Abstract
An 18-multifilamentary MgB 2 wire, classified within the 250 m-class, was produced utilizing a technique to improve the uniformity of powder filling by employing three-dimensional vibrators. A comprehensive evaluation of the fabricated wire revealed that the uniformity of the critical current ( I c ) and fill factor, determined through the coefficient of variation, were 2 and 4%, respectively, along the wire direction. Building upon this achievement, a scaled-up MgB 2 wire was fabricated, with dimensions of approximately 3 km in length and 0.83 mm in diameter. At 20 K and 2 T, the I c was measured to be 191 A. The corresponding critical current density ( J c ), determined to be 190,000 A/cm 2 , represents a significant improvement when compared to that yielded by the conventional gravity-based powder filling method.
Funding Information
  • Ministry of Science and ICT, South Korea
  • National R&D Program, National Research Foundation of Korea (2022M3I9A1076881)
  • Gangwon Province, Kangwon High Magnetic Field Research Center
  • Gangwon Technopark

This publication has 14 references indexed in Scilit: