Konstantin V. Grigorovich
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Konstantin V. Grigorovich has a total of 113 co-authors. Here are the top co-authors by number of shared publications:
- O. A. Komolova
Baikov Institute of Metallurgy and Materials Science of the Russian Academy of Sciences
6 shared publications - A. Yu. Em
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences
5 shared publications - A. O. Morozov
Baikov Institute of Metallurgy and Materials Science of the Russian Academy of Sciences
4 shared publications - A. A. Zhemkov
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences
2 shared publications - A. G. Kanevskiy
Baikov Institute of Metallurgy and Materials Science of the Russian Academy of Sciences
2 shared publications A. K. Garber
Russian Academy of Sciences
2 shared publications
Latest Publications
- 1 November 2026
- Published by Autonomous Non-profit Organization Editorial Board of the journal Uspekhi Khimii in Russian Chemical Reviews
- Vol. 95 (11) , RCR5247
Artificial Intelligence in the Preparation of Scientific Articles
The use of artificial intelligence (AI) tools in the preparation of scientific publications has become an integral part of research practice. Large language models assist in translating and editing texts, structuring articles, drafting abstracts, adapting manuscripts to journal requirements, and accelerating preliminary literature reviews, among other useful functions. However, the technical utility of the tool does not alter the fundamental principle: a scientific article remains the product of a researcher's work, for which they bear responsibility. AI cannot be recognized as a co-author, nor can it be held accountable for data authenticity, the correctness of chemical nomenclature, the logic of the presentation, the completeness of citations, or the validity of conclusions. This article presents the position of Editors-in-Chief and Editorial Board members from several Russian chemistry journals regarding the use of AI in preparing scientific publications. To practically regulate the use of AI in scientific article preparation, the VALENCE set of rules is proposed, in alignment with international publishing practices. Bibliography includes 42 references.
- 1 November 2026
- Published by Autonomous Non-profit Organization Editorial Board of the journal Uspekhi Khimii in Russian Chemical Reviews
- Vol. 95 (11) , RCR5247
Artificial Intelligence in the Preparation of Scientific Articles
The use of artificial intelligence (AI) tools in the preparation of scientific publications has become an integral part of research practice. Large language models assist in translating and editing texts, structuring articles, drafting abstracts, adapting manuscripts to journal requirements, and accelerating preliminary literature reviews, among other useful functions. However, the technical utility of the tool does not alter the fundamental principle: a scientific article remains the product of a researcher's work, for which they bear responsibility. AI cannot be recognized as a co-author, nor can it be held accountable for data authenticity, the correctness of chemical nomenclature, the logic of the presentation, the completeness of citations, or the validity of conclusions. This article presents the position of Editors-in-Chief and Editorial Board members from several Russian chemistry journals regarding the use of AI in preparing scientific publications. To practically regulate the use of AI in scientific article preparation, the VALENCE set of rules is proposed, in alignment with international publishing practices. Bibliography includes 42 references.
- Open Access
- 28 October 2026
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 69 (5) , 466-474
Interaction of refractory MgO-based ceramics with iron-carbon melt
The authors used the sessile drop method to study the interaction of rail-steel melt with MgO-based ceramics in He + 10 % H 2 at different temperatures (isothermal holding at 1743 and 1973 K). It was shown that, after experiments, carbon and manganese concentrations decreased and silicon and chromium contents increased. At the high-temperature holding (1973 K), carbon concentration in the metal increased at an order of magnitude, which indicated its intense interaction with oxides of ceramics, reduction of the elements from oxides and their transition to the melt. The contact angles decreased from 135 to about 123° in the first 15 min of the experiment with the subsequent increase to 136° or the decrease to 114° depending on the temperature conditions. The structure and the elemental mapping of the boundaries of transverse sections of the metal and ceramics were analyzed. In the metal-ceramics contact zone, in the bonding phase, a new phase was formed which corresponded to merwinite (Ca 3 MgSi 2 O 8 ). This can be related to a change in silicon concentration due to its interaction with carbon dissolved in the metal. An increase in the total oxygen concentration in the metal after experiments was observed, which can be related to the transition of oxide particles from the ceramics into the melt. Analysis of non-metallic inclusions showed that, after the low-temperature holding (1743 K), complex magnesium-containing inclusions prevail and, after the high-temperature holding (1973 K), aluminum- and silicon-containing inclusions are mainly observed.
