Konstantin V. Krukovskii
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Konstantin V. Krukovskii has a total of 77 co-authors. Here are the top co-authors by number of shared publications:
- Aleksandr Ivanovich Lotkov
Institute of Strength Physics and Materials Science, Siberian Branch, Russian Academy of Sciences, Tomsk, Russia
20 shared publications - Oleg A. Kashin
Institute of Strength Physics and Materials Science SB RAS, Tomsk, 634055 Russia
11 shared publications - Andrey N. Kudryashov
Angioline Interventional Device Ltd., Novosibirsk, 630090 Russia
5 shared publications - Dorzhima Zhapova
Institute of Strength Physics and Materials Science, Siberian Branch, Russian Academy of Sciences, Tomsk, Russia
5 shared publications - Angelina Gusarenko
Institute of Strength Physics and Materials Science, Siberian Branch, Russian Academy of Sciences, Tomsk, Russia
4 shared publications - Sergei A. Martynov
Institute of Strength Physics and Materials Science, Far Siberian Branch of Russian Academy of Sciences, Tomsk, Russia
4 shared publications
Latest Publications
- 8 December 2025
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 16 (6) , 1980-1986
Structural Phase State, Martensitic Transformations and Inelastic Properties of TiNi-based Alloy Fabricated by Electron Beam Wire-Feed Additive Manufacturing
In this paper, the structural phase state, martensitic transformation temperatures, and inelastic properties of a TiNi-based alloy obtained by electron beam wire-feed additive manufacturing (EBAM) on a Ti49.8Ni50.2 (at %) substrate were studied. It was shown that the printed samples had an inhomogeneous coarse-grained microstructure both in the direction perpendicular and parallel to the substrate. The microstructure type of the samples obtained by EBAM depends on the distance from the substrate and is determined by the cooling conditions in the vacuum chamber of the setup for 20 h from 800°C. At room temperature, the obtained samples had a high-temperature B2-phase structure. It was established that the printed samples underwent a B2 ↔ B19' martensitic transformation upon cooling and heating. It was shown that the studied samples exhibit a superelasticity of 9.01% under torsion with an accumulated plastic strain of 1.28% (including 5.78% in the absence of plastic deformation).
- 8 December 2025
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 16 (6) , 1980-1986
Structural Phase State, Martensitic Transformations and Inelastic Properties of TiNi-based Alloy Fabricated by Electron Beam Wire-Feed Additive Manufacturing
In this paper, the structural phase state, martensitic transformation temperatures, and inelastic properties of a TiNi-based alloy obtained by electron beam wire-feed additive manufacturing (EBAM) on a Ti49.8Ni50.2 (at %) substrate were studied. It was shown that the printed samples had an inhomogeneous coarse-grained microstructure both in the direction perpendicular and parallel to the substrate. The microstructure type of the samples obtained by EBAM depends on the distance from the substrate and is determined by the cooling conditions in the vacuum chamber of the setup for 20 h from 800°C. At room temperature, the obtained samples had a high-temperature B2-phase structure. It was established that the printed samples underwent a B2 ↔ B19' martensitic transformation upon cooling and heating. It was shown that the studied samples exhibit a superelasticity of 9.01% under torsion with an accumulated plastic strain of 1.28% (including 5.78% in the absence of plastic deformation).
- 28 October 2025
- Published by Pleiades Publishing Ltd in Bulletin of the Russian Academy of Sciences: Physics
- Vol. 89 (10) , 2038-2045
Effect of Titanium and Titanium Nickelide Substrates on the Structural-Phase State and Mechanical Properties of Electron Beam Additive Manufacturing TiNi-Based Alloys
We investigated the structural-phase state and mechanical properties of a TiNi-based alloy, obtained by electron beam wire-feed additive manufacturing on titanium and titanium nickelide substrates. It was shown that the printed samples have a heterogeneous coarse-grained microstructure. At room temperature, the obtained samples have the structure of the high-temperature B2-phase of TiNi and the secondary Ti2Ni (or Ti4Ni2Ox) phase. It was found that the printed samples on the Grade 2 substrate failed brittlely during testing. The printed samples on Ti49.8Ni50.2 (at %) substrate were plastically deformed and demonstrated pseudoelasticity plateau. It is shown that the value of mechanical properties correlates with the content of Ti2Ni (or Ti4Ni2Ox).
