Paramasivam Sivaraj
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Paramasivam Sivaraj has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
- Tushar Sonar
Department of Welding Equipment and Technology, Institution of Engineering and Technology, South Ural State University (National Research University), Chelyabinsk, Russia
6 shared publications - Venkatakrishnan Balasubramanian
Annamalai University
6 shared publications - Chakkaravarthi Rajarajan
Department of Mechanical Engineering , Meenakshi Ramaswamy Engineering College , Thathanur 621804, Tamil Nadu , India
5 shared publications V. Balasubramanian
Center for Material Joining and Research (CEMAJOR), Annamalai University
5 shared publications- Dhamothara Kannan Thirumalaikkannan
School of Mechanical Engineering (SMEC), Vellore Institute of Technology (VIT), Vellore, India
3 shared publications - C. Mukundhan
Centre for Materials Joining and Research (CEMAJOR), Department of Manufacturing Engineering, Annamalai University, Annamalai Nagar, Chidambaram 608002, Tamil Nadu, India
2 shared publications
Latest Publications
- Open Access
- 19 March 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (7)
Influence of Tool Traverse Speed on Microstructural Characteristics and Mechanical Properties of Friction Stir Processed AA5754 Aluminium Alloy Under Overlap Configuration
AA5754-H111, a non-heat-treatable aluminium alloy of the 5000 series, is widely used in automotive and marine structures owing to its good strength-to-weight ratio, with strength enhancement achieved through strain hardening. Friction Stir Processing (FSP), derived from the Friction Stir Welding (FSW) technique, is increasingly applied to refine microstructures in the stir zone under solid-state conditions, thereby avoiding solidification-related defects. The effectiveness of FSP depends largely on three process parameters: tool rotational speed, tool traverse speed, and tool tilt angle. Although considerable work has been conducted on these parameters for aluminium alloys, the influence of tool traverse speed on AA5754 under overlap configuration has not been reported. In this study, two overlapped AA5754 plates (6 mm each) were processed using a tapered threaded HSS tool at three different traverse speeds (10, 15, and 20 mm/min), with other parameters kept constant. Post-FSP, the stir zone was examined through optical microscopy and XRD analysis, and tensile properties were evaluated. Results revealed that a traverse speed of 15 mm/min produced a defect-free stir zone and delivered the highest tensile properties, with an ultimate tensile strength of 232 MPa, yield strength of 192 MPa, and elongation of 37%, compared to the base metal values of 181 MPa, 167 MPa, and 14%, respectively. From the micro-structural evaluation, it is observed that the formation of a fine, equiaxed dynamically recrystallized grain structure in the stir zone, along with reduced grain size and homogeneous microstructural distribution as compared to the base material. The findings confirm that tool traverse speed critically controls heat generation and thereby governs microstructural refinement and mechanical performance of AA5754 alloy joints.
- 19 March 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (7)
Open AccessInfluence of Tool Traverse Speed on Microstructural Characteristics and Mechanical Properties of Friction Stir Processed AA5754 Aluminium Alloy Under Overlap Configuration
AA5754-H111, a non-heat-treatable aluminium alloy of the 5000 series, is widely used in automotive and marine structures owing to its good strength-to-weight ratio, with strength enhancement achieved through strain hardening. Friction Stir Processing (FSP), derived from the Friction Stir Welding (FSW) technique, is increasingly applied to refine microstructures in the stir zone under solid-state conditions, thereby avoiding solidification-related defects. The effectiveness of FSP depends largely on three process parameters: tool rotational speed, tool traverse speed, and tool tilt angle. Although considerable work has been conducted on these parameters for aluminium alloys, the influence of tool traverse speed on AA5754 under overlap configuration has not been reported. In this study, two overlapped AA5754 plates (6 mm each) were processed using a tapered threaded HSS tool at three different traverse speeds (10, 15, and 20 mm/min), with other parameters kept constant. Post-FSP, the stir zone was examined through optical microscopy and XRD analysis, and tensile properties were evaluated. Results revealed that a traverse speed of 15 mm/min produced a defect-free stir zone and delivered the highest tensile properties, with an ultimate tensile strength of 232 MPa, yield strength of 192 MPa, and elongation of 37%, compared to the base metal values of 181 MPa, 167 MPa, and 14%, respectively. From the micro-structural evaluation, it is observed that the formation of a fine, equiaxed dynamically recrystallized grain structure in the stir zone, along with reduced grain size and homogeneous microstructural distribution as compared to the base material. The findings confirm that tool traverse speed critically controls heat generation and thereby governs microstructural refinement and mechanical performance of AA5754 alloy joints.
