Said Nategh
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Said Nategh has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Arman Rabieifar
Department of Materials Engineering, Faculty of Engineering, Karaj Branch, Islamic Azad University, Karaj, Iran
5 shared publications - Hamidreza Najafi
Department of Materials Engineering, Faculty of Engineering, Science and Research Branch, Islamic Azad University, Tehran, Iran
4 shared publications - Mohammadreza Afshar
Department of Materials Engineering, Faculty of Engineering, Science and Research Branch, Islamic Azad University, Tehran, Iran
4 shared publications Alireza Khodabandeh
Department of Materials Engineering, Science and Research Branch, Islamic Azad University, Tehran, Iran
1 shared publicationHamed Kaypour
Department of Materials Engineering, Science and Research Branch, Islamic Azad University, Tehran, Iran
1 shared publicationHamidreza Najafi
1 shared publication
Latest Publications
- 5 September 2025
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 14 (5) , 1084-1113
The Effect of Cyclic Hot Corrosion of High-Activity Low-Temperature Pt-Al-7YSZ Coating on Tensile Properties of Gas Turbine Second-Row Blades at 870 °C
- 5 September 2025
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 14 (5) , 1084-1113
The Effect of Cyclic Hot Corrosion of High-Activity Low-Temperature Pt-Al-7YSZ Coating on Tensile Properties of Gas Turbine Second-Row Blades at 870 °C
- 6 October 2021
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
- Vol. 57 (1) , 55-65
The evaluation of oxide scale formation during hot corrosion of Rene-80 superalloy under thermal shock at different dwell times
In this study, the oxide scale formation on the Rene-80 superalloy after hot corrosion under thermal shock has been investigated. The X-ray diffraction (XRD) and field-emission scanning electron microscope (FE-SEM) were used for the phase identification and evaluation of oxide scale, respectively. The hot corrosion test under thermal shock was performed by depositing Na2SO4 salt at the beginning of each cycle on the surface of the specimens. The results showed that hot corrosion occurred intermittently with the basic fluxing mechanism of the oxide scale and re-precipitation of discontinuous and porous oxides. The growth rate of the Cr2O3 layer increased with decreasing the dwell time per cycle and the dissolution of titanium. Decreasing the dwell time in each hot corrosion cycle increased the growth rate of the Cr2O3 layer, the chromium depletion from the substrate/oxide scale interface, the internal oxidation of aluminium, and the internal sulfidation of chromium.
- 6 October 2021
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
- Vol. 57 (1) , 55-65
The evaluation of oxide scale formation during hot corrosion of Rene-80 superalloy under thermal shock at different dwell times
In this study, the oxide scale formation on the Rene-80 superalloy after hot corrosion under thermal shock has been investigated. The X-ray diffraction (XRD) and field-emission scanning electron microscope (FE-SEM) were used for the phase identification and evaluation of oxide scale, respectively. The hot corrosion test under thermal shock was performed by depositing Na2SO4 salt at the beginning of each cycle on the surface of the specimens. The results showed that hot corrosion occurred intermittently with the basic fluxing mechanism of the oxide scale and re-precipitation of discontinuous and porous oxides. The growth rate of the Cr2O3 layer increased with decreasing the dwell time per cycle and the dissolution of titanium. Decreasing the dwell time in each hot corrosion cycle increased the growth rate of the Cr2O3 layer, the chromium depletion from the substrate/oxide scale interface, the internal oxidation of aluminium, and the internal sulfidation of chromium.
- Open Access
- 1 June 2021
- Published by IOP Publishing in Materials Research Express
- Vol. 8 (6) , 066505
High-temperature compressive behavior and kinetics analysis of Al0.4MnCrCoFeNi high entropy alloy
In the present study, AlxMnCrCoFeNi alloys (x = 0, 0.4) were produced by vacuum melting and casting. For this aim, ingots were subjected to the homogenization, cold roll, and annealing. X-ray diffraction analysis and SEM images indicated that the crystal structure is FCC solid solution for MnCrCoFeNi. Moreover, in addition to FCC solid solution, the alloy with aluminum (x = 0.4) ordered B2 precipitates. Besides, hot compressive tests were conducted at different temperatures and strain rates of 0.01, 0.05 and 0.1/s. Investigating the stress-strain diagrams and work hardening rate, it was revealed that twins played a role in the deformation mechanism. In the constitutive equation, the values of the stress exponent and activation energy were measured and they were 6.86 and 434 kJ mol−1, respectively. The exponential equations of peak stress and peak strain, as well as steady-state stress, were obtained due to the Zener-Hollomon parameter. Regarding the linear relationship between the work hardening rate and the dislocation annihilation coefficients, the activation energy of deformation changes at 600 °C. Finally, another effect of the Al addition was shown to be increase in initiation temperature of necklace structure about 200 °C in hot compression test. In addition, B2 nanoprecipitate and nanotwins indicated that there was twin deformation mechanism in alloy containing Al.
