Dong Peng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Dong Peng has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
- Dalong Cong
Southwest Institute of Technology and Engineering, Chongqing 400039, China
4 shared publications - Kaiqiang Song
Southwest Institute of Technology and Engineering, Chongqing 400039, China
4 shared publications - Min Zhang
Southwest Institute of Technology and Engineering, Chongqing 400039, China
4 shared publications - Zhongsheng Li
Southwest Institute of Technology and Engineering, Chongqing 400039, China
4 shared publications - Anwei Huang
Southwest Institute of Technology and Engineering, Chongqing 400039, China
3 shared publications - Xingxing Ding
Southwest Institute of Technology and Engineering, Chongqing 400039, China
3 shared publications
Latest Publications
- Open Access
Study on Damage Behavior of NiCoCrAlY/MSZ Plasma-Sprayed Coating in Neutral Salt Spray Environment
In order to explore the corrosion damage behavior of plasma-sprayed NiCoCrAlY/magnesia-stabilized zirconia (18~22 wt.% MgO-ZrO2, MSZ) thermal barrier and anti-ablation coatings in a salt spray environment, a series of neutral salt spray (NSS) tests for 96 h (N-2), 192 h (N-4) and 288 h (N-6) were carried out on the coatings. The microstructures, composition distributions, potentiodynamic polarization curves, bonding strengths and anti-ablation properties of the coatings before and after the NSS tests were characterized. The results show that, with the increase in salt spray time, the expansion and overflow of corrosion products (FexOy) led to more defects forming inside the coating; the porosity of the top coat (TC) of N-6 increased to 15.2% in comparison to that of the blank control sample (N-0), which was 8.5%. According to the potentiodynamic polarization curves, accelerated corrosion occurred in the coating samples after the salt spray time reached 192 h, and the corrosion current density rapidly surged from 2.2 × 10−8 A·cm−2 (N-4) to 2.2 × 10−5 A·cm−2 (N-6). Similar degradation tends could be found in the bonding strengths and mass ablation rates of the coatings due to the accumulation of loose corrosion products on the substrate, which affected the bonding states of the coatings and promoted their spalling under an oxyacetylene flame (OAF). As a result, the maximum service life of the NiCoCrAlY/MSZ coatings in the neutral salt spray environment was about 192 h. This work is instructive for studying the environmental adaptability of metal/ceramic double-layer coatings.
Open AccessStudy on Damage Behavior of NiCoCrAlY/MSZ Plasma-Sprayed Coating in Neutral Salt Spray Environment
In order to explore the corrosion damage behavior of plasma-sprayed NiCoCrAlY/magnesia-stabilized zirconia (18~22 wt.% MgO-ZrO2, MSZ) thermal barrier and anti-ablation coatings in a salt spray environment, a series of neutral salt spray (NSS) tests for 96 h (N-2), 192 h (N-4) and 288 h (N-6) were carried out on the coatings. The microstructures, composition distributions, potentiodynamic polarization curves, bonding strengths and anti-ablation properties of the coatings before and after the NSS tests were characterized. The results show that, with the increase in salt spray time, the expansion and overflow of corrosion products (FexOy) led to more defects forming inside the coating; the porosity of the top coat (TC) of N-6 increased to 15.2% in comparison to that of the blank control sample (N-0), which was 8.5%. According to the potentiodynamic polarization curves, accelerated corrosion occurred in the coating samples after the salt spray time reached 192 h, and the corrosion current density rapidly surged from 2.2 × 10−8 A·cm−2 (N-4) to 2.2 × 10−5 A·cm−2 (N-6). Similar degradation tends could be found in the bonding strengths and mass ablation rates of the coatings due to the accumulation of loose corrosion products on the substrate, which affected the bonding states of the coatings and promoted their spalling under an oxyacetylene flame (OAF). As a result, the maximum service life of the NiCoCrAlY/MSZ coatings in the neutral salt spray environment was about 192 h. This work is instructive for studying the environmental adaptability of metal/ceramic double-layer coatings.
- Open Access
Effects of Additives Containing Cyanopyridine on Electrodeposition of Bright Al Coatings from AlCl3-EMIC Ionic Liquids
The Al coatings were electrodeposited on the Cu substrate from AlCl3-EMIC ionic liquid (AlCl3:EMIC = 2:1 molar ratio) containing three cyanopyridine additives with different positions of the substituent group on the pyridine ring, which were 2-cyanopyridine, 3-cyanopyridine, and 4-cyanopyridine. The effects of cyanopyridine additives on the deposition potential, morphology, brightness, and corrosion properties of Al coatings were investigated. It was considered that the deposition potential of Al shifted to more negative overpotentials, the quality of Al coatings was promoted, and the corrosion property was improved by the cyanopyridine additives to a varying degree. Especially in the presence of 4-cyanopyridine, the flattest mirror bright Al coating was obtained, which had the smallest homogeneous nanocrystal grain size and strongest Al (200) crystallographic orientation. The average roughness Ra value was as low as 31 nm compared to that in the absence of cyanopyridine additives, which was 417 nm. Furthermore, the corrosion current density of the bright Al coating was three orders of magnitude lower than the rough Al coating, which resulted from the dense nanocrystal structure.