- 28 October 2025
- Published by Pleiades Publishing Ltd in Bulletin of the Russian Academy of Sciences: Physics
- Vol. 89 (10) , 2038-2045
Effect of Titanium and Titanium Nickelide Substrates on the Structural-Phase State and Mechanical Properties of Electron Beam Additive Manufacturing TiNi-Based Alloys
We investigated the structural-phase state and mechanical properties of a TiNi-based alloy, obtained by electron beam wire-feed additive manufacturing on titanium and titanium nickelide substrates. It was shown that the printed samples have a heterogeneous coarse-grained microstructure. At room temperature, the obtained samples have the structure of the high-temperature B2-phase of TiNi and the secondary Ti2Ni (or Ti4Ni2Ox) phase. It was found that the printed samples on the Grade 2 substrate failed brittlely during testing. The printed samples on Ti49.8Ni50.2 (at %) substrate were plastically deformed and demonstrated pseudoelasticity plateau. It is shown that the value of mechanical properties correlates with the content of Ti2Ni (or Ti4Ni2Ox).
- 1 November 2024
- Published by Springer Nature in Russian Physics Journal
- Vol. 67 (11) , 2088-2092
Features of the structural-phase state of thin-walled samples produced by electron beam wire-feed additive manufacturing on a titanium substrate
- 1 November 2024
- Published by Springer Nature in Russian Physics Journal
- Vol. 67 (11) , 2088-2092
Features of the structural-phase state of thin-walled samples produced by electron beam wire-feed additive manufacturing on a titanium substrate
- Open Access
RHEED Study of the Epitaxial Growth of Silicon and Germanium on Highly Oriented Pyrolytic Graphite
Two-dimensional silicon (silicene) and germanium (germanene) have attracted special attention from researchers in recent years. At the same time, highly oriented pyrolytic graphite (HOPG) and graphene are some of the promising substrates for growing silicene and germanene. However, to date, the processes occurring during the epitaxial growth of silicon and germanium on the surface of such substrates have been poorly studied. In this work, the epitaxial growth of silicon and germanium is studied directly during the process of the molecular beam epitaxy deposition of material onto the HOPG surface by reflection high-energy electron diffraction (RHEED). In addition, the obtained samples are studied by Raman spectroscopy and scanning electron microscopy. A wide range of deposition temperatures from 100 to 800 °C is considered and temperature intervals are determined for various growth modes of silicon and germanium on HOPG. Conditions for amorphous and polycrystalline growth are distinguished. Diffraction spots corresponding to the lattice constants of silicene and germanene are identified that may indicate the presence of areas of graphene-like 2D phases during epitaxial deposition of silicon and germanium onto the surface of highly oriented pyrolytic graphite.
Open AccessRHEED Study of the Epitaxial Growth of Silicon and Germanium on Highly Oriented Pyrolytic Graphite
Two-dimensional silicon (silicene) and germanium (germanene) have attracted special attention from researchers in recent years. At the same time, highly oriented pyrolytic graphite (HOPG) and graphene are some of the promising substrates for growing silicene and germanene. However, to date, the processes occurring during the epitaxial growth of silicon and germanium on the surface of such substrates have been poorly studied. In this work, the epitaxial growth of silicon and germanium is studied directly during the process of the molecular beam epitaxy deposition of material onto the HOPG surface by reflection high-energy electron diffraction (RHEED). In addition, the obtained samples are studied by Raman spectroscopy and scanning electron microscopy. A wide range of deposition temperatures from 100 to 800 °C is considered and temperature intervals are determined for various growth modes of silicon and germanium on HOPG. Conditions for amorphous and polycrystalline growth are distinguished. Diffraction spots corresponding to the lattice constants of silicene and germanene are identified that may indicate the presence of areas of graphene-like 2D phases during epitaxial deposition of silicon and germanium onto the surface of highly oriented pyrolytic graphite.
