Safiye İpEk Ayvaz
Research Subjects
Safiye İpEk Ayvaz has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Emre Özer
Osmaniye Korkut Ata University, Faculty of Engineering, Department of Industrial Engineering
2 shared publications Ali İhSan Bahçepınar
1 shared publication- Demet Zalaoğlu
Department of Mechanical Engineering, Osmaniye Korkut Ata University, Osmaniye 80000, Turkey
1 shared publication - Dilek Arslan
Manisa Celal Bayar Üniversitesi
1 shared publication Ibrahim Aydin
Vocational School of Manisa Technical Sciences, Celal Bayar University, Manisa, Turkey
1 shared publication- Ibrahim Fadil Soykok
Manisa Celal Bayar Üniversitesi
1 shared publication
Latest Publications
- 30 June 2026
- Published by Celal Bayar University Journal of Science in Celal Bayar Üniversitesi Fen Bilimleri Dergisi
- Vol. 22 (2) , 372-382
The Effect of Pass Number on the Wear Properties of AA5754-SiC Surface Composites Produced by Friction Stir Processing
In this study, AA5754 matrix SiC-reinforced surface composites were produced using the friction stir technique to improve their microstructural properties, wear resistance, and surface hardness. The effect of the number of passes on these properties was also investigated. Homogeneous particle distribution could not be achieved with single-pass production. Production with two and three passes using the friction stir technique was successfully achieved. The surface hardness of these SiC-reinforced surface composites showed an increase of 16% and 22%, respectively, compared to the AA5754 aluminum alloy. The wear resistance of the AA5754 aluminum alloy increased by 34.2% and 45.9%, respectively, with the production of SiC-reinforced surface composites in two and three passes.
- 30 June 2026
- Published by Celal Bayar University Journal of Science in Celal Bayar Üniversitesi Fen Bilimleri Dergisi
- Vol. 22 (2) , 372-382
The Effect of Pass Number on the Wear Properties of AA5754-SiC Surface Composites Produced by Friction Stir Processing
In this study, AA5754 matrix SiC-reinforced surface composites were produced using the friction stir technique to improve their microstructural properties, wear resistance, and surface hardness. The effect of the number of passes on these properties was also investigated. Homogeneous particle distribution could not be achieved with single-pass production. Production with two and three passes using the friction stir technique was successfully achieved. The surface hardness of these SiC-reinforced surface composites showed an increase of 16% and 22%, respectively, compared to the AA5754 aluminum alloy. The wear resistance of the AA5754 aluminum alloy increased by 34.2% and 45.9%, respectively, with the production of SiC-reinforced surface composites in two and three passes.
- Open Access
- 20 August 2024
- Published by International Advanced Researches and Engineering Journal in International Advanced Researches and Engineering Journal
- Vol. 8 (2) , 76-83
Influences of post-weld artificial aging on microstructural and tensile properties of friction stir-welded Al-Zn-Mg-Si-Cu aluminum alloy joints
In this study, the effect of heat treatment on the mechanical and microstructural properties of welded joints after friction stir welding of age-hardenable Al-Zn-Mg-Si-Cu wrought aluminum alloy plates was investigated. For this purpose, some of the samples welded using FSW technique with a rotational speed of 1250 rpm and a traverse speed of 40 mm·min-1 were subjected to annealing and some to artificial aging heat treatment at different temperatures and times. In FSWed artificial aged samples where AlFeSi precipitate formations were detected, hardness and strength increase were realized with grain-boundary strengthening and Orowan hardening mechanisms. The lowest ultimate tensile strength was 156.3 N·mm-2 in the annealed sample, while the highest ultimate tensile strength was 210.8 N·mm-2 in the sample artificially aged at 190 °C for 2 hours. Fractographic examination revealed that ductile fracture occurred in all specimens.