- Open Access
- 1 July 2025
- Published by IOP Publishing in Materials Research Express
- Vol. 12 (7) , 076515
Influence of tool rotational speed on microstructural characteristics and mechanical properties of friction stir processed AA5754 aluminium alloy under overlap configuration
Friction Stir Processing (FSP) is a variant of the Friction Stir Welding (FSW) technique. Recently, FSP has been extensively used to modify the microstructure of many low-temperature alloys and subsequently to enhance the mechanical properties. Dynamic recrystallization caused by the rotating tool is the main reason for modifying (refining) the microstructure in the stir zone. Since this process operates under solid-state conditions, it eliminates many solidification-related problems. In this research work, 6-mm-thick AA5754 aluminium alloy sheets were overlapped to attain a total thickness of 12 mm. A tapered-threaded HSS tool was then used to perform friction stir processing at the center of the overlapped plates using five different rotational speeds. The other parameters were kept constant. This investigation found that a tool’s rotational speed of 700 rpm yielded a defect-free FSP region, likely due to optimum heat generation under this condition. Moreover, the FSP material at 700 rpm exhibited a maximum tensile strength of 245 MPa. This is mainly due to the formation of finer grains and more refined strengthening precipitates in the FSP region. It is concluded that the tool’s rotational speed plays a vital role in heat generation and subsequently influences the microstructure and mechanical properties.
- 1 July 2025
- Published by IOP Publishing in Materials Research Express
- Vol. 12 (7) , 076515
Open AccessInfluence of tool rotational speed on microstructural characteristics and mechanical properties of friction stir processed AA5754 aluminium alloy under overlap configuration
Friction Stir Processing (FSP) is a variant of the Friction Stir Welding (FSW) technique. Recently, FSP has been extensively used to modify the microstructure of many low-temperature alloys and subsequently to enhance the mechanical properties. Dynamic recrystallization caused by the rotating tool is the main reason for modifying (refining) the microstructure in the stir zone. Since this process operates under solid-state conditions, it eliminates many solidification-related problems. In this research work, 6-mm-thick AA5754 aluminium alloy sheets were overlapped to attain a total thickness of 12 mm. A tapered-threaded HSS tool was then used to perform friction stir processing at the center of the overlapped plates using five different rotational speeds. The other parameters were kept constant. This investigation found that a tool’s rotational speed of 700 rpm yielded a defect-free FSP region, likely due to optimum heat generation under this condition. Moreover, the FSP material at 700 rpm exhibited a maximum tensile strength of 245 MPa. This is mainly due to the formation of finer grains and more refined strengthening precipitates in the FSP region. It is concluded that the tool’s rotational speed plays a vital role in heat generation and subsequently influences the microstructure and mechanical properties.