- 1 April 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (2) , 489-497
Features of the Grain-Subgrain Structure of Ti49.8Ni50.2 Alloy after Megaplastic Deformation by abc Pressing and Subsequent Annealing
Using the backscattered electron diffraction method, the features of grain-subgrain structure of the Ti49.8Ni50.2 (at %) alloy after megaplastic deformation by multiaxial forging (abc pressing) at 573 K and subsequent annealing were studied. It has been shown that the best detection of patterns of grain-subgrain structure of the Ti49.8Ni50.2 alloy after a given true deformation of e = 9.55 and annealing at 773 K for 2 h is observed in zones without martensitic relief on the surface of a samples. The clearest backscattered electron diffraction patterns are observed in the central part of grains, and the quality of the Kikuchi lines deteriorates with distance from the grain center. Calculation based on the equivalent grain diameter showed that the average grain size is 0.203 ± 0.053 μm. Grains are mainly elliptical in shape with an axial ratio of 0.48. Elongated grains along their length have a discrete-continuous misorientation of the crystal structure, which can reach 5 degrees per 1 μm.
- 1 April 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (2) , 489-497
Features of the Grain-Subgrain Structure of Ti49.8Ni50.2 Alloy after Megaplastic Deformation by abc Pressing and Subsequent Annealing
Using the backscattered electron diffraction method, the features of grain-subgrain structure of the Ti49.8Ni50.2 (at %) alloy after megaplastic deformation by multiaxial forging (abc pressing) at 573 K and subsequent annealing were studied. It has been shown that the best detection of patterns of grain-subgrain structure of the Ti49.8Ni50.2 alloy after a given true deformation of e = 9.55 and annealing at 773 K for 2 h is observed in zones without martensitic relief on the surface of a samples. The clearest backscattered electron diffraction patterns are observed in the central part of grains, and the quality of the Kikuchi lines deteriorates with distance from the grain center. Calculation based on the equivalent grain diameter showed that the average grain size is 0.203 ± 0.053 μm. Grains are mainly elliptical in shape with an axial ratio of 0.48. Elongated grains along their length have a discrete-continuous misorientation of the crystal structure, which can reach 5 degrees per 1 μm.
- Open Access
Transformations of the Microstructure and Phase Compositions of Titanium Alloys during Ultrasonic Impact Treatment Part III: Combination with Electrospark Alloying Applied to Additively Manufactured Ti-6Al-4V Titanium Alloy
Scanning electron microscopy, 3D optical surface profilometry, as well as X-ray diffraction and electron backscatter diffraction analysis were implemented for studying the effects of both ultrasonic impact treatment (UIT) and ultrasonic impact electrospark treatment (UIET) procedures on the microstructure, phase composition, as well as the mechanical and tribological properties of Ti-6Al-4V samples fabricated by wire-feed electron beam additive manufacturing. It was shown that he UIET procedure with the WC-6%Co striker enabled to deposit the ~10 µm thick coating, which consists of fine grains of both tungsten and titanium-tungsten carbides, as well as titanium oxide. For the UIET process, the effect of shielding gas on the studied parameters was demonstrated. It was found that the UIET procedure in argon resulted in the formation of a dense, continuous and thick (~20 µm) coating. After the UIET procedures in air and argon, the microhardness levels were 26 and 16 GPa, respectively. After tribological tests, wear track surfaces were examined on the as-built sample, as well as the ones subjected to the UIT and UIET procedures. It was shown that the coating formed during UIET in air had twice the wear resistance compared to the coating formed in argon. The evidence showed that the multiple impact of a WC-Co striker with simultaneous electrical discharges was an effective way to improve wear resistance of the Ti-6Al-4V sample.