- 20 August 2024
- Published by International Advanced Researches and Engineering Journal in International Advanced Researches and Engineering Journal
- Vol. 8 (2) , 76-83
Open AccessInfluences of post-weld artificial aging on microstructural and tensile properties of friction stir-welded Al-Zn-Mg-Si-Cu aluminum alloy joints
In this study, the effect of heat treatment on the mechanical and microstructural properties of welded joints after friction stir welding of age-hardenable Al-Zn-Mg-Si-Cu wrought aluminum alloy plates was investigated. For this purpose, some of the samples welded using FSW technique with a rotational speed of 1250 rpm and a traverse speed of 40 mm·min-1 were subjected to annealing and some to artificial aging heat treatment at different temperatures and times. In FSWed artificial aged samples where AlFeSi precipitate formations were detected, hardness and strength increase were realized with grain-boundary strengthening and Orowan hardening mechanisms. The lowest ultimate tensile strength was 156.3 N·mm-2 in the annealed sample, while the highest ultimate tensile strength was 210.8 N·mm-2 in the sample artificially aged at 190 °C for 2 hours. Fractographic examination revealed that ductile fracture occurred in all specimens.
- 1 March 2024
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 65 (11-12) , 751-757
Growth Kinetics and Microstructure of Iron Boride Layers on AISI 1050 Steel
- 1 March 2024
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 65 (11-12) , 751-757
Growth Kinetics and Microstructure of Iron Boride Layers on AISI 1050 Steel
- 10 December 2023
- Published by Folium Publishing Company in Металловедение и термическая обработка металлов
- No. 12,p. 18-24
Growth kinetics and microstructure of iron boride layers on AISI 1050 steel
Исследована кинетика диффузии бора в стали AISI 1050 (сталь 50). Проведено борирование стали в течение 2, 4 и 6 ч при 850, 900 и 950 °C с использованием порошка Экабор-II (Ekabor-II) методом пакетного борирования. На поверхности образцов получены боридные слои FeB/Fe2B толщиной 25,4 – 118,9 мкм. Сформированные боридные слои имеют типичную зубчатую морфологию и твердость 1071 – 1460 HV0,1. Рассчитанные по результатам диффузионно-кинетических исследований константы скорости роста боридного слоя для стали AISI 1050 при температурах борирования 850, 900 и 950 °C составляют 1,522 ' 10 – 12; 2,964 ' 10 – 13 и 6,354 ' 10 – 12 м2 ' с – 1 соответственно. Определена энергия активации диффузии бора в стали AISI 1050, равная 162,93 кДж ' моль – 1.
- 10 December 2023
- Published by Folium Publishing Company in Металловедение и термическая обработка металлов
- No. 12,p. 18-24
Growth kinetics and microstructure of iron boride layers on AISI 1050 steel
Исследована кинетика диффузии бора в стали AISI 1050 (сталь 50). Проведено борирование стали в течение 2, 4 и 6 ч при 850, 900 и 950 °C с использованием порошка Экабор-II (Ekabor-II) методом пакетного борирования. На поверхности образцов получены боридные слои FeB/Fe2B толщиной 25,4 – 118,9 мкм. Сформированные боридные слои имеют типичную зубчатую морфологию и твердость 1071 – 1460 HV0,1. Рассчитанные по результатам диффузионно-кинетических исследований константы скорости роста боридного слоя для стали AISI 1050 при температурах борирования 850, 900 и 950 °C составляют 1,522 ' 10 – 12; 2,964 ' 10 – 13 и 6,354 ' 10 – 12 м2 ' с – 1 соответственно. Определена энергия активации диффузии бора в стали AISI 1050, равная 162,93 кДж ' моль – 1.