- Open Access
- 7 May 2024
- Published by IOP Publishing in Physica Scripta
- Vol. 99 (6) , 065926
Role of oscillation frequency and amplitude on the microstructure and properties of linear friction welded nickel aluminium bronze joints
This study explores the influence of oscillation frequency and amplitude on the quality of linear friction welded joints using as-cast nickel aluminium bronze. Welding was conducted at 30 Hz, 50 Hz, and 70 Hz oscillated frequencies and amplitudes of 1.5 mm, 2 mm, and 3 mm. The joint’s performance was thoroughly investigated through systematic analysis, including macrostructure examination, peak interfacial temperature measurement, microstructure evaluation, strain assessment, cooling rate determination, microhardness testing, and tensile property characterization. The width of the weld zone varied from 183 μm to 297 μm, and the thermomechanical affected zone (TMAZ) area ranged from 4.48 mm2 to 14.79 mm2 across different process parameters. In the parent material, the volume fraction of the β-phase was as low as 20.2%, contrasting with the dominant α-phase at 79.8%. The average grain size of the lamellar and globular α-phase mixture was 26.4 μm. Notably, the weld zone exhibited extremely refined α-phase grains, with diameters less than 5 μm in all cases. The volume fraction of the β‘-phase increased significantly with higher frequencies, from 15.299% at 30 Hz to 26.98% at 50 Hz, peaking at 40.08% at 70 Hz, leading to varying k phases. This variation in microstructure had a substantial impact on mechanical properties. Tensile strength ranged from 503 MPa to 582 MPa, while ductility varied from 13.5% to 21.7%. Additionally, the hardness of the parent material increased from approximately 155 Hv to 260 Hv. This study demonstrates that controlling the oscillation frequency and amplitude in linear friction welding processes can yield consistent, high-quality welds in nickel aluminium bronze.
- 7 May 2024
- Published by IOP Publishing in Physica Scripta
- Vol. 99 (6) , 065926
Open AccessRole of oscillation frequency and amplitude on the microstructure and properties of linear friction welded nickel aluminium bronze joints
This study explores the influence of oscillation frequency and amplitude on the quality of linear friction welded joints using as-cast nickel aluminium bronze. Welding was conducted at 30 Hz, 50 Hz, and 70 Hz oscillated frequencies and amplitudes of 1.5 mm, 2 mm, and 3 mm. The joint’s performance was thoroughly investigated through systematic analysis, including macrostructure examination, peak interfacial temperature measurement, microstructure evaluation, strain assessment, cooling rate determination, microhardness testing, and tensile property characterization. The width of the weld zone varied from 183 μm to 297 μm, and the thermomechanical affected zone (TMAZ) area ranged from 4.48 mm2 to 14.79 mm2 across different process parameters. In the parent material, the volume fraction of the β-phase was as low as 20.2%, contrasting with the dominant α-phase at 79.8%. The average grain size of the lamellar and globular α-phase mixture was 26.4 μm. Notably, the weld zone exhibited extremely refined α-phase grains, with diameters less than 5 μm in all cases. The volume fraction of the β‘-phase increased significantly with higher frequencies, from 15.299% at 30 Hz to 26.98% at 50 Hz, peaking at 40.08% at 70 Hz, leading to varying k phases. This variation in microstructure had a substantial impact on mechanical properties. Tensile strength ranged from 503 MPa to 582 MPa, while ductility varied from 13.5% to 21.7%. Additionally, the hardness of the parent material increased from approximately 155 Hv to 260 Hv. This study demonstrates that controlling the oscillation frequency and amplitude in linear friction welding processes can yield consistent, high-quality welds in nickel aluminium bronze.
- 19 January 2023
- Published by Springer Nature in International Journal on Interactive Design and Manufacturing (IJIDeM)
- Vol. 18 (3) , 1731-1759
Unsymmetric rod to plate rotary friction welding of dissimilar martensitic stainless steel and low carbon steel for automotive applications–mathematical modeling and optimization
- 19 January 2023
- Published by Springer Nature in International Journal on Interactive Design and Manufacturing (IJIDeM)
- Vol. 18 (3) , 1731-1759
Unsymmetric rod to plate rotary friction welding of dissimilar martensitic stainless steel and low carbon steel for automotive applications–mathematical modeling and optimization
- Open Access
- 1 January 2023
- Published by Walter de Gruyter GmbH in Journal of the Mechanical Behavior of Materials
- Vol. 32 (1)
Microstructural characteristics and mechanical properties of rotary friction-welded dissimilar AISI 431 steel/AISI 1018 steel joints
The main objective of this study was to analyze the microstructural characteristics and strength performance of dissimilar AISI 431 steel/AISI 1018 steel joints developed using rotary friction welding. The microstructural characteristics of different regions of dissimilar rod-to-plate joints were analyzed using optical microscopy. The tensile properties and microhardness of dissimilar rod-to-plate joints were evaluated to assess the joint performance. The microhardness distribution across the cross-sectional region of dissimilar rod-to-plate joints was recorded and correlated with the tensile failure. Scanning electron microscopy was used to analyze the fractured region of dissimilar rod-to-plate tensile specimens. Results showed that the dissimilar AISI 431 steel/AISI 1018 steel joints steel exhibited a tensile strength of 650 MPa, a yield strength of 452 MPa, and a % elongation of 18%. The microhardness of the weld interface (WI) was higher up to 515 HV 0.5 . The grain growth and resulting lower hardness in heat-affected zone (HAZ) are mainly responsible for the failure of the joints in HAZ only. The superior tensile properties and greater interface hardness of dissimilar AISI 431 steel/AISI 1018 steel joints are correlated with the evolution of finer grain microstructure in the WI zone.