Open AccessTransformations of the Microstructure and Phase Compositions of Titanium Alloys during Ultrasonic Impact Treatment Part III: Combination with Electrospark Alloying Applied to Additively Manufactured Ti-6Al-4V Titanium Alloy
Scanning electron microscopy, 3D optical surface profilometry, as well as X-ray diffraction and electron backscatter diffraction analysis were implemented for studying the effects of both ultrasonic impact treatment (UIT) and ultrasonic impact electrospark treatment (UIET) procedures on the microstructure, phase composition, as well as the mechanical and tribological properties of Ti-6Al-4V samples fabricated by wire-feed electron beam additive manufacturing. It was shown that he UIET procedure with the WC-6%Co striker enabled to deposit the ~10 µm thick coating, which consists of fine grains of both tungsten and titanium-tungsten carbides, as well as titanium oxide. For the UIET process, the effect of shielding gas on the studied parameters was demonstrated. It was found that the UIET procedure in argon resulted in the formation of a dense, continuous and thick (~20 µm) coating. After the UIET procedures in air and argon, the microhardness levels were 26 and 16 GPa, respectively. After tribological tests, wear track surfaces were examined on the as-built sample, as well as the ones subjected to the UIT and UIET procedures. It was shown that the coating formed during UIET in air had twice the wear resistance compared to the coating formed in argon. The evidence showed that the multiple impact of a WC-Co striker with simultaneous electrical discharges was an effective way to improve wear resistance of the Ti-6Al-4V sample.
- Open Access
Mechanical Properties of the Ti49.8Ni50.2 Alloy after Multi-Axial Forging at 573 K
The mechanical properties of Ti49.8Ni50.2 (at %) alloy under tension at room temperature are studied in dependence on the true strain (e = 1.84–9.55) specified during isothermal multi-axial forging (abc-pressing). It was found that the stress at the beginning of the pseudoyield plateau does not depend on the value of the true abc-strain. It was found that after abs-pressing, already at a true strain e = 1.84, the yield stress σy was 900 ± 25 MPa, which is more than twice as high as compared to σy in the initial state of the specimens. With a further increase in the abc-strain, the yield stress continues to increase slightly and reaches 1000 ± 25 MPa at e = 9.55. In this case, the ultimate tensile strength of the samples increases by about 15%. The strain-hardening coefficient ϴ = dσ/dε at the III (linear) stage of the σ(ε) curve has a similar dependence on e. It is shown that after abc-pressing with e from 1.84 to 9.55, the yield stress and ultimate tensile increase linearly with increasing d−1/2 in accordance with the Hall–Petch relation, where d is the average grain–subgrain size.
Open AccessMechanical Properties of the Ti49.8Ni50.2 Alloy after Multi-Axial Forging at 573 K
The mechanical properties of Ti49.8Ni50.2 (at %) alloy under tension at room temperature are studied in dependence on the true strain (e = 1.84–9.55) specified during isothermal multi-axial forging (abc-pressing). It was found that the stress at the beginning of the pseudoyield plateau does not depend on the value of the true abc-strain. It was found that after abs-pressing, already at a true strain e = 1.84, the yield stress σy was 900 ± 25 MPa, which is more than twice as high as compared to σy in the initial state of the specimens. With a further increase in the abc-strain, the yield stress continues to increase slightly and reaches 1000 ± 25 MPa at e = 9.55. In this case, the ultimate tensile strength of the samples increases by about 15%. The strain-hardening coefficient ϴ = dσ/dε at the III (linear) stage of the σ(ε) curve has a similar dependence on e. It is shown that after abc-pressing with e from 1.84 to 9.55, the yield stress and ultimate tensile increase linearly with increasing d−1/2 in accordance with the Hall–Petch relation, where d is the average grain–subgrain size.
- Open Access
Effect of abc Pressing at 573 K on the Microstructure and Martensite Transformation Temperatures in Ti49.8Ni50.2 (at%)
This paper presents experimental data on the microstructure and martensite transformation temperatures of Ti49.8Ni50.2 (at%) after abc pressing (multi-axial forging) to different true strains e from 1.84 to 9.55 at 573 K. The data show that increasing the true strain results in grain–subgrain refinement on different scales at a time. With e = 9.55 at 573 K, the average grain–subgrain size measured approximately 130 nm. Decreasing the abc pressing temperature from 723 to 573 K caused a decrease in all martensite transformation temperatures, a change in the lattice parameters, R phase formation, and angular shifts of diffraction peaks and their broadening. The largest change in the microstructure of Ti49.8Ni50.2 was provided by abc pressing to e = 1.84. Increasing the true strain to e = 9.55 resulted in a much smaller effect, suggesting that the alloy obtained a high density of structural defects even at e = 1.84. Two possible mechanisms of grain–subgrain refinement are discussed.