- 1 June 2021
- Published by IOP Publishing in Materials Research Express
- Vol. 8 (6) , 066505
Open AccessHigh-temperature compressive behavior and kinetics analysis of Al0.4MnCrCoFeNi high entropy alloy
In the present study, AlxMnCrCoFeNi alloys (x = 0, 0.4) were produced by vacuum melting and casting. For this aim, ingots were subjected to the homogenization, cold roll, and annealing. X-ray diffraction analysis and SEM images indicated that the crystal structure is FCC solid solution for MnCrCoFeNi. Moreover, in addition to FCC solid solution, the alloy with aluminum (x = 0.4) ordered B2 precipitates. Besides, hot compressive tests were conducted at different temperatures and strain rates of 0.01, 0.05 and 0.1/s. Investigating the stress-strain diagrams and work hardening rate, it was revealed that twins played a role in the deformation mechanism. In the constitutive equation, the values of the stress exponent and activation energy were measured and they were 6.86 and 434 kJ mol−1, respectively. The exponential equations of peak stress and peak strain, as well as steady-state stress, were obtained due to the Zener-Hollomon parameter. Regarding the linear relationship between the work hardening rate and the dislocation annihilation coefficients, the activation energy of deformation changes at 600 °C. Finally, another effect of the Al addition was shown to be increase in initiation temperature of necklace structure about 200 °C in hot compression test. In addition, B2 nanoprecipitate and nanotwins indicated that there was twin deformation mechanism in alloy containing Al.
- 9 November 2020
- Published by Springer Nature in Oxidation of Metals
- Vol. 94 (5-6) , 549-567
The Cyclic Hot Corrosion Behavior of Pt–Al–7%YSZ Coating
- 9 November 2020
- Published by Springer Nature in Oxidation of Metals
- Vol. 94 (5-6) , 549-567
The Cyclic Hot Corrosion Behavior of Pt–Al–7%YSZ Coating
- Open Access
- 1 January 2020
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (1) , 016575
Microstructural evolution and cyclic oxidation of Pt-Al-YSZ coating under thermal shock
In this research, the effect of thermal shock has been investigated on the microstructure and cyclic oxidation of Pt-Al-7%YSZ coating applied on Rene-80 superalloy. The microstructural evaluation and phase identification were performed by field emission scanning electron microscope (FE-SEM) and X-ray diffraction (XRD). The thermal shock test consisted of repeated cycles of rapid cooling between 900 °C and 400 °C. Prior to the thermal shock test, the specimen coated by Pt-electroplating, high-activity low-temperature (HALT) aluminizing and the thermal spray of YSZ ceramic layer. From surface towards the substrate; the coating consisted of 5 layers including: 7% YSZ, PtAl2 + β-(Ni,Pt)Al, β-(Ni,Pt)Al with fine precipitates rich in α-(Cr) and α-(W), precipitate-free β-NiAl, and inter-diffusion zone next to the specimen surface. After the thermal shock test, spallation and delamination have been observed in the YSZ layer. The Pt-Al layer was found in upper and lower parts of the coating with different Pt concentration. Also, the chemical composition of the Pt-Al layer demonstrated the removal of PtAl2 particles and β transformation to both γ and γ′ phases. Degradation of Pt-Al layer occurred by ratcheting the thermally grown oxide (TGO), rumpling, and cavitation. Comparison of weight changes showed that the thermal shock resistance is improved by Pt-Al-7% YSZ coating.
- 1 January 2020
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (1) , 016575
Open AccessMicrostructural evolution and cyclic oxidation of Pt-Al-YSZ coating under thermal shock
In this research, the effect of thermal shock has been investigated on the microstructure and cyclic oxidation of Pt-Al-7%YSZ coating applied on Rene-80 superalloy. The microstructural evaluation and phase identification were performed by field emission scanning electron microscope (FE-SEM) and X-ray diffraction (XRD). The thermal shock test consisted of repeated cycles of rapid cooling between 900 °C and 400 °C. Prior to the thermal shock test, the specimen coated by Pt-electroplating, high-activity low-temperature (HALT) aluminizing and the thermal spray of YSZ ceramic layer. From surface towards the substrate; the coating consisted of 5 layers including: 7% YSZ, PtAl2 + β-(Ni,Pt)Al, β-(Ni,Pt)Al with fine precipitates rich in α-(Cr) and α-(W), precipitate-free β-NiAl, and inter-diffusion zone next to the specimen surface. After the thermal shock test, spallation and delamination have been observed in the YSZ layer. The Pt-Al layer was found in upper and lower parts of the coating with different Pt concentration. Also, the chemical composition of the Pt-Al layer demonstrated the removal of PtAl2 particles and β transformation to both γ and γ′ phases. Degradation of Pt-Al layer occurred by ratcheting the thermally grown oxide (TGO), rumpling, and cavitation. Comparison of weight changes showed that the thermal shock resistance is improved by Pt-Al-7% YSZ coating.