Tomoaki Yoshino
Research Subjects
Tomoaki Yoshino has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Tatsuhiko Aizawa
Surface Engineering Design Laboratory, Shibaura Institute of Technology, Tokyo 144-0056, Japan
13 shared publications - Tomomi Shiratori
University of Toyama
8 shared publications - Yohei Suzuki
Komatsu-Seiki Kosakusho, Co., Ltd., Suwa 392-0012, Japan
8 shared publications - Tadahiko Inohara
LPS-Works, Co., Ltd., Tokyo 144-0033, Japan
2 shared publications - Tatsuya Fukuda
Tokai Engineering Service, Co., Ltd., Gifu 504-0852, Japan
2 shared publications - Abdelrahman Farghali
Department of Mechanical Engineering, The University of Tokyo, 7-3-1 Hongo, Bunkyo-ku, Bunkyo-ku, Tokyo, 113-0033, JAPAN
1 shared publication
Latest Publications
- Open Access
- 14 September 2022
- Published by IntechOpen
Nitrogen Supersaturation of AISI316 Base Stainless Steels at 673 K and 623 K for Hardening and Microstructure Control
The high-density plasma nitriding at 673 K and 623 K was employed to make 10% of nitrogen supersaturation on AISI316 base austenitic stainless steels. The processing parameters and nitrogen-hydrogen gas flow ratio were optimized to increase the yield of N2+ ion and NH-radical for efficient nitriding. The nitrided AISI316 specimens were prepared for multidimensional analysis to describe the fundamental features of low-temperature plasma nitriding. First, macroscopic evaluation revealed that nitrogen supersaturation induced the γ-lattice expansion and the higher nitrogen content than 4% of mass in depth. The mesoscopic analysis describes the holding temperature and initial grain-size effects on the microstructure changes. Plastic straining, grain-size refinement, and nitrogen zone-boundary diffusion processes advance with nitrogen supersaturation to drive the inner nitriding behavior. The microscopic analysis explains the microstructure refinement, the two-phase structuring, and the microstructure modification. Through this multi-dimensional analysis, the essential characteristics of the low-temperature plasma nitriding of 316 austenitic stainless steels were precisely understood to extend the engineering treatise on the bulk nitrogen stainless steels for surface modification and treatment of stainless steels by nitriding. This plasma nitriding was applied to strengthen and harden the AISI316 wire surfaces toward its application on surgery wires.
- 14 September 2022
- Published by IntechOpen
Open AccessNitrogen Supersaturation of AISI316 Base Stainless Steels at 673 K and 623 K for Hardening and Microstructure Control
The high-density plasma nitriding at 673 K and 623 K was employed to make 10% of nitrogen supersaturation on AISI316 base austenitic stainless steels. The processing parameters and nitrogen-hydrogen gas flow ratio were optimized to increase the yield of N2+ ion and NH-radical for efficient nitriding. The nitrided AISI316 specimens were prepared for multidimensional analysis to describe the fundamental features of low-temperature plasma nitriding. First, macroscopic evaluation revealed that nitrogen supersaturation induced the γ-lattice expansion and the higher nitrogen content than 4% of mass in depth. The mesoscopic analysis describes the holding temperature and initial grain-size effects on the microstructure changes. Plastic straining, grain-size refinement, and nitrogen zone-boundary diffusion processes advance with nitrogen supersaturation to drive the inner nitriding behavior. The microscopic analysis explains the microstructure refinement, the two-phase structuring, and the microstructure modification. Through this multi-dimensional analysis, the essential characteristics of the low-temperature plasma nitriding of 316 austenitic stainless steels were precisely understood to extend the engineering treatise on the bulk nitrogen stainless steels for surface modification and treatment of stainless steels by nitriding. This plasma nitriding was applied to strengthen and harden the AISI316 wire surfaces toward its application on surgery wires.