Open AccessEffect of abc Pressing at 573 K on the Microstructure and Martensite Transformation Temperatures in Ti49.8Ni50.2 (at%)
This paper presents experimental data on the microstructure and martensite transformation temperatures of Ti49.8Ni50.2 (at%) after abc pressing (multi-axial forging) to different true strains e from 1.84 to 9.55 at 573 K. The data show that increasing the true strain results in grain–subgrain refinement on different scales at a time. With e = 9.55 at 573 K, the average grain–subgrain size measured approximately 130 nm. Decreasing the abc pressing temperature from 723 to 573 K caused a decrease in all martensite transformation temperatures, a change in the lattice parameters, R phase formation, and angular shifts of diffraction peaks and their broadening. The largest change in the microstructure of Ti49.8Ni50.2 was provided by abc pressing to e = 1.84. Increasing the true strain to e = 9.55 resulted in a much smaller effect, suggesting that the alloy obtained a high density of structural defects even at e = 1.84. Two possible mechanisms of grain–subgrain refinement are discussed.
- 1 October 2020
- Published by Springer Nature in Russian Physics Journal
- Vol. 63 (6) , 997-1002
Enhancement of Mechanical Stability of Silicon Macrospecimens Containing Hierarchically-Structured Porous Silicon
- 1 October 2020
- Published by Springer Nature in Russian Physics Journal
- Vol. 63 (6) , 997-1002
Enhancement of Mechanical Stability of Silicon Macrospecimens Containing Hierarchically-Structured Porous Silicon
- Open Access
Effect of True Strains in Isothermal abc Pressing on Mechanical Properties of Ti49.8Ni50.2 Alloy
The paper analyzes the microstructure and mechanical properties of Ti49.8Ni50.2 alloy (at.%) under uniaxial tension at room temperature after isothermal abc pressing to true strains e = 0.29 − 8.44 at T = 723 K. The analysis shows that as the true strain e is increased, the grain–subgrain structure of the alloy is gradually refined. This leads to an increase in its yield stress σy and strain hardening coefficient θ = dσ/dε at linear stage III of its tensile stress–strain curve according to the Hall–Petch relation. However, the ultimate tensile strength remains invariant to such refinement. The possible mechanism is proposed to explain why the ultimate tensile strength can remain invariant to the average grains size (dav). It is assumed that the sharp increase of the ultimate tensile strength σUTS begins when (dav) is less than the critical average grain size (dav)cr. In our opinion, for the investigated alloy (dav)cr ≈ 0.5 µm. In our study, the attained average grain size is larger the critical one. The main idea of the mechanism is next. In alloys with an average grain size (dav) less than the critical one, a higher external stress is required for the nucleation and propagation of the main crack.
Open AccessEffect of True Strains in Isothermal abc Pressing on Mechanical Properties of Ti49.8Ni50.2 Alloy
The paper analyzes the microstructure and mechanical properties of Ti49.8Ni50.2 alloy (at.%) under uniaxial tension at room temperature after isothermal abc pressing to true strains e = 0.29 − 8.44 at T = 723 K. The analysis shows that as the true strain e is increased, the grain–subgrain structure of the alloy is gradually refined. This leads to an increase in its yield stress σy and strain hardening coefficient θ = dσ/dε at linear stage III of its tensile stress–strain curve according to the Hall–Petch relation. However, the ultimate tensile strength remains invariant to such refinement. The possible mechanism is proposed to explain why the ultimate tensile strength can remain invariant to the average grains size (dav). It is assumed that the sharp increase of the ultimate tensile strength σUTS begins when (dav) is less than the critical average grain size (dav)cr. In our opinion, for the investigated alloy (dav)cr ≈ 0.5 µm. In our study, the attained average grain size is larger the critical one. The main idea of the mechanism is next. In alloys with an average grain size (dav) less than the critical one, a higher external stress is required for the nucleation and propagation of the main crack.