- Open Access
- 12 May 2023
- Published by University North in Tehnički glasnik
- Vol. 17 (2) , 286-292
Comparative Study of Conventional and Microwave-Assisted Boriding of AISI 1040 and AISI 4140 Steels
In this study, AISI 1040 and AISI 4140 steels were boriding using Ekabor-II commercial boriding powder with powder-pack boriding method using microwave and conventional heating methods. The samples were borided at 950 °C for 2 and 6 hours in an Ar atmosphere in a microwave oven of Enerzi-Mh2912-V8. Biphasic structure (FeB/Fe2B) was formed in all borided AISI 4140 samples and AISI 1040 samples borided for 6 hours. A single-phase structure was observed in AISI 1040 steel borided for 2 hours. Compared to the conventional method, a 1.5-1.6 times thicker boride layer was obtained in AISI 4140 and AISI 1040 steels with microwave-assisted powder-pack boriding. The highest hardness was measured as 1561.8 HV0.05 for boriding AISI 4140 steel and 1499.7 HV0.05 for boriding AISI 1040 steel. The Vickers indentation fracture toughness of borided steels with microwave energy varied between 2.31 and 3.46 MPa·m1/2. It was determined that in all samples borided by the microwave-assisted and conventional powder-pack boriding method, the adhesion strength between the boride layers and the substrate obtained was sufficient.
- 12 May 2023
- Published by University North in Tehnički glasnik
- Vol. 17 (2) , 286-292
Open AccessComparative Study of Conventional and Microwave-Assisted Boriding of AISI 1040 and AISI 4140 Steels
In this study, AISI 1040 and AISI 4140 steels were boriding using Ekabor-II commercial boriding powder with powder-pack boriding method using microwave and conventional heating methods. The samples were borided at 950 °C for 2 and 6 hours in an Ar atmosphere in a microwave oven of Enerzi-Mh2912-V8. Biphasic structure (FeB/Fe2B) was formed in all borided AISI 4140 samples and AISI 1040 samples borided for 6 hours. A single-phase structure was observed in AISI 1040 steel borided for 2 hours. Compared to the conventional method, a 1.5-1.6 times thicker boride layer was obtained in AISI 4140 and AISI 1040 steels with microwave-assisted powder-pack boriding. The highest hardness was measured as 1561.8 HV0.05 for boriding AISI 4140 steel and 1499.7 HV0.05 for boriding AISI 1040 steel. The Vickers indentation fracture toughness of borided steels with microwave energy varied between 2.31 and 3.46 MPa·m1/2. It was determined that in all samples borided by the microwave-assisted and conventional powder-pack boriding method, the adhesion strength between the boride layers and the substrate obtained was sufficient.
- Open Access
- 15 April 2023
- Published by International Advanced Researches and Engineering Journal in International Advanced Researches and Engineering Journal
- Vol. 7 (1) , 1-7
Investigation of the effect of boriding on the wear behaviour of AISI 1050 carbon steel
In this study, AISI 1050 carbon steel samples were boronized with the powder pack boriding technique at 875°C for 2, 4 and 6 hours using Ekabor 2 boriding powder. The boride layer thicknesses obtained with the boriding time increased and after 2, 4 and 6 hours of boriding, a 30.6, 40.0 and 71.8 µm boride layer, predominantly composed of Fe2B phase, was obtained. Boride layers were formed in tooth-like morphology. Thanks to this boride layer, the surface hardness of the substrate was improved 6.2-6.4 times and a maximum surface hardness of 1543.8 HV was reached. With the Daimler-Benz Rockwell-C adhesion tests, it was determined that the adhesion quality of the boride layer was generally at the HF1 level. With the boriding carried out, the specific wear loss of AISI 1050 steel was reduced from 421.25 mm3/Nm x10-6 to 17.67 mm3/Nm x10-6, and the wear resistance was increased approximately 24 times.