- Open Access
- 20 April 2022
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 6 (3) , 49
Fabrication of Punch and Die Using Plasma-Assisted 3D Printing Technology for Piercing Sheet Metals
A pair of punch and die was often fabricated using subtractive manufacturing processes such as milling and other machining processes. However, additive manufacturing could be used to perform the same processes. This study explored this possibility. In particular, this study fabricated a pair of T-shaped punch and die made of AISI316L austenitic stainless steel using an additive manufacturing process called plasma-assisted 3D printing. Accordingly, T-shaped negative and positive 2D patterns were screen-printed onto the mirror-polished surfaces of the substrates made of AISI316L austenitic stainless steel. The printed film worked like a mask to prevent the printed substrate surfaces from nitriding. In order to form a thick nitrided layer, the unprinted substrate surfaces were selectively nitrided at 673 K for 14.4 ks. The un-nitrided segments of the substrates were uniformly removed by sand-blasting that involved shooting silica particles on the substrate’s surfaces. As a result, the substrates printed with negative and positive T-shaped patterns were transformed into the punch head and die cavity. In order to see the efficacy of the fabricated punch and die pair, this pair was used for piercing the electrical steel sheets under a controlled clearance. Scanning Electron Microscopy with Energy Dispersive X-ray (SEM-EDX) was used to measure surface topography after piercing. In addition, SEM and a 3D profilometer were used to measure the punch and die profiles after piercing. The abovementioned measurement results showed that the fabricated punch and die exhibited highly accurate piercing behavior. Thus, the plasma-assisted 3D printing was useful for punch and die fabrication.
- 20 April 2022
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 6 (3) , 49
Open AccessFabrication of Punch and Die Using Plasma-Assisted 3D Printing Technology for Piercing Sheet Metals
A pair of punch and die was often fabricated using subtractive manufacturing processes such as milling and other machining processes. However, additive manufacturing could be used to perform the same processes. This study explored this possibility. In particular, this study fabricated a pair of T-shaped punch and die made of AISI316L austenitic stainless steel using an additive manufacturing process called plasma-assisted 3D printing. Accordingly, T-shaped negative and positive 2D patterns were screen-printed onto the mirror-polished surfaces of the substrates made of AISI316L austenitic stainless steel. The printed film worked like a mask to prevent the printed substrate surfaces from nitriding. In order to form a thick nitrided layer, the unprinted substrate surfaces were selectively nitrided at 673 K for 14.4 ks. The un-nitrided segments of the substrates were uniformly removed by sand-blasting that involved shooting silica particles on the substrate’s surfaces. As a result, the substrates printed with negative and positive T-shaped patterns were transformed into the punch head and die cavity. In order to see the efficacy of the fabricated punch and die pair, this pair was used for piercing the electrical steel sheets under a controlled clearance. Scanning Electron Microscopy with Energy Dispersive X-ray (SEM-EDX) was used to measure surface topography after piercing. In addition, SEM and a 3D profilometer were used to measure the punch and die profiles after piercing. The abovementioned measurement results showed that the fabricated punch and die exhibited highly accurate piercing behavior. Thus, the plasma-assisted 3D printing was useful for punch and die fabrication.
- Open Access
- 31 March 2022
- Published by MDPI AG in Micromachines
- Vol. 13 (4) , 562
Quantitative Characterization of the Affected Zones in a Single Crystal Fe-6Si Steel Sheet by Fine Piercing
An iron loss in the motor core was often enhanced by formation of plastically affected zones in piercing the electrical steel sheets. A platform methodology to carry out quantitative evaluation of these affected zones in the pierced electrical steel sheets was proposed to search for the way to minimize the affected zone widths. A coarse-grained electrical steel sheet was employed as a work material for a fine piercing experiment under the narrowed clearance between the plasma-nitrided SKD11 punch and core-die. The shearing behavior by the applied loading for piercing was described by in situ measurement of the load-stroke relationship. The plastic straining in the single-crystal electrical steel sheet was characterized by SEM (scanning electron microscopy) and EBSD (electron back-scattering diffraction) to define the affected zone size and to analyze the rotation of crystallographic orientations by the induced plastic distortion during piercing. Integral and differentiation of spin rotation measured the affected zones. The effect of punch edge sharpness on these spin-rotation measures was also discussed using the nitrided and ion-milled SKD11 punch and core-die.