- 1 January 2023
- Published by Walter de Gruyter GmbH in Journal of the Mechanical Behavior of Materials
- Vol. 32 (1)
Open AccessMicrostructural characteristics and mechanical properties of rotary friction-welded dissimilar AISI 431 steel/AISI 1018 steel joints
The main objective of this study was to analyze the microstructural characteristics and strength performance of dissimilar AISI 431 steel/AISI 1018 steel joints developed using rotary friction welding. The microstructural characteristics of different regions of dissimilar rod-to-plate joints were analyzed using optical microscopy. The tensile properties and microhardness of dissimilar rod-to-plate joints were evaluated to assess the joint performance. The microhardness distribution across the cross-sectional region of dissimilar rod-to-plate joints was recorded and correlated with the tensile failure. Scanning electron microscopy was used to analyze the fractured region of dissimilar rod-to-plate tensile specimens. Results showed that the dissimilar AISI 431 steel/AISI 1018 steel joints steel exhibited a tensile strength of 650 MPa, a yield strength of 452 MPa, and a % elongation of 18%. The microhardness of the weld interface (WI) was higher up to 515 HV 0.5 . The grain growth and resulting lower hardness in heat-affected zone (HAZ) are mainly responsible for the failure of the joints in HAZ only. The superior tensile properties and greater interface hardness of dissimilar AISI 431 steel/AISI 1018 steel joints are correlated with the evolution of finer grain microstructure in the WI zone.
- Open Access
- 24 September 2022
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2022, 1-10
Microstructural Features, Tensile Properties, and Impact Toughness of Linear Friction Welded High-Temperature Alloy Joints for Blisk Assembly Applications
The main objective of this investigation is to analyze the microstructure, tensile properties, and impact toughness of Ti6Al4V alloy joints developed using optimized parameters of linear friction welding (LFW) for gas turbine blisk assembly applications. The 6mm thick plates of Ti6Al4V alloy were joined using a friction time of 40sec, a friction pressure of 20MPa, a forging pressure of 10MPa, a forging time of 3sec, and an oscillating frequency of 14Hz. The different regions of joints were analyzed using a stereo zoom microscope. Optical and scanning electron microscope (SEM) was used for analysing the microstructural features of joints. The room temperature tensile properties, hardness, and impact toughness of LFW-Ti6Al4V alloy joints were evaluated and correlated to the microstructural features of weld region. The fractured sections of tensile and impact toughness specimens of joints were analyzed using SEM and the failure of joints was correlated with the hardness survey. Results showed that the LFW-Ti6Al4V alloy joints developed using the optimized parameters exhibited a tensile strength (TS) of 1015MPa, a yield strength (YS) of 940MPa, and an elongation (EL) of 8. The joints revealed 98.54, 95.91, and 66.67 of tensile strength, yield strength, and ductility of the parent metal. The LFW joints disclosed impact toughness (IT) of 17.2J which is 89.77 impact toughness of the parent metal. The superior tensile properties and impact toughness of LFW-Ti6Al4V alloy joints are mainly attributed to a greater degree of refinement of α+β grains in the weld interface, which offers greater resistance to tensile deformation and crack propagation.