- 28 October 2026
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 69 (5) , 466-474
Open AccessInteraction of refractory MgO-based ceramics with iron-carbon melt
The authors used the sessile drop method to study the interaction of rail-steel melt with MgO-based ceramics in He + 10 % H 2 at different temperatures (isothermal holding at 1743 and 1973 K). It was shown that, after experiments, carbon and manganese concentrations decreased and silicon and chromium contents increased. At the high-temperature holding (1973 K), carbon concentration in the metal increased at an order of magnitude, which indicated its intense interaction with oxides of ceramics, reduction of the elements from oxides and their transition to the melt. The contact angles decreased from 135 to about 123° in the first 15 min of the experiment with the subsequent increase to 136° or the decrease to 114° depending on the temperature conditions. The structure and the elemental mapping of the boundaries of transverse sections of the metal and ceramics were analyzed. In the metal-ceramics contact zone, in the bonding phase, a new phase was formed which corresponded to merwinite (Ca 3 MgSi 2 O 8 ). This can be related to a change in silicon concentration due to its interaction with carbon dissolved in the metal. An increase in the total oxygen concentration in the metal after experiments was observed, which can be related to the transition of oxide particles from the ceramics into the melt. Analysis of non-metallic inclusions showed that, after the low-temperature holding (1743 K), complex magnesium-containing inclusions prevail and, after the high-temperature holding (1973 K), aluminum- and silicon-containing inclusions are mainly observed.
- Open Access
- 28 October 2026
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 69 (5) , 457-465
Analysis of ladle processing technologies for IF steel
Three different IF steel production technologies at metallurgical plants were analyzed and compared. Using process logs of completed smelts, changes in the carbon, nitrogen, and oxygen contents of the metal during ladle processing were compared, as well as the contents of various types of oxide nonmetallic inclusions in the analyzed metal samples collected at different sections of the steel ladle processing. The comparison revealed that the technologies at the plants differed in ladle weights, different types of vacuum degassers, different alloying and deoxidation schemes, types of introduced additives, and different ladle movement logistics between ladle metal processing units during IF steel production. The initial concentrations of dissolved carbon, nitrogen, and oxygen in the steel melt before vacuum processing also differ significantly. Metal samples collected at various stages of IF steel production were analyzed. As a result of the study of metal samples taken during the ladle treatment and casting stages of IF steel, using scanning electron microscopy (SEM) and fractional gas analysis (FGA), the main types of nonmetallic inclusions in the steel were quantitatively determined, as well as the total content of oxygen and nitrogen in the metal, respectively. The paper describes the dynamics of changes in various types of nonmetallic inclusions in metal samples during ladle processing after vacuum decarburization and IF steel casting.
- 28 October 2026
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 69 (5) , 457-465
Open AccessAnalysis of ladle processing technologies for IF steel
Three different IF steel production technologies at metallurgical plants were analyzed and compared. Using process logs of completed smelts, changes in the carbon, nitrogen, and oxygen contents of the metal during ladle processing were compared, as well as the contents of various types of oxide nonmetallic inclusions in the analyzed metal samples collected at different sections of the steel ladle processing. The comparison revealed that the technologies at the plants differed in ladle weights, different types of vacuum degassers, different alloying and deoxidation schemes, types of introduced additives, and different ladle movement logistics between ladle metal processing units during IF steel production. The initial concentrations of dissolved carbon, nitrogen, and oxygen in the steel melt before vacuum processing also differ significantly. Metal samples collected at various stages of IF steel production were analyzed. As a result of the study of metal samples taken during the ladle treatment and casting stages of IF steel, using scanning electron microscopy (SEM) and fractional gas analysis (FGA), the main types of nonmetallic inclusions in the steel were quantitatively determined, as well as the total content of oxygen and nitrogen in the metal, respectively. The paper describes the dynamics of changes in various types of nonmetallic inclusions in metal samples during ladle processing after vacuum decarburization and IF steel casting.
- 26 April 2026
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 69 (2)
Evolution of oxide non-metallic inclusions in production of pipe steel
Under the conditions of pipe rolling mill, during the production of 12 heats of medium-carbon aluminum-killed steel, 10 samples were taken from each heat at different stages of production – from the beginning of ladle treatment to pipe rolling. The samples were examined by high-temperature extraction in a carrier gas to determine the total oxygen content and by scanning electron microscopy to determine the composition and size distribution of non-metallic inclusions. The dynamics of change in the content of inclusions was established according to the following criteria: total oxygen content, volume fraction, density and average diameter of inclusions. The composition of non-metallic inclusions was plotted on ternary diagrams: the oxide component on the diagrams CaO – Al 2 O 3 – SiO 2 and CaO – Al 2 O 3 – MgO, the sulfide – on Ca – Mn – S. The trajectory of change in the chemical composition of inclusions in the steelmaking process was established. The paper shows the role of steel treatment with calcium and importance of observing thermodynamic conditions. A relationship is established between deviations in calcium treatment parameters, composition of non-metallic inclusions, steel castability and sorting of pipe products by surface and internal defects. Decreasing total oxygen content, practically does not occur at the main stage of ladle treatment. The highest intensity of steel refining from inclusions is observed at the stage between the samples before and after steel treatment with calcium, this time interval is less than 10 min. Comparison of the obtained data on the chemical composition of inclusions with the calculated data on the boundary of liquid phase region of the CaO – Al 2 O 3 – SiO 2 – MgO system shows that at this stage, the chemical and phase composition of non-metallic inclusions is transformed. After the addition of calcium, the composition of oxide non-metallic inclusions shifted to the liquid region of the CaO – Al 2 O 3 – SiO 2 system at MgO content of 10 wt. % and 1600 °C.
- 26 April 2026
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 69 (2)
Evolution of oxide non-metallic inclusions in production of pipe steel
Under the conditions of pipe rolling mill, during the production of 12 heats of medium-carbon aluminum-killed steel, 10 samples were taken from each heat at different stages of production – from the beginning of ladle treatment to pipe rolling. The samples were examined by high-temperature extraction in a carrier gas to determine the total oxygen content and by scanning electron microscopy to determine the composition and size distribution of non-metallic inclusions. The dynamics of change in the content of inclusions was established according to the following criteria: total oxygen content, volume fraction, density and average diameter of inclusions. The composition of non-metallic inclusions was plotted on ternary diagrams: the oxide component on the diagrams CaO – Al 2 O 3 – SiO 2 and CaO – Al 2 O 3 – MgO, the sulfide – on Ca – Mn – S. The trajectory of change in the chemical composition of inclusions in the steelmaking process was established. The paper shows the role of steel treatment with calcium and importance of observing thermodynamic conditions. A relationship is established between deviations in calcium treatment parameters, composition of non-metallic inclusions, steel castability and sorting of pipe products by surface and internal defects. Decreasing total oxygen content, practically does not occur at the main stage of ladle treatment. The highest intensity of steel refining from inclusions is observed at the stage between the samples before and after steel treatment with calcium, this time interval is less than 10 min. Comparison of the obtained data on the chemical composition of inclusions with the calculated data on the boundary of liquid phase region of the CaO – Al 2 O 3 – SiO 2 – MgO system shows that at this stage, the chemical and phase composition of non-metallic inclusions is transformed. After the addition of calcium, the composition of oxide non-metallic inclusions shifted to the liquid region of the CaO – Al 2 O 3 – SiO 2 system at MgO content of 10 wt. % and 1600 °C.
