QLQiang Lu

Qiang Lu

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Qiang Lu has a total of 10 co-authors. Here are the top co-authors by number of shared publications:

  • Qudong Wang

    National Engineering Research Center of Light Alloy Net Forming, State Key Laboratory of Metal Matrix Composites, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China

    4 shared publications
  • Dezhi Li

    Warwick Manufacturing Group, University of Warwick, Coventry CV4 7AL, UK

    3 shared publications
  • Yuchao Zhao

    National Engineering Research Center of Light Alloy Net Forming and Key State Laboratory of Metal Matrix Composites, School of Material Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China

    3 shared publications
  • Chuan Lei

    National Engineering Research Center of Light Alloy Net Forming, State Key Laboratory of Metal Matrix Composites, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China

    1 shared publication
  • Feng Li

    GD Midea Heating & Ventilating Equipment Co., Ltd., Foshan 528308, China

    1 shared publication
  • Haiyan Jiang

    National Engineering Research Center of Light Alloy Net Forming and Key State Laboratory of Metal Matrix Composites, School of Material Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China

    1 shared publication

Latest Publications

  • Open Access

    Layer Thickness Effects on Residual Stress, Microstructure, and Tensile Properties of Cu18150/Al1060/Cu18150 Multilayered Composites: An Integrated EBSD-KAM Approach

    by Yuchao Zhao, Mahmoud Ebrahimi, Shokouh Attarilar, Qiang Lu, Haiyan Jiang, Qudong Wang

    This study examines the influence of layer thickness (0.9, 1.6, 2.4, and 4 mm) on the distribution of residual stress, microstructural evolution, and tensile properties of Cu18150/Al1060/Cu18150 multilayered composites fabricated via a combined cast-rolling and hot-rolling technique. The grain refinement, dislocation density, and residual stress gradients across the interfaces were characterized and analyzed using integrated electron backscatter diffraction and kernel average misorientation mapping. The results demonstrated that specimens with a lower layer thickness (0.9–1.6 mm) possess a significantly improved tensile strength of 351 MPa, which is mainly due to the significant grain refinement and the presence of compressive residual stresses at the region of the Al/Cu interfaces. However, tensile strength decreased to 261 MPa in specimens with thicker layers (4 mm), accompanied by improved ductility, e.g., elongation of 30%. This is associated with a reduction in the degrees of interfacial constraint and the formation of more homogeneous deformation structures that accommodate a larger strain. The intermediate layer thickness of 2.4 mm offers an optimal compromise, achieving a tensile strength of 317 MPa while maintaining balanced mechanical performance. These results emphasize the importance of layer thickness in controlling such stress profiles and optimizing the mechanical behavior of hybrid metal composites, providing useful guidance on the design and fabrication of superior structural-form materials.


  • Open Access

    Effect of Al-5Ti-1B-xCe Refiner on Microstructure and Mechanical Properties of Cast Al-5Mg-3Zn-1Cu Alloys

    by Shenshen Cui, Qiang Lu, Qudong Wang, Dezhi Li, Chuan Lei

    The effects of Ce content on the microstructure and phase composition of the Al-5Ti-1B refiner and the refining effect of the Al-5Ti-1B-xCe (x = 0, 1, 5, 10 wt.%) refiner on the grain size, microstructure, and mechanical properties of Al-5Mg-3Zn-1Cu alloys were studied. The results show that the addition of 1.0 wt.% Ce in the Al-5Ti-1B refiner changes the TiAl3 phase from block to strip, and the massive Ti2Al20Ce phase is formed. When the Ce content of the Al-5Ti-1B refiner increases to 5.0 wt.%, the plate-like TiAl3 phase is surrounded by the Ti2Al20Ce phase, and the reticulate Al4Ce phase is formed. With the Ce content of the Al-5Ti-1B refiner further increasing to 10.0 wt.%, a lot of network distribution Al4Ce phase is formed. The volume of the Mg32(AlCuZn)49 phase of the as-cast Al-5Mg-3Zn-1Cu alloys is reduced after refining with the Al-5Ti-1B-xCe refiner. The Al-5Ti-1B-1Ce refiner has the best refining effect on as-cast Al-5Mg-3Zn-1Cu alloys, and the grain size of as-cast Al-5Mg-3Zn-1Cu alloys refined by the Al-5Ti-1B-1Ce refiner is reduced by 43% compared with as-cast Al-5Mg-3Zn-1Cu alloys refined by the Al-5Ti-1B refiner. Compared to the aged Al-5Mg-3Zn-1Cu alloys refined by the Al-5Ti-1B refiner, the yield strength, ultimate tensile strength, and fracture elongation of aged Al-5Mg-3Zn-1Cu alloys refined by the Al-5Ti-1B-5Ce refiner are improved by 4.0%, 4.6%, and 25.6%, respectively. Therefore, it can be seen that Al-5Ti-1B-1Ce refiner and Al-5Ti-1B-5Ce refiner have broad application prospects.