- 31 March 2022
- Published by MDPI AG in Micromachines
- Vol. 13 (4) , 562
Open AccessQuantitative Characterization of the Affected Zones in a Single Crystal Fe-6Si Steel Sheet by Fine Piercing
An iron loss in the motor core was often enhanced by formation of plastically affected zones in piercing the electrical steel sheets. A platform methodology to carry out quantitative evaluation of these affected zones in the pierced electrical steel sheets was proposed to search for the way to minimize the affected zone widths. A coarse-grained electrical steel sheet was employed as a work material for a fine piercing experiment under the narrowed clearance between the plasma-nitrided SKD11 punch and core-die. The shearing behavior by the applied loading for piercing was described by in situ measurement of the load-stroke relationship. The plastic straining in the single-crystal electrical steel sheet was characterized by SEM (scanning electron microscopy) and EBSD (electron back-scattering diffraction) to define the affected zone size and to analyze the rotation of crystallographic orientations by the induced plastic distortion during piercing. Integral and differentiation of spin rotation measured the affected zones. The effect of punch edge sharpness on these spin-rotation measures was also discussed using the nitrided and ion-milled SKD11 punch and core-die.
- Open Access
- 6 February 2022
- Published by MDPI AG in Micromachines
- Vol. 13 (2) , 265
Micro-/Nano-Texturing onto Plasma-Nitrided Tool Surface by Laser Printing for CNC Imprinting and Piercing
A new data transformation method for micro-manufacturing using a topological model for a micro-/nano-texture was proposed for a surface-decorated product. Femtosecond laser printing was utilized to form the micro-/nano-textures into the hardened thick layer of dies by plasma nitriding. At first, the plasma-nitrided AISI316L flat substrate was laser-printed as a punch to imprint the tailored nano-textures onto the AA1060 aluminum plate for its surface decoration with topological emblems. Second, the plasma-nitrided SKD11 cylindrical punch was laser-trimmed to form the nanostructures on its side surface. This nano-texture was imprinted onto the hole surface concurrently with piercing a circular hole into electrical steel sheet. The fully burnished surface had a shiny, metallic quality due to the nano-texturing. The plasma nitriding, the laser printing and the CNC (computer numerical control) imprinting provided a way of transforming the tailored textures on the metallic product.
- 6 February 2022
- Published by MDPI AG in Micromachines
- Vol. 13 (2) , 265
Open AccessMicro-/Nano-Texturing onto Plasma-Nitrided Tool Surface by Laser Printing for CNC Imprinting and Piercing
A new data transformation method for micro-manufacturing using a topological model for a micro-/nano-texture was proposed for a surface-decorated product. Femtosecond laser printing was utilized to form the micro-/nano-textures into the hardened thick layer of dies by plasma nitriding. At first, the plasma-nitrided AISI316L flat substrate was laser-printed as a punch to imprint the tailored nano-textures onto the AA1060 aluminum plate for its surface decoration with topological emblems. Second, the plasma-nitrided SKD11 cylindrical punch was laser-trimmed to form the nanostructures on its side surface. This nano-texture was imprinted onto the hole surface concurrently with piercing a circular hole into electrical steel sheet. The fully burnished surface had a shiny, metallic quality due to the nano-texturing. The plasma nitriding, the laser printing and the CNC (computer numerical control) imprinting provided a way of transforming the tailored textures on the metallic product.
- Open Access
- 18 August 2021
- Published by IntechOpen
Laser Treatment CVD Diamond Coated Punch for Ultra-Fine Piercing of Metallic Sheets
CVD-diamond coated special tools have been widely utilized to prolong their tool life in practical production lines. WC (Co) punch for fine piercing of metallic sheets required for high wear-toughness to be free from chipping and damages and for high product quality to punch out the holes with sufficient dimensional accuracy. The laser trimming process was developed to reduce the surface roughness of diamond coating down to submicron level and to adjust its diamond layer dimensions with a sharp punch edge for accurate piercing. The pulsed laser irradiation was employed to demonstrate that micro-groove was accurately formed into the diamond coating. Less deterioration in the worked diamond film by this laser treatment was proved by the Raman spectroscopy. The femtosecond laser trimming was proposed to sharpen the punch edge down to 2 μm and to form the nano-textured punch side surfaces with the LIPSS (Laser Induced Periodic Surface Structuring)-period of 300 nm. Fine piercing experiments were performed to demonstrate that punch life was significantly extended to continuous punching in more than 10,000 shots and that mirror-shining hole surfaces were attained in every shot by regularly coining the nanotextures. The sharp punch edge with homogeneous edge profile was responsible for reduction of the induced damages into work sheet by piercing. The punch life was extended by the ejection mechanism of debris particles through the nanotextures on the punch side surface. The present laser treatment was useful in trimming and nanostructuring the complex-shaped punch edge for industrial application.