- Open Access
- 8 November 2025
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 68 (5) , 468-475
Interaction of Al2O3-based ceramics with slag melt 45 % CaO – 40 % Al2O3 – 10 % SiO2 – 5 % MgO
In steelmaking, the refractory material used as a lining is easily destroyed by slag, which not only decreases the service life of ceramics but also makes worse a production quality because of increase in the number of nonmetallic inclusions in metal. If the slag has good wettability, it tends to penetrate the refractory through pores and cracks. As a result, a boundary layer is formed, which has a structure and properties different from the initial material. The sessile drop method was used to study the interaction of Al 2 O 3 -based refractory ceramics with the liquid slag 45 % CaO – 40 % Al 2 O 3 – 10 % SiO 2 – 5 % MgO. The substantial decrease in the wetting angle to 20° in the initial 5 min of experiment and the further small decrease to 13.5° in the next 115 min were observed. The microstructural examination and elemental mapping of the boundaries of cross sections of slag and ceramics were carried out. The slag consists of several phases, namely: Ca2(Mg 0.25 Al 0.75 )(Si 1.25 Al 0.75 O 7 ); CaAl 2 O 4 , CaAl 4 O 7 and MgAl 2 O 4 . As was found, the slag–ceramics boundary layer consisted of calcium aluminate (CaAl 4 O 7 ) and, at the grain boundaries of aluminum oxide in the refractory material, hibonite (CaAl 12 O 19 ) was formed. X -ray diffraction analysis of initial ceramics showed that it contained ~8 % CaAl 4 O 7 , and after interaction with the slag ~32 % CaAl 12 O 19 . At a depth of 4 mm, the presence of calcium aluminates both in the central and peripheral zones of ceramics was observed. This indicates the slag penetration into the ceramics and their chemical interaction.
- 8 November 2025
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 68 (5) , 468-475
Open AccessInteraction of Al2O3-based ceramics with slag melt 45 % CaO – 40 % Al2O3 – 10 % SiO2 – 5 % MgO
In steelmaking, the refractory material used as a lining is easily destroyed by slag, which not only decreases the service life of ceramics but also makes worse a production quality because of increase in the number of nonmetallic inclusions in metal. If the slag has good wettability, it tends to penetrate the refractory through pores and cracks. As a result, a boundary layer is formed, which has a structure and properties different from the initial material. The sessile drop method was used to study the interaction of Al 2 O 3 -based refractory ceramics with the liquid slag 45 % CaO – 40 % Al 2 O 3 – 10 % SiO 2 – 5 % MgO. The substantial decrease in the wetting angle to 20° in the initial 5 min of experiment and the further small decrease to 13.5° in the next 115 min were observed. The microstructural examination and elemental mapping of the boundaries of cross sections of slag and ceramics were carried out. The slag consists of several phases, namely: Ca2(Mg 0.25 Al 0.75 )(Si 1.25 Al 0.75 O 7 ); CaAl 2 O 4 , CaAl 4 O 7 and MgAl 2 O 4 . As was found, the slag–ceramics boundary layer consisted of calcium aluminate (CaAl 4 O 7 ) and, at the grain boundaries of aluminum oxide in the refractory material, hibonite (CaAl 12 O 19 ) was formed. X -ray diffraction analysis of initial ceramics showed that it contained ~8 % CaAl 4 O 7 , and after interaction with the slag ~32 % CaAl 12 O 19 . At a depth of 4 mm, the presence of calcium aluminates both in the central and peripheral zones of ceramics was observed. This indicates the slag penetration into the ceramics and their chemical interaction.
- Open Access
- 20 October 2024
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 67 (5) , 549-555
Formation of non-metallic inclusions in production of 08Kh18N10T corrosion-resistant steel
Corrosion-resistant steels are in demand in the modern world due to their high performance properties and a wide range of applications. Such areas of application include kitchenware, furniture, medical equipment, nuclear reactors, spacecraft, etc. Oxygen in steel, especially in corrosion-resistant steel, is one of the most harmful elements. Oxide inclusions disrupt the homogeneity of the metal, negatively affect the ductility, fracture toughness, fatigue strength and corrosion resistance of steel. In corrosion-resistant steels, non-metallic inclusions (NI) lead to the formation of defects in cold-rolled sheets. Aluminate inclusions also lead to clogging of steel-casting equipment. An analysis of the production technology of corrosion-resistant steel 08Kh8N10T was carried out in order to determine the causes of NI formation that affect the pourability of steel and its quality. The studies determined the content of total oxygen and nitrogen, as well as oxygen bound in various non-metallic inclusions at the stages of ladle processing and continuous steel casting. It was shown that after the introduction of titanium wire into the melt, the total nitrogen content decreases due to the formation and subsequent removal of titanium nitrides. At the same time, the content of titanium oxides in the melt increases. It was shown that the causes of clogging of steel-pouring nozzles during continuous casting are complex non-metallic inclusions based on titanium oxides, which were deposited on the inner surface of the pouring nozzle-doser. Recommendations were made to adjust the technology of steel melting in EAF and ladle processing. Based on the results of electron microscopic analysis, it was established that mixing of refining liquid-mobile slag in ladle steel processing units contributed to the assimilation of non-metallic inclusions by slag and a decrease in their sizes in the metal. After the implementation of the corrective recommendations, clogging of steel-pouring nozzles during continuous casting was not observed.
- 20 October 2024
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 67 (5) , 549-555
Open AccessFormation of non-metallic inclusions in production of 08Kh18N10T corrosion-resistant steel
Corrosion-resistant steels are in demand in the modern world due to their high performance properties and a wide range of applications. Such areas of application include kitchenware, furniture, medical equipment, nuclear reactors, spacecraft, etc. Oxygen in steel, especially in corrosion-resistant steel, is one of the most harmful elements. Oxide inclusions disrupt the homogeneity of the metal, negatively affect the ductility, fracture toughness, fatigue strength and corrosion resistance of steel. In corrosion-resistant steels, non-metallic inclusions (NI) lead to the formation of defects in cold-rolled sheets. Aluminate inclusions also lead to clogging of steel-casting equipment. An analysis of the production technology of corrosion-resistant steel 08Kh8N10T was carried out in order to determine the causes of NI formation that affect the pourability of steel and its quality. The studies determined the content of total oxygen and nitrogen, as well as oxygen bound in various non-metallic inclusions at the stages of ladle processing and continuous steel casting. It was shown that after the introduction of titanium wire into the melt, the total nitrogen content decreases due to the formation and subsequent removal of titanium nitrides. At the same time, the content of titanium oxides in the melt increases. It was shown that the causes of clogging of steel-pouring nozzles during continuous casting are complex non-metallic inclusions based on titanium oxides, which were deposited on the inner surface of the pouring nozzle-doser. Recommendations were made to adjust the technology of steel melting in EAF and ladle processing. Based on the results of electron microscopic analysis, it was established that mixing of refining liquid-mobile slag in ladle steel processing units contributed to the assimilation of non-metallic inclusions by slag and a decrease in their sizes in the metal. After the implementation of the corrective recommendations, clogging of steel-pouring nozzles during continuous casting was not observed.
- Open Access
- 1 September 2024
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 67 (4) , 471-480
Development of a methodology for determining the content of non-metallic inclusions in steel
As part of the study, a method was proposed for assessing the metal purity for non-metallic inclusions using optical emission spectrometry. To assess the content of non-metallic inclusions in the slabs, two columns of metal were selected from two slabs of low-alloy metal deoxidized with aluminum. Each column was divided into seven samples in the direction from the small radius of the continuously cast ingot to the large one. We studied these samples to assess metal contamination with non-metallic inclusions using quantitative optical metallography according to ASTM E1245-03, fractional gas analysis (FGA) and optical emission spectral analysis PDA. Analysis of the samples according to ASTM E1245-03 standard showed that in all samples the percentage of oxides and sulfides is on average 10 and 90 %, respectively. According to the results of FGA, it was concluded that such non-metallic oxide inclusions as aluminates predominate in the metal samples of both ingots. A comparison was made between the results of the determination of oxygen in non-metallic inclusions obtained by FGA method and the number of sparks in inclusions at the analysis by PDA method; analysis of the dependencies showed that there are two clearly defined point distributions. To carry out PDA analysis, a program was developed that allows determining the number of inclusions of various types and calculate their volume fraction.
- 1 September 2024
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 67 (4) , 471-480
Open AccessDevelopment of a methodology for determining the content of non-metallic inclusions in steel
As part of the study, a method was proposed for assessing the metal purity for non-metallic inclusions using optical emission spectrometry. To assess the content of non-metallic inclusions in the slabs, two columns of metal were selected from two slabs of low-alloy metal deoxidized with aluminum. Each column was divided into seven samples in the direction from the small radius of the continuously cast ingot to the large one. We studied these samples to assess metal contamination with non-metallic inclusions using quantitative optical metallography according to ASTM E1245-03, fractional gas analysis (FGA) and optical emission spectral analysis PDA. Analysis of the samples according to ASTM E1245-03 standard showed that in all samples the percentage of oxides and sulfides is on average 10 and 90 %, respectively. According to the results of FGA, it was concluded that such non-metallic oxide inclusions as aluminates predominate in the metal samples of both ingots. A comparison was made between the results of the determination of oxygen in non-metallic inclusions obtained by FGA method and the number of sparks in inclusions at the analysis by PDA method; analysis of the dependencies showed that there are two clearly defined point distributions. To carry out PDA analysis, a program was developed that allows determining the number of inclusions of various types and calculate their volume fraction.
