Harun Koçak
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Harun Koçak has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Çetin Karataş
Gazi Üniversitesi
3 shared publications - Asghar Safarian
Islamic Azad University
2 shared publications - Mehmet Subasi
Department of Machinery and Metal Technologies, Technical Sciences Vocational School, Gazi University, Ostim, Ankara 06374, Türkiye
2 shared publications Çetin Karataş
Gazi University
2 shared publications- Abdullah Onur Özdemi̇r
Gazi Üniversitesi, Teknoloji Fakültesi
1 shared publication Erkutay Taşdemirci
1 shared publication
Latest Publications
- 10 March 2026
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 58 (4) , 828-844
Taguchi and ANOVA-based analysis of injection parameters affecting automotive reflector surface and optical efficiency
In this study, the effect of injection parameters on sink marks and photometric properties in the production of reflector used in automobiles was investigated. Mold filling analysis was performed with Moldflow software and sinkmarks and warpage were determined before production. Afterwards, the reflector was produced. The effects of injection parameters such as melt temperature, mold temperature, injection speed, injection pressure, holding time and cooling time on sink marks and photometry were investigated by Taguchi and Anova analysis. In the mold filling simulation, a sink mark of 0.05 mm was formed, while an average of 0.053 mm of sink mark was formed in the experimental results. It was found that the most effective parameter on the sink mark was melt temperature, while cooling time was found for photometry. In the experiment, the lowest sink marks value was 0.053 mm in avarage, and the highest photometry value (923.33 mcd/lux) was measured in the same test. The lowest photometry value was measured as 700.33 mcd/lux and the sink marks value in this experiment was 0.082 mm. The sink marks on the reflector surface change the illumination angles by disrupting the surface planarity, and the reflector’s reflective properties are also affected by this.
- 10 March 2026
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 58 (4) , 828-844
Taguchi and ANOVA-based analysis of injection parameters affecting automotive reflector surface and optical efficiency
In this study, the effect of injection parameters on sink marks and photometric properties in the production of reflector used in automobiles was investigated. Mold filling analysis was performed with Moldflow software and sinkmarks and warpage were determined before production. Afterwards, the reflector was produced. The effects of injection parameters such as melt temperature, mold temperature, injection speed, injection pressure, holding time and cooling time on sink marks and photometry were investigated by Taguchi and Anova analysis. In the mold filling simulation, a sink mark of 0.05 mm was formed, while an average of 0.053 mm of sink mark was formed in the experimental results. It was found that the most effective parameter on the sink mark was melt temperature, while cooling time was found for photometry. In the experiment, the lowest sink marks value was 0.053 mm in avarage, and the highest photometry value (923.33 mcd/lux) was measured in the same test. The lowest photometry value was measured as 700.33 mcd/lux and the sink marks value in this experiment was 0.082 mm. The sink marks on the reflector surface change the illumination angles by disrupting the surface planarity, and the reflector’s reflective properties are also affected by this.
- Open Access
- 1 December 2023
- Published by Gazi University Journal of Science in Gazi University Journal of Science
- Vol. 36 (4) , 1722-1731
Investigation of Sinterability of WC-Co Component Comprising of AISI 4340 Steel Inserts
In this study, sinterability of WC-9% Co component with AISI 4340 steel insert was investigated using Inserted Powder Injection Molding (IPIM) method. Sintering experiments were performed at temperatures of 1200 °C to 1350 °C with dwell times of 120, 240, 360 min. Defects such as gaps, cracks and macro-porosities were observed in specimens, sintered at temperatures of 1200 °C and 1250 °C for all dwell times. It was proved that sintering temperature of 1350 °C was as high as it caused insert to get deformed and melted. As a result, the optimum sintering temperature and dwell time were determined to be 1300 °C and 240 min, respectively, at which the highest hardness, compression strength, and sintered density were obtained without any defects such as cracks or gaps.
- 1 December 2023
- Published by Gazi University Journal of Science in Gazi University Journal of Science
- Vol. 36 (4) , 1722-1731
Open AccessInvestigation of Sinterability of WC-Co Component Comprising of AISI 4340 Steel Inserts
In this study, sinterability of WC-9% Co component with AISI 4340 steel insert was investigated using Inserted Powder Injection Molding (IPIM) method. Sintering experiments were performed at temperatures of 1200 °C to 1350 °C with dwell times of 120, 240, 360 min. Defects such as gaps, cracks and macro-porosities were observed in specimens, sintered at temperatures of 1200 °C and 1250 °C for all dwell times. It was proved that sintering temperature of 1350 °C was as high as it caused insert to get deformed and melted. As a result, the optimum sintering temperature and dwell time were determined to be 1300 °C and 240 min, respectively, at which the highest hardness, compression strength, and sintered density were obtained without any defects such as cracks or gaps.
- 17 May 2022
- Published by SAGE Publications in Journal of Thermoplastic Composite Materials
- Vol. 36 (5) , 2154-2168
Investigation of earing defect and thickness distribution in stamp forming of continuous glass fiber reinforced polypropylene composite laminates
When lightweighting studies are examined, thermoplastic matrix composites come to the fore as they have a high specific strength, are recyclable, and can be formed by thermoforming. Some obscurity needs to be overcome for the rapid forming of three-dimensional parts from laminated thermoplastic composites. In this study, deep drawing experiments were carried out to investigate the forming capabilities of continuous glass fiber reinforced polypropylene composite laminates. The parameters of drawing depth, laminate temperature, holding pressure, and punch speed were examined at each three different levels. The effects of these parameters were evaluated on the earing defect and the thickness distribution. It was concluded that the laminate temperature affected both deformations the most. It was determined that all parameters caused a change in flange diameter, but the amount of earing increased with the increase of drawing depth. It was established that inhomogeneous thickness distributions occurred in the part and the highest thickening took place in the curve region.
- 17 May 2022
- Published by SAGE Publications in Journal of Thermoplastic Composite Materials
- Vol. 36 (5) , 2154-2168
Investigation of earing defect and thickness distribution in stamp forming of continuous glass fiber reinforced polypropylene composite laminates
When lightweighting studies are examined, thermoplastic matrix composites come to the fore as they have a high specific strength, are recyclable, and can be formed by thermoforming. Some obscurity needs to be overcome for the rapid forming of three-dimensional parts from laminated thermoplastic composites. In this study, deep drawing experiments were carried out to investigate the forming capabilities of continuous glass fiber reinforced polypropylene composite laminates. The