- 18 August 2021
- Published by IntechOpen
Open AccessLaser Treatment CVD Diamond Coated Punch for Ultra-Fine Piercing of Metallic Sheets
CVD-diamond coated special tools have been widely utilized to prolong their tool life in practical production lines. WC (Co) punch for fine piercing of metallic sheets required for high wear-toughness to be free from chipping and damages and for high product quality to punch out the holes with sufficient dimensional accuracy. The laser trimming process was developed to reduce the surface roughness of diamond coating down to submicron level and to adjust its diamond layer dimensions with a sharp punch edge for accurate piercing. The pulsed laser irradiation was employed to demonstrate that micro-groove was accurately formed into the diamond coating. Less deterioration in the worked diamond film by this laser treatment was proved by the Raman spectroscopy. The femtosecond laser trimming was proposed to sharpen the punch edge down to 2 μm and to form the nano-textured punch side surfaces with the LIPSS (Laser Induced Periodic Surface Structuring)-period of 300 nm. Fine piercing experiments were performed to demonstrate that punch life was significantly extended to continuous punching in more than 10,000 shots and that mirror-shining hole surfaces were attained in every shot by regularly coining the nanotextures. The sharp punch edge with homogeneous edge profile was responsible for reduction of the induced damages into work sheet by piercing. The punch life was extended by the ejection mechanism of debris particles through the nanotextures on the punch side surface. The present laser treatment was useful in trimming and nanostructuring the complex-shaped punch edge for industrial application.
- Open Access
- 17 May 2021
- Published by MDPI AG in Micromachines
- Vol. 12 (5) , 568
Femtosecond Laser Trimming with Simultaneous Nanostructuring to Fine Piercing Punch to Electrical Amorphous Steel Sheets
A CVD (Chemical Vapor Deposition) diamond coated tungsten carbide (WC) and cobalt (Co) sintered alloy punch was trimmed by the femtosecond laser machining to sharpen its edge with about 2 μm and to simultaneously make nanostructuring to its side surface. In addition to the sharpened edge, its edge profile was formed to be homogeneous enough to reduce the damage layer width by piercing the electrical amorphous steel sheet stack. Each brittle sheet in the stacked work was damaged to have three kinds of defects by piercing; e.g., the droop-like cracking in the thickness and at the vicinity of hole, the wrinkling in peak-to-valley with partial cracking on the peaks, and the circumferential cracking. When using the WC (Co) punch with the inhomogeneous edge profile in the sharpened edge width, these three damages were induced into each sheet and the maximum damage width exceeded 80 μm. When using the punch with the sharpened edge and homogeneous edge profile, the wrinkling mode was saved and the total affected layer width was significantly reduced to less than 20 μm. Through the precise embossing experiments, this effect of punch edge profile condition to the induced damages was discussed with a statement on the nanostructuring effect on the reduction of damaged width in electrical amorphous steel sheets. The developed tool with the sharpened edge and homogenous edge condition contributes to the realization of a low iron loss motor with a reduced affected layer width.
- 17 May 2021
- Published by MDPI AG in Micromachines
- Vol. 12 (5) , 568
Open AccessFemtosecond Laser Trimming with Simultaneous Nanostructuring to Fine Piercing Punch to Electrical Amorphous Steel Sheets
A CVD (Chemical Vapor Deposition) diamond coated tungsten carbide (WC) and cobalt (Co) sintered alloy punch was trimmed by the femtosecond laser machining to sharpen its edge with about 2 μm and to simultaneously make nanostructuring to its side surface. In addition to the sharpened edge, its edge profile was formed to be homogeneous enough to reduce the damage layer width by piercing the electrical amorphous steel sheet stack. Each brittle sheet in the stacked work was damaged to have three kinds of defects by piercing; e.g., the droop-like cracking in the thickness and at the vicinity of hole, the wrinkling in peak-to-valley with partial cracking on the peaks, and the circumferential cracking. When using the WC (Co) punch with the inhomogeneous edge profile in the sharpened edge width, these three damages were induced into each sheet and the maximum damage width exceeded 80 μm. When using the punch with the sharpened edge and homogeneous edge profile, the wrinkling mode was saved and the total affected layer width was significantly reduced to less than 20 μm. Through the precise embossing experiments, this effect of punch edge profile condition to the induced damages was discussed with a statement on the nanostructuring effect on the reduction of damaged width in electrical amorphous steel sheets. The developed tool with the sharpened edge and homogenous edge condition contributes to the realization of a low iron loss motor with a reduced affected layer width.