Open AccessEffects of Additives Containing Cyanopyridine on Electrodeposition of Bright Al Coatings from AlCl3-EMIC Ionic Liquids
The Al coatings were electrodeposited on the Cu substrate from AlCl3-EMIC ionic liquid (AlCl3:EMIC = 2:1 molar ratio) containing three cyanopyridine additives with different positions of the substituent group on the pyridine ring, which were 2-cyanopyridine, 3-cyanopyridine, and 4-cyanopyridine. The effects of cyanopyridine additives on the deposition potential, morphology, brightness, and corrosion properties of Al coatings were investigated. It was considered that the deposition potential of Al shifted to more negative overpotentials, the quality of Al coatings was promoted, and the corrosion property was improved by the cyanopyridine additives to a varying degree. Especially in the presence of 4-cyanopyridine, the flattest mirror bright Al coating was obtained, which had the smallest homogeneous nanocrystal grain size and strongest Al (200) crystallographic orientation. The average roughness Ra value was as low as 31 nm compared to that in the absence of cyanopyridine additives, which was 417 nm. Furthermore, the corrosion current density of the bright Al coating was three orders of magnitude lower than the rough Al coating, which resulted from the dense nanocrystal structure.
- Open Access
Mirror-like Bright Al-Mn Coatings Electrodeposition from 1-Ethyl-3 Methylimidazolium Chloride-AlCl3-MnCl2 Ionic Liquids with Pyridine Derivatives
The effects of three pyridine derivative additives, 4-hydroxypyridine, 4-picolinic acid, and 4-cyanopyridine, on Al-Mn coatings were investigated in 1-ethyl-3-methylimidazolium chloride-AlCl3-MnCl2 (EMIC-AlCl3-MnCl2) ionic liquids. The smooth mirror-like bright Al-Mn coatings were obtained only in the EMIC-AlCl3-MnCl2 ionic liquids containing 4-cyanopyridine, while the matte Al-Mn coatings were electrodeposited from EMIC-AlCl3-MnCl2 without additives or containing either 4-hydroxypyridine or 4-picolinic acid. The scanning electron microscope and X-ray diffraction showed that the bright Al-Mn coatings consisted of nanocrystals and had a strong (200) preferential orientation, while the particle size of matte Al-Mn coatings were within the micron range. The brightening mechanism of 4-cyanopyridine is due to it being adsorbed onto the cathode to produce the combined effect of (1) generating an overpotential to promote Al-Mn nucleation; (2) inhibiting the growth of the deposited nuclei and enabling them grow preferentially, making the coating composed of nanocrystals and with a smooth surface. The brightening effect of 4-cyanopyridine on the Al-Mn coatings was far better than that of the 4-hydroxypyridine and the 4-picolinic acid. In addition, the bright Al-Mn coating was prepared in a bath with 6 mmol·L−1 4-cyanopyridine and displayed superior corrosion resistance relative to the matte coatings, which could be attributed to its unique nanocrystalline structure that increased the number of grain boundaries and accelerated the formation of the protective layer of the corrosion products.
Open AccessMirror-like Bright Al-Mn Coatings Electrodeposition from 1-Ethyl-3 Methylimidazolium Chloride-AlCl3-MnCl2 Ionic Liquids with Pyridine Derivatives
The effects of three pyridine derivative additives, 4-hydroxypyridine, 4-picolinic acid, and 4-cyanopyridine, on Al-Mn coatings were investigated in 1-ethyl-3-methylimidazolium chloride-AlCl3-MnCl2 (EMIC-AlCl3-MnCl2) ionic liquids. The smooth mirror-like bright Al-Mn coatings were obtained only in the EMIC-AlCl3-MnCl2 ionic liquids containing 4-cyanopyridine, while the matte Al-Mn coatings were electrodeposited from EMIC-AlCl3-MnCl2 without additives or containing either 4-hydroxypyridine or 4-picolinic acid. The scanning electron microscope and X-ray diffraction showed that the bright Al-Mn coatings consisted of nanocrystals and had a strong (200) preferential orientation, while the particle size of matte Al-Mn coatings were within the micron range. The brightening mechanism of 4-cyanopyridine is due to it being adsorbed onto the cathode to produce the combined effect of (1) generating an overpotential to promote Al-Mn nucleation; (2) inhibiting the growth of the deposited nuclei and enabling them grow preferentially, making the coating composed of nanocrystals and with a smooth surface. The brightening effect of 4-cyanopyridine on the Al-Mn coatings was far better than that of the 4-hydroxypyridine and the 4-picolinic acid. In addition, the bright Al-Mn coating was prepared in a bath with 6 mmol·L−1 4-cyanopyridine and displayed superior corrosion resistance relative to the matte coatings, which could be attributed to its unique nanocrystalline structure that increased the number of grain boundaries and accelerated the formation of the protective layer of the corrosion products.