Stefan Heinze
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Stefan Heinze has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Christoph Leyens
TU Dresden
2 shared publications - Andreas Stark
Institute of Materials Research, Helmholtz-Zentrum Geesthacht, Max-Planck-Str. 1, 21502 Geesthacht, Germany
1 shared publication - Anton Davydok
Institute of Materials Physics Helmholtz‐Zentrum Hereon Outstation at DESY Hamburg Germany
1 shared publication - Axel Marquardt
Institute for Materials Science
1 shared publication - Christina Krywka
Institute of Materials Research Helmholtz Zentrum Hereon c/o DESY Notkestraße 85 22607 Hamburg Germany
1 shared publication Elena López
Technology Field Additive Manufacturing and Surface Technologies Fraunhofer Institute for Material and Beam Technology IWS 01277 Dresden Germany
1 shared publication
Latest Publications
- Open Access
- 21 October 2022
- Published by Wiley in Advanced Engineering Materials
- Vol. 25 (2)
Influence of Two‐Step Heat Treatments on Microstructure and Mechanical Properties of a β‐Solidifying Titanium Aluminide Alloy Fabricated via Electron Beam Powder Bed Fusion
Additive manufacturing technologies, particularly electron beam powder bed fusion (PBF‐EB/M), are becoming increasingly important for the processing of intermetallic titanium aluminides. This study presents the effects of hot isostatic pressing (HIP) and subsequent two‐step heat treatments on the microstructure and mechanical properties of the TNM‐B1 alloy (Ti–43.5Al–4Nb–1Mo–0.1B) fabricated via PBF‐EB/M. Adequate solution heat treatment temperatures allow the adjustment of fully lamellar (FL) and nearly lamellar (NL‐β) microstructures. The specimens are characterized by optical microscopy and scanning electron microscopy (SEM), X‐ray computed tomography (CT), X‐ray diffraction (XRD), and electron backscatter diffraction (EBSD). The mechanical properties at ambient temperatures are evaluated via tensile testing and subsequent fractography. While lack‐of‐fusion defects are the main causes of failure in the as‐built condition, the mechanical properties in the heat‐treated conditions are predominantly controlled by the microstructure. The highest ultimate tensile strength is achieved after HIP due to the elimination of lack‐of‐fusion defects. The results reveal challenges originating from the PBF‐EB/M process, for example, local variations in chemical composition due to aluminum evaporation, which in turn affect the microstructures after heat treatment. For designing suitable heat treatment strategies, particular attention should therefore be paid to the microstructural characteristics associated with additive manufacturing.
- 21 October 2022
- Published by Wiley in Advanced Engineering Materials
- Vol. 25 (2)
Open AccessInfluence of Two‐Step Heat Treatments on Microstructure and Mechanical Properties of a β‐Solidifying Titanium Aluminide Alloy Fabricated via Electron Beam Powder Bed Fusion
Additive manufacturing technologies, particularly electron beam powder bed fusion (PBF‐EB/M), are becoming increasingly important for the processing of intermetallic titanium aluminides. This study presents the effects of hot isostatic pressing (HIP) and subsequent two‐step heat treatments on the microstructure and mechanical properties of the TNM‐B1 alloy (Ti–43.5Al–4Nb–1Mo–0.1B) fabricated via PBF‐EB/M. Adequate solution heat treatment temperatures allow the adjustment of fully lamellar (FL) and nearly lamellar (NL‐β) microstructures. The specimens are characterized by optical microscopy and scanning electron microscopy (SEM), X‐ray computed tomography (CT), X‐ray diffraction (XRD), and electron backscatter diffraction (EBSD). The mechanical properties at ambient temperatures are evaluated via tensile testing and subsequent fractography. While lack‐of‐fusion defects are the main causes of failure in the as‐built condition, the mechanical properties in the heat‐treated conditions are predominantly controlled by the microstructure. The highest ultimate tensile strength is achieved after HIP due to the elimination of lack‐of‐fusion defects. The results reveal challenges originating from the PBF‐EB/M process, for example, local variations in chemical composition due to aluminum evaporation, which in turn affect the microstructures after heat treatment. For designing suitable heat treatment strategies, particular attention should therefore be paid to the microstructural characteristics associated with additive manufacturing.
- Open Access
- 17 July 2022
- Published by Elsevier in SSRN Electronic Journal
Influence of the Deposition Process and Substrate on Microstructure, Phase Composition, and Residual Stress State on As-Deposited Cr-Al-C Coatings
This paper focuses on the influence of the deposition process, deposition parameters, and substrate on various properties of the as-deposited state of Cr-Al-C thin films deposited by Direct Current Magnetron Sputtering (DCMS) and High Power Pulsed Magnetron Sputtering (HPPMS) with the variation of bias voltage and deposition temperature. Three substrates with different coefficients of thermal expansion and electrical conductivity were used. To investigate the microstructure, phase composition, residual stress state, and mechanical properties, ex-situ and in-situ synchrotron experiments were conducted accompanied by electron microscopy and nanoindentation. As-deposited Cr-Al-C coatings consisted of amorphous and crystalline areas, with the ratio highly dependent on the deposition process and substrate. The crystalline phase was identified as metastable (Cr,Al)2C. The highest crystallinity was determined for DCMS coatings. Increasing temperature and decreasing bias voltage increased coating crystallinity for HPPMS coatings. The influence of the deposition process and bias voltage was highly reduced for the substrate with low electrical conductivity. In-situ investigations of the stress state of amorphous areas revealed, that those were acting as a residual stress buffer. The hardness and Young’s modulus of the coatings were found to increase with crystallinity and were slightly increased for crystalline HPPMS coatings compared to DCMS coatings.
- 17 July 2022
- Published by Elsevier in SSRN Electronic Journal
Open AccessInfluence of the Deposition Process and Substrate on Microstructure, Phase Composition, and Residual Stress State on As-Deposited Cr-Al-C Coatings
This paper focuses on the influence of the deposition process, deposition parameters, and substrate on various properties of the as-deposited state of Cr-Al-C thin films deposited by Direct Current Magnetron Sputtering (DCMS) and High Power Pulsed Magnetron Sputtering (HPPMS) with the variation of bias voltage and deposition temperature. Three substrates with different coefficients of thermal expansion and electrical conductivity were used. To investigate the microstructure, phase composition, residual stress state, and mechanical properties, ex-situ and in-situ synchrotron experiments were conducted accompanied by electron microscopy and nanoindentation. As-deposited Cr-Al-C coatings consisted of amorphous and crystalline areas, with the ratio highly dependent on the deposition process and substrate. The crystalline phase was identified as metastable (Cr,Al)2C. The highest crystallinity was determined for DCMS coatings. Increasing temperature and decreasing bias voltage increased coating crystallinity for HPPMS coatings. The influence of the deposition process and bias voltage was highly reduced for the substrate with low electrical conductivity. In-situ investigations of the stress state of amorphous areas revealed, that those were acting as a residual stress buffer. The hardness and Young’s modulus of the coatings were found to increase with crystallinity and were slightly increased for crystalline HPPMS coatings compared to DCMS coatings.