- 15 April 2023
- Published by International Advanced Researches and Engineering Journal in International Advanced Researches and Engineering Journal
- Vol. 7 (1) , 1-7
Open AccessInvestigation of the effect of boriding on the wear behaviour of AISI 1050 carbon steel
In this study, AISI 1050 carbon steel samples were boronized with the powder pack boriding technique at 875°C for 2, 4 and 6 hours using Ekabor 2 boriding powder. The boride layer thicknesses obtained with the boriding time increased and after 2, 4 and 6 hours of boriding, a 30.6, 40.0 and 71.8 µm boride layer, predominantly composed of Fe2B phase, was obtained. Boride layers were formed in tooth-like morphology. Thanks to this boride layer, the surface hardness of the substrate was improved 6.2-6.4 times and a maximum surface hardness of 1543.8 HV was reached. With the Daimler-Benz Rockwell-C adhesion tests, it was determined that the adhesion quality of the boride layer was generally at the HF1 level. With the boriding carried out, the specific wear loss of AISI 1050 steel was reduced from 421.25 mm3/Nm x10-6 to 17.67 mm3/Nm x10-6, and the wear resistance was increased approximately 24 times.
- 1 February 2023
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 65 (2) , 279-290
Enhancing the wear performance of Ti-6Al-4V against Al2O3 and WC-6Co via TiBn layer produced by boriding
In this study, mechanical and tribological properties of the borided dual-phase α + β type Ti6Al4V titanium alloy were examined. For this purpose, Ti6Al4V alloy samples were borided for 6 h at a temperature of 1100 °C by the powder-pack boriding process. As a result of boriding, a boride layer consisting of TiB2 with a thickness of max ∼25 µm and TiB phases with a thickness of max ∼10 µm was obtained on the Ti6Al4V sample surfaces. As a result of the boride layer’s nanoindentation tests carried out using the Berkovich indenter, it was found to have an elastic modulus of 534.255 GPa and a hardness of 36.537 GPa. Wear tests were carried out using the pin-on-disc method under a load of 10 N and with a sliding distance of 1000 m. Whereas the dominant type of wear in non-borided samples was abrasive wear, oxidative mild wear was generally observed in borided samples. In borided samples, as a result of becoming of surface smoother by hard asperities breaking and increasing the actual contact area, the friction coefficients increased. It was determined that with boriding, the wear performance of Ti6Al4V alloy improved ∼46.8 times against the Al2O3 counterpart and ∼4.57 times against WC-6Co counterpart.
- 1 February 2023
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 65 (2) , 279-290
Enhancing the wear performance of Ti-6Al-4V against Al2O3 and WC-6Co via TiBn layer produced by boriding
In this study, mechanical and tribological properties of the borided dual-phase α + β type Ti6Al4V titanium alloy were examined. For this purpose, Ti6Al4V alloy samples were borided for 6 h at a temperature of 1100 °C by the powder-pack boriding process. As a result of boriding, a boride layer consisting of TiB2 with a thickness of max ∼25 µm and TiB phases with a thickness of max ∼10 µm was obtained on the Ti6Al4V sample surfaces. As a result of the boride layer’s nanoindentation tests carried out using the Berkovich indenter, it was found to have an elastic modulus of 534.255 GPa and a hardness of 36.537 GPa. Wear tests were carried out using the pin-on-disc method under a load of 10 N and with a sliding distance of 1000 m. Whereas the dominant type of wear in non-borided samples was abrasive wear, oxidative mild wear was generally observed in borided samples. In borided samples, as a result of becoming of surface smoother by hard asperities breaking and increasing the actual contact area, the friction coefficients increased. It was determined that with boriding, the wear performance of Ti6Al4V alloy improved ∼46.8 times against the Al2O3 counterpart and ∼4.57 times against WC-6Co counterpart.