- Open Access
Free-Forging of Pure Titanium with High Reduction of Thickness by Plasma-Carburized SKD11 Dies
A tool steel type SKD11 punch was plasma carburized at 673 K for 14.4 ks at 70 Pa to make carbon supersaturation. This carburized SKD11 punch was employed for upsetting the pure titanium wire with the diameter of 1.00 mm up to the reduction of thickness by 70% in a single shot. Its contact interface to titanium work was analyzed to describe the anti-galling behavior in this forging. Little trace of titanium proved that the galling process was suppressed by the in situ solid lubrication. The isolated free carbon agglomerates are wrought as a solid lubricant to sustain the galling-free forging process. This anti-galling upsetting reduced the residual strains in the forged wires. A long titanium wire with a length of 45 mm was incrementally upset to yield the titanium ribbon with a thickness of 0.3 mm, the width of 2.3 mm, and the length of 50 mm. The grain size of original pure titanium was much reduced to 2 μm on average. A micro-pillared microtexture was imprinted onto this forged titanium ribbon.
Open AccessFree-Forging of Pure Titanium with High Reduction of Thickness by Plasma-Carburized SKD11 Dies
A tool steel type SKD11 punch was plasma carburized at 673 K for 14.4 ks at 70 Pa to make carbon supersaturation. This carburized SKD11 punch was employed for upsetting the pure titanium wire with the diameter of 1.00 mm up to the reduction of thickness by 70% in a single shot. Its contact interface to titanium work was analyzed to describe the anti-galling behavior in this forging. Little trace of titanium proved that the galling process was suppressed by the in situ solid lubrication. The isolated free carbon agglomerates are wrought as a solid lubricant to sustain the galling-free forging process. This anti-galling upsetting reduced the residual strains in the forged wires. A long titanium wire with a length of 45 mm was incrementally upset to yield the titanium ribbon with a thickness of 0.3 mm, the width of 2.3 mm, and the length of 50 mm. The grain size of original pure titanium was much reduced to 2 μm on average. A micro-pillared microtexture was imprinted onto this forged titanium ribbon.
- Open Access
Microstructure/Mechanical Characterization of Plasma Nitrided Fine-Grain Austenitic Stainless Steels in Low Temperature
Fine-grained austenitic stainless steels (FGSS) were plasma nitrided below 700 K to describe their microstructure evolution during the nitrogen supersaturation process and to investigate the post-stressing effect on the microstructure and mechanical properties of nitrided FGSS. Normal- and fine-grained AISI304 plates were nitrided at 623 K and 673 K to investigate the grain size effect on the nitrogen supersaturation process as well as the microstructure evolution during the nitriding process. Fine-grained AISI316 (FGSS316) wires were nitrided at 623 K to demonstrate that their outer surfaces were uniformly nitrided to have the same two-phase, refined microstructure with high nitrogen solute content. This nitrided FGSS316 wire had a core structure where the original FGSS316 core matrix was bound by the nitrided FGSS316 layer. The nitrided wire had higher stiffness, ultimate strength, and elongation in the uniaxial tensile testing than its un-nitrided wires. The core microstructure was refined and homogenized by this applied loading together with an increase of nitrided layer hardness.
Open AccessMicrostructure/Mechanical Characterization of Plasma Nitrided Fine-Grain Austenitic Stainless Steels in Low Temperature
Fine-grained austenitic stainless steels (FGSS) were plasma nitrided below 700 K to describe their microstructure evolution during the nitrogen supersaturation process and to investigate the post-stressing effect on the microstructure and mechanical properties of nitrided FGSS. Normal- and fine-grained AISI304 plates were nitrided at 623 K and 673 K to investigate the grain size effect on the nitrogen supersaturation process as well as the microstructure evolution during the nitriding process. Fine-grained AISI316 (FGSS316) wires were nitrided at 623 K to demonstrate that their outer surfaces were uniformly nitrided to have the same two-phase, refined microstructure with high nitrogen solute content. This nitrided FGSS316 wire had a core structure where the original FGSS316 core matrix was bound by the nitrided FGSS316 layer. The nitrided wire had higher stiffness, ultimate strength, and elongation in the uniaxial tensile testing than its un-nitrided wires. The core microstructure was refined and homogenized by this applied loading together with an increase of nitrided layer hardness.