- Open Access
- 30 June 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (3) , 344-355
Lead and zinc selective extraction from EAF dust while heating in resistance furnace with flowing argon
The elemental and phase compositions of electric arc furnace (EAF) dust from PJSC Severstal were studied. We carried out the thermodynamic modeling of zinc and lead selective extraction process and determined its possible mechanisms. EAF dust was heated in the temperature range of 20 – 1300 °C in vacuum resistance furnace and the Tamman furnace with flowing argon. Experiments in the vacuum resistance furnace with linear heating showed that lead and zinc removal from the sample occurs in the temperature range of 800 – 1200 °C, with higher lead removal rate. Intensive lead removal was observed at temperature above 1000 °C, while intensive zinc removal occurs at temperature above 1200 °C. Clarifying isothermal experiments performed in the Tamman furnace showed that lead complete transition to the gas phase was achieved at a temperature of 1100 °C (holding time – 12 min) and at a temperature of 1200 °C (holding time – 6 min or more). At the same time, zinc removal was observed in the amount of 14.4 % ratio and 32.2 % ratio, respectively, which allows us to conclude that it is possible to consistently obtain two products: lead and zinc mixture and zinc not contaminated with lead. When comparing experimental and thermodynamic modeling data, the reactions that are most likely to occur during the carbon reduction of lead- and zinc-containing phases were determined.
- 30 June 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (3) , 344-355
Open AccessLead and zinc selective extraction from EAF dust while heating in resistance furnace with flowing argon
The elemental and phase compositions of electric arc furnace (EAF) dust from PJSC Severstal were studied. We carried out the thermodynamic modeling of zinc and lead selective extraction process and determined its possible mechanisms. EAF dust was heated in the temperature range of 20 – 1300 °C in vacuum resistance furnace and the Tamman furnace with flowing argon. Experiments in the vacuum resistance furnace with linear heating showed that lead and zinc removal from the sample occurs in the temperature range of 800 – 1200 °C, with higher lead removal rate. Intensive lead removal was observed at temperature above 1000 °C, while intensive zinc removal occurs at temperature above 1200 °C. Clarifying isothermal experiments performed in the Tamman furnace showed that lead complete transition to the gas phase was achieved at a temperature of 1100 °C (holding time – 12 min) and at a temperature of 1200 °C (holding time – 6 min or more). At the same time, zinc removal was observed in the amount of 14.4 % ratio and 32.2 % ratio, respectively, which allows us to conclude that it is possible to consistently obtain two products: lead and zinc mixture and zinc not contaminated with lead. When comparing experimental and thermodynamic modeling data, the reactions that are most likely to occur during the carbon reduction of lead- and zinc-containing phases were determined.
- 1 November 2022
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2022 (11) , 1449-1455
Features of the Formation of Surface Layers on Metal Materials by the of Electric Arc Vacuum-Ion-Plasma Deposition Method
Methods of electric arc ion vacuum plasma deposition (VIPD) are widely used to improve the performance of metallic materials in mechanical engineering, aviation, space technology and medicine. The influence of electron and ion streams of argon plasma on the structure and elements distribution in the surface layers of steels has been investigated by using glow discharge optical emission spectrometry and Auger electron spectrometry. It was shown that the sign and magnitude of the reference voltage on the treated samples determine the result of the influence of argon plasma on the structure and properties of the surface layer of structural metallic materials. The influence of the sequence of technological effects during the application of surface layers on the layer-by-layer composition and properties of the material being processed was investigated. It was shown that the interaction of the plasma flow with the material being processed leads to the development of processes of inverse diffusion of matrix elements to the surface, and the formation of micron and nano-sized particles of oxides, carbides and carbonitrides in the surface layer, thus changing the properties of the products.