- 1 February 2022
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 64 (2) , 249-259
Tribological and adhesion properties of microwave-assisted borided AISI 316L steel
In this study, AISI 316L stainless steel alloy samples were borided with powder-pack boriding method using Ekabor II powder with the support of a microwave furnace with a power of 2.9 KW and a frequency of 2.45 GHz. Boriding was carried out at 850, 900 and 950 °C temperatures for 2, 4 and 6 h of operation. A distinct diffusion barrier consisting of Fe–Ni–Si elements was detected in borided samples at 950 °C for 4 and 6 h. As a result of the Daimler Benz Rockwell-C adhesion tests, regions with insufficient adhesion strength were detected in these samples. In other samples, adhesion qualities between boride layers and substrate were in the range of HF1–HF3. The lowest specific wear rates were determined as 5.208 (mm3 Nm−1) × 10−6 and 5.210 (mm3 Nm−1) × 10−6 for the samples borided for 6 h at 850 °C and 4 h at 900 °C, respectively. It was determined that the increase in thickness of the brittle FeB compound increased the wear with the three-body abrasive wear mechanism.
- 1 February 2022
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 64 (2) , 249-259
Tribological and adhesion properties of microwave-assisted borided AISI 316L steel
In this study, AISI 316L stainless steel alloy samples were borided with powder-pack boriding method using Ekabor II powder with the support of a microwave furnace with a power of 2.9 KW and a frequency of 2.45 GHz. Boriding was carried out at 850, 900 and 950 °C temperatures for 2, 4 and 6 h of operation. A distinct diffusion barrier consisting of Fe–Ni–Si elements was detected in borided samples at 950 °C for 4 and 6 h. As a result of the Daimler Benz Rockwell-C adhesion tests, regions with insufficient adhesion strength were detected in these samples. In other samples, adhesion qualities between boride layers and substrate were in the range of HF1–HF3. The lowest specific wear rates were determined as 5.208 (mm3 Nm−1) × 10−6 and 5.210 (mm3 Nm−1) × 10−6 for the samples borided for 6 h at 850 °C and 4 h at 900 °C, respectively. It was determined that the increase in thickness of the brittle FeB compound increased the wear with the three-body abrasive wear mechanism.
- 23 August 2021
- Published by Izmir UOD
Investigation of the Wear Behavior of AA6082 Against Different Counterparts
In this study, the effect of different counterparts on the wear resistance of AA6082 aluminum alloy was investigated. In tests using pin-on-disk method, 6 mm diameter Al2O3, 100Cr6 and WC-6Co balls were used as counterparts. The tests were carried out using 500 m sliding distance and 5N load. The lowest specific wear rate was measured as 7.58x10-4 mm3/Nm in WC-6Co / AA6082 couple, and the highest value was measured as 9.71x10-4 mm3/Nm in 100Cr6/AA6082 couple. In the Al2O3/AA6082 couple, the specific wear rate of the AA6082-T6 sample was determined as 8.23x10-4 mm3/Nm. While it was observed that the dominant wear type in the 100Cr6/AA6082 pair was abrasive wear, oxidation wear and oxide tribofilm were detected in the WC-6Co/AA6082 and Al2O3/AA6082 couple besides the abrasive wear.
- 23 August 2021
- Published by Izmir UOD
Investigation of the Wear Behavior of AA6082 Against Different Counterparts
In this study, the effect of different counterparts on the wear resistance of AA6082 aluminum alloy was investigated. In tests using pin-on-disk method, 6 mm diameter Al2O3, 100Cr6 and WC-6Co balls were used as counterparts. The tests were carried out using 500 m sliding distance and 5N load. The lowest specific wear rate was measured as 7.58x10-4 mm3/Nm in WC-6Co / AA6082 couple, and the highest value was measured as 9.71x10-4 mm3/Nm in 100Cr6/AA6082 couple. In the Al2O3/AA6082 couple, the specific wear rate of the AA6082-T6 sample was determined as 8.23x10-4 mm3/Nm. While it was observed that the dominant wear type in the 100Cr6/AA6082 pair was abrasive wear, oxidation wear and oxide tribofilm were detected in the WC-6Co/AA6082 and Al2O3/AA6082 couple besides the abrasive wear.