  • Open Access

    Corrosion Behavior of Homogenized and Extruded 1100 Aluminum Alloy in Acidic Salt Spray

    by Yuchao Zhao, Qiang Lu, Qudong Wang, Dezhi Li, Feng Li, Yuzhao Luo

    The 1100 aluminum alloy has been widely used in many industrial fields due to its high specific strength, fracture toughness, excellent thermal conductivity, and corrosion resistance. In this study, the corrosion behavior of the homogenized and hot-extruded 1100 aluminum alloy in acid salt spray environment for different time was studied. The microstructure of the 1100 aluminum alloy before and after corrosion was characterized by an optical microscope (OM), scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS), and a laser scanning confocal microscope (LSCM). The difference in corrosion resistance between the homogenized and extruded 1100 aluminum alloy was analyzed via the electrochemical method. The results indicate that after hot extrusion at 400 °C, the microstructure of the 1100 aluminum alloy changes from an equiaxed crystal structure with (111) preferentially distributed in a fibrous structure with (220) preferentially distributed. There was no obvious dynamic recrystallization occurring during extrusion, and the second-phase particles containing Al-Fe-Si were coarse and unevenly distributed. With the increase in corrosion time, corrosion pits appeared on the surface of the 1100 aluminum alloy, and a corrosion product layer was formed on the surface of the homogenized 1100 aluminum alloy, which reduced the corrosion rate. After 96 h of corrosion, the CPR of the extruded samples was 0.619 mm/a, and that of the homogenized samples was 0.442 mm/a. The corrosion resistance of the extruded 1100 aluminum alloy was affected by the microstructure and the second phase, and no protective layer of corrosion products was formed on the surface, resulting in a faster corrosion rate and deeper corrosion pits.


  • Open Access

    Investigation on the Corrosion Resistance of 3003 Aluminum Alloy in Acidic Salt Spray under Different Processing States

    by Qiang Lu, Yuchao Zhao, Qudong Wang, Dezhi Li

    3003 aluminum alloy exhibits commendable corrosion resistance, ease of processing, and good formability, rendering it extensively utilized across many industrial sectors. In this study, the corrosion behavior of 3003 aluminum alloy in a homogenized state and after hot extrusion deformation in an acidic salt spray environment for different times was studied. The microstructure of the 3003 aluminum alloy in the homogenized state and after hot extrusion was characterized using scanning electron microscopy (SEM), optical microscope (OM), laser scanning confocal microscope (LSCM) etc., while electrochemical methods were employed to study the difference in corrosion resistance between these two states. The results show that corrosion pits on the surface of the homogenized 3003 aluminum alloy increase with time, and corrosion extends along the second phase arrangement, while the hot extruded 3003 aluminum alloy mainly exhibits corrosion pit extension. The grain size of the homogenized 3003 aluminum alloy is larger than that of the hot extruded state, and the second phase is distributed in a reticular pattern. Hot extrusion deformation ensures not only a uniform distribution of the second phase in the 3003 aluminum alloy but also a reduced grain size, an increased grain boundary density, a heightened electrochemical activity in acidic environments, and an augmented pitting density. Compared with the homogenized 3003 aluminum alloy, the pitting density, maximum pitting depth, and weight loss of the hot extruded state are increased.