- 1 November 2022
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2022 (11) , 1449-1455
Features of the Formation of Surface Layers on Metal Materials by the of Electric Arc Vacuum-Ion-Plasma Deposition Method
Methods of electric arc ion vacuum plasma deposition (VIPD) are widely used to improve the performance of metallic materials in mechanical engineering, aviation, space technology and medicine. The influence of electron and ion streams of argon plasma on the structure and elements distribution in the surface layers of steels has been investigated by using glow discharge optical emission spectrometry and Auger electron spectrometry. It was shown that the sign and magnitude of the reference voltage on the treated samples determine the result of the influence of argon plasma on the structure and properties of the surface layer of structural metallic materials. The influence of the sequence of technological effects during the application of surface layers on the layer-by-layer composition and properties of the material being processed was investigated. It was shown that the interaction of the plasma flow with the material being processed leads to the development of processes of inverse diffusion of matrix elements to the surface, and the formation of micron and nano-sized particles of oxides, carbides and carbonitrides in the surface layer, thus changing the properties of the products.
- 15 March 2022
- Published by Institute of Metallurgy and Ore Benefication (Publications) in Kompleksnoe Ispolzovanie Mineralnogo Syra = Complex Use of Mineral Resources
- Vol. 320 (1) , 51-59
Smelting options for carbon ferrochrome based on ore raw materials, middlings and their technological evaluation
The article presents the results of large-scale laboratory tests carried out in the conditions of the Chemical and Metallurgical Institute named after V.I. Zh. Abishev on the use of briquetted mono-charge in the smelting of carbon ferrochrome on a 250 kVA furnace. The purpose of these studies was to determine the technological parameters of the use of briquetted mono-charge containing in its composition chrome ore, wastes from the production of high-carbon ferrochrome, middlings and various carbonaceous reducing agents. The main idea of using these briquettes was to multiply the contact surface of the reductant and ore, which should speed up the technological process. The principal possibility of smelting a standard alloy using briquetted mono-charge is shown. The alloy for individual charge options meets the requirements of the standards. In comparison with the technology without the use of briquettes, the mono-charge technology has shown advantages in all main parameters. The technology with the use of briquettes from the dust of the AktZF gas cleaning system is distinguished by a low yield of non-standard metal and slag, the bulk of the material goes into the gas collection system. Technologies from briquettes from fines pellet production area of Donskoy ore mining and processing plant and flash have very low specific technical and economic indicators and cannot be recommended for industrial use. Improvement of briquetting modes and technology of their smelting is required. The technical and economic indicators were higher than the current one, showed briquettes from ore and coke of the People's Republic of China, briquettes of ore from borlin and shubarkol coals of Kazakhstan.
- 15 March 2022
- Published by Institute of Metallurgy and Ore Benefication (Publications) in Kompleksnoe Ispolzovanie Mineralnogo Syra = Complex Use of Mineral Resources
- Vol. 320 (1) , 51-59
Smelting options for carbon ferrochrome based on ore raw materials, middlings and their technological evaluation
The article presents the results of large-scale laboratory tests carried out in the conditions of the Chemical and Metallurgical Institute named after V.I. Zh. Abishev on the use of briquetted mono-charge in the smelting of carbon ferrochrome on a 250 kVA furnace. The purpose of these studies was to determine the technological parameters of the use of briquetted mono-charge containing in its composition chrome ore, wastes from the production of high-carbon ferrochrome, middlings and various carbonaceous reducing agents. The main idea of using these briquettes was to multiply the contact surface of the reductant and ore, which should speed up the technological process. The principal possibility of smelting a standard alloy using briquetted mono-charge is shown. The alloy for individual charge options meets the requirements of the standards. In comparison with the technology without the use of briquettes, the mono-charge technology has shown advantages in all main parameters. The technology with the use of briquettes from the dust of the AktZF gas cleaning system is distinguished by a low yield of non-standard metal and slag, the bulk of the material goes into the gas collection system. Technologies from briquettes from fines pellet production area of Donskoy ore mining and processing plant and flash have very low specific technical and economic indicators and cannot be recommended for industrial use. Improvement of briquetting modes and technology of their smelting is required. The technical and economic indicators were higher than the current one, showed briquettes from ore and coke of the People's Republic of China, briquettes of ore from borlin and shubarkol coals of Kazakhstan.