Manolya Kandemir
Research Subjects
Manolya Kandemir has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
- Ahmet Ferdi Şenol
Department of Civil Engineering, Faculty of Engineering, Bilecik Şeyh Edebali University, Bilecik, Turkey
1 shared publication - Ali Ozer
Department of Materials Science and Engineering University of Illinois at Urbana‐Champaign Urbana Illinois USA
1 shared publication - Fatih Apaydin
Department of Metallurgical and Materials Engineering, Faculty of Engineering, Bilecik Şeyh Edebali University, Bilecik, Turkey
1 shared publication
Latest Publications
- Open Access
- 26 May 2025
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 61 (5) , 1837-1851
The effect of cupola furnace iron slag on the physical and mechanical properties of alkali-activated fly ash-based mortars
This study investigates the physical and mechanical properties of alkali-activated mortars, in which thermal power plant fly ash (FA) was partially replaced by cupola furnace iron slag (IS). An optimal mix design determined through preliminary tests consisted of an aggregate-to-binder ratio of 1.5 (by weight), NaOH solution concentration of 10 M, Na₂SiO₃ (liquid) to NaOH (solid) ratio of 2, and a water-to-binder ratio of 0.3, all maintained consistently across mixtures. Chemical compositions and phase structures of raw materials were characterized using X-ray fluorescence (XRF) and X-ray diffraction (XRD), respectively. Particle size distribution was determined by laser diffraction analysis, and microstructural morphology was examined using scanning electron microscopy (SEM). Bulk density and apparent porosity were measured using Archimedes’ method with water as the immersion medium. Mechanical properties were evaluated through compressive strength and three-point bending tests after 28 days of curing. Results showed that mortars incorporating 75 wt% cupola furnace iron slag as a fly ash replacement exhibited superior performance, achieving a bulk density of 2118 kg/m³, apparent porosity of 12.2%, compressive strength of 44 MPa, and flexural strength of 10.2 MPa. These findings highlight the potential of iron slag as an effective supplementary material in alkali-activated mortars, enhancing mechanical properties and contributing to microstructural densification.
- 26 May 2025
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 61 (5) , 1837-1851
Open AccessThe effect of cupola furnace iron slag on the physical and mechanical properties of alkali-activated fly ash-based mortars
This study investigates the physical and mechanical properties of alkali-activated mortars, in which thermal power plant fly ash (FA) was partially replaced by cupola furnace iron slag (IS). An optimal mix design determined through preliminary tests consisted of an aggregate-to-binder ratio of 1.5 (by weight), NaOH solution concentration of 10 M, Na₂SiO₃ (liquid) to NaOH (solid) ratio of 2, and a water-to-binder ratio of 0.3, all maintained consistently across mixtures. Chemical compositions and phase structures of raw materials were characterized using X-ray fluorescence (XRF) and X-ray diffraction (XRD), respectively. Particle size distribution was determined by laser diffraction analysis, and microstructural morphology was examined using scanning electron microscopy (SEM). Bulk density and apparent porosity were measured using Archimedes’ method with water as the immersion medium. Mechanical properties were evaluated through compressive strength and three-point bending tests after 28 days of curing. Results showed that mortars incorporating 75 wt% cupola furnace iron slag as a fly ash replacement exhibited superior performance, achieving a bulk density of 2118 kg/m³, apparent porosity of 12.2%, compressive strength of 44 MPa, and flexural strength of 10.2 MPa. These findings highlight the potential of iron slag as an effective supplementary material in alkali-activated mortars, enhancing mechanical properties and contributing to microstructural densification.