- Open Access
- 9 January 2021
- Published by MDPI AG in Applied Sciences
- Vol. 11 (2) , 595
Anti-Galling Cold, Dry Forging of Pure Titanium by Plasma-Carburized AISI420J2 Dies
A bare AISI420J2 punch often suffers from severe adhesion of metallic titanium as well as titanium oxide debris particles in dry, cold forging of biomedical titanium alloys. This punch was plasma-carburized at 673 K for 14.4 ks to harden it up to 1200 HV on average and to achieve carbon supersaturation in the carburized layer. This plasma-carburized punch was employed in the cold, dry forging of a pure titanium wire into a flat plate while reducing the thickness by 70%. The contact interface width approached the forged workpiece width with increasing the reduction ratio. This smaller bulging deformation reveals that the workpiece is upset by homogeneous plastic flow with a lower friction coefficient. This low-friction and anti-galling forging process was sustained by an in situ solid lubrication mechanism. Unbound free carbon was isolated from the carbon-supersaturated AISI420J2 matrix and deposited as a thin tribofilm to protect the contact interface from mass transfer of metallic titanium.
- 9 January 2021
- Published by MDPI AG in Applied Sciences
- Vol. 11 (2) , 595
Open AccessAnti-Galling Cold, Dry Forging of Pure Titanium by Plasma-Carburized AISI420J2 Dies
A bare AISI420J2 punch often suffers from severe adhesion of metallic titanium as well as titanium oxide debris particles in dry, cold forging of biomedical titanium alloys. This punch was plasma-carburized at 673 K for 14.4 ks to harden it up to 1200 HV on average and to achieve carbon supersaturation in the carburized layer. This plasma-carburized punch was employed in the cold, dry forging of a pure titanium wire into a flat plate while reducing the thickness by 70%. The contact interface width approached the forged workpiece width with increasing the reduction ratio. This smaller bulging deformation reveals that the workpiece is upset by homogeneous plastic flow with a lower friction coefficient. This low-friction and anti-galling forging process was sustained by an in situ solid lubrication mechanism. Unbound free carbon was isolated from the carbon-supersaturated AISI420J2 matrix and deposited as a thin tribofilm to protect the contact interface from mass transfer of metallic titanium.
- Open Access
Dry Cold Forging of Pure Titanium Wire to Thin Plate with Use of β-SiC Coating Dies
Dense β-SiC coating with 3C-structure was utilized as a dry cold forging punch and core-die. Pure titanium T328H wires of industrial grade II were employed as a work material. No adhesion or galling of metallic titanium was detected on the contact interface between this β-SiC die and titanium work, even after this continuous forging process, up to a reduction in thickness by 70%. SEM (Scanning Electron Microscopy) and EDX (Electron Dispersive X-ray spectroscopy) were utilized to analyze this contact interface. A very thin titanium oxide layer was in situ formed in the radial direction from the center of the contact interface. Isolated carbon from β-SiC agglomerated and distributed in dots at the center of the initial contact interface. Raman spectroscopy was utilized, yielding the discovery that this carbon is unbound as a free carbon or not bound in SiC or TiC and that intermediate titanium oxides are formed with TiO2 as a tribofilm.
Open AccessDry Cold Forging of Pure Titanium Wire to Thin Plate with Use of β-SiC Coating Dies
Dense β-SiC coating with 3C-structure was utilized as a dry cold forging punch and core-die. Pure titanium T328H wires of industrial grade II were employed as a work material. No adhesion or galling of metallic titanium was detected on the contact interface between this β-SiC die and titanium work, even after this continuous forging process, up to a reduction in thickness by 70%. SEM (Scanning Electron Microscopy) and EDX (Electron Dispersive X-ray spectroscopy) were utilized to analyze this contact interface. A very thin titanium oxide layer was in situ formed in the radial direction from the center of the contact interface. Isolated carbon from β-SiC agglomerated and distributed in dots at the center of the initial contact interface. Raman spectroscopy was utilized, yielding the discovery that this carbon is unbound as a free carbon or not bound in SiC or TiC and that intermediate titanium oxides are formed with TiO2 as a tribofilm.