitaxial growth chamber and were subsequently annealed in a tube furnace under environmental conditions with H 2 S gas. After sulfurization, an ∼80- to ∼100-nm-thick CuIn(SSe) 2 layer with significantly small Ga contents (CISSe:Ga) was formed on the CIGSe layer. The newly formed CISSe:Ga layer exhibited graded S contents from surface to bulk, thus resulting in a front-graded band gap. In addition, CISSe:Ga was covered with S-enriched CISSe region that was extended from the surface to a depth of a few nm and was depleted of Ga. A device with the sulfurized CIGSe showed reduced recombination at the buffer–absorber interface, in space-charge region and in bulk. Consequently, the open circuit voltage increased from 0.58 V (in the non-sulfurized case) to 0.66 V, and the conversion efficiency improved from 15.5 to 19.4%. This large improvement is caused by the front graded band gap at the surface and the hole-blocking barrier, which suppress recombination at the CdS/CISSe:Ga interface. In addition, sulfurization followed by KF post-deposition treatment (PDT) increased the efficiency to 20.1%. Compared to the untreated sulfurized device, the KF-PDT device delivered an increased carrier lifetime and reduced the recombination in bulk probably because the defects were passivated by the K, which penetrated into the bulk region.
- 29 March 2018
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 57 (5)
Reduced recombination in a surface-sulfurized Cu(InGa)Se 2 thin-film solar cell
This study demonstrates surface sulfurization effects on Cu(InGa)Se 2 (CIGSe) thin-film solar cells with a single back-graded band gap. Single back-graded CIGSe thin films were prepared via a three-stage process in a high-vacuum molecular beam epitaxial growth chamber and were subsequently annealed in a tube furnace under environmental conditions with H 2 S gas. After sulfurization, an ∼80- to ∼100-nm-thick CuIn(SSe) 2 layer with significantly small Ga contents (CISSe:Ga) was formed on the CIGSe layer. The newly formed CISSe:Ga layer exhibited graded S contents from surface to bulk, thus resulting in a front-graded band gap. In addition, CISSe:Ga was covered with S-enriched CISSe region that was extended from the surface to a depth of a few nm and was depleted of Ga. A device with the sulfurized CIGSe showed reduced recombination at the buffer–absorber interface, in space-charge region and in bulk. Consequently, the open circuit voltage increased from 0.58 V (in the non-sulfurized case) to 0.66 V, and the conversion efficiency improved from 15.5 to 19.4%. This large improvement is caused by the front graded band gap at the surface and the hole-blocking barrier, which suppress recombination at the CdS/CISSe:Ga interface. In addition, sulfurization followed by KF post-deposition treatment (PDT) increased the efficiency to 20.1%. Compared to the untreated sulfurized device, the KF-PDT device delivered an increased carrier lifetime and reduced the recombination in bulk probably because the defects were passivated by the K, which penetrated into the bulk region.