- 24 September 2022
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2022, 1-10
Open AccessMicrostructural Features, Tensile Properties, and Impact Toughness of Linear Friction Welded High-Temperature Alloy Joints for Blisk Assembly Applications
The main objective of this investigation is to analyze the microstructure, tensile properties, and impact toughness of Ti6Al4V alloy joints developed using optimized parameters of linear friction welding (LFW) for gas turbine blisk assembly applications. The 6mm thick plates of Ti6Al4V alloy were joined using a friction time of 40sec, a friction pressure of 20MPa, a forging pressure of 10MPa, a forging time of 3sec, and an oscillating frequency of 14Hz. The different regions of joints were analyzed using a stereo zoom microscope. Optical and scanning electron microscope (SEM) was used for analysing the microstructural features of joints. The room temperature tensile properties, hardness, and impact toughness of LFW-Ti6Al4V alloy joints were evaluated and correlated to the microstructural features of weld region. The fractured sections of tensile and impact toughness specimens of joints were analyzed using SEM and the failure of joints was correlated with the hardness survey. Results showed that the LFW-Ti6Al4V alloy joints developed using the optimized parameters exhibited a tensile strength (TS) of 1015MPa, a yield strength (YS) of 940MPa, and an elongation (EL) of 8. The joints revealed 98.54, 95.91, and 66.67 of tensile strength, yield strength, and ductility of the parent metal. The LFW joints disclosed impact toughness (IT) of 17.2J which is 89.77 impact toughness of the parent metal. The superior tensile properties and impact toughness of LFW-Ti6Al4V alloy joints are mainly attributed to a greater degree of refinement of α+β grains in the weld interface, which offers greater resistance to tensile deformation and crack propagation.
- 1 August 2022
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 64 (8) , 1223-1233
Nugget formation, microstructural features and strength of resistance spot welded cold-rolled dual-phase steel lap joints for automotive applications
The main objective of this research paper is to investigate the nugget formation, microstructure and strength performance of DP 800 steel joints developed using resistance spot welding (RSW) process for automotive application. The influence of RSW parameters on nugget formation was studied using one variable at a time approach. The RSW joint showing optimum nugget area was further characterized for microstructural features and strength performance. The microstructural features of nugget were studied using optical and scanning electron microscopy (SEM). The lap tensile shear fractured specimens were analyzed using SEM for optimized condition. The microstructural features were correlated to the tensile shear strength and hardness of RSW joints. Results showed that welding current significantly influences the nugget formation than electrode force and welding time. The DP 800 RSW joints made using a welding current of 5.5 kA, an electrode pressure of 4.0 MPa and a welding time of 2.0 s disclosed defect free weld nugget of 7.28 mm diameter. It showed a higher tensile shear strength of 20 kN and microhardness of 564 HV thereby satisfying the requirement of automotive applications.
- 1 August 2022
- Published by Walter de Gruyter GmbH in Materials Testing
- Vol. 64 (8) , 1223-1233
Nugget formation, microstructural features and strength of resistance spot welded cold-rolled dual-phase steel lap joints for automotive applications
The main objective of this research paper is to investigate the nugget formation, microstructure and strength performance of DP 800 steel joints developed using resistance spot welding (RSW) process for automotive application. The influence of RSW parameters on nugget formation was studied using one variable at a time approach. The RSW joint showing optimum nugget area was further characterized for microstructural features and strength performance. The microstructural features of nugget were studied using optical and scanning electron microscopy (SEM). The lap tensile shear fractured specimens were analyzed using SEM for optimized condition. The microstructural features were correlated to the tensile shear strength and hardness of RSW joints. Results showed that welding current significantly influences the nugget formation than electrode force and welding time. The DP 800 RSW joints made using a welding current of 5.5 kA, an electrode pressure of 4.0 MPa and a welding time of 2.0 s disclosed defect free weld nugget of 7.28 mm diameter. It showed a higher tensile shear strength of 20 kN and microhardness of 564 HV thereby satisfying the requirement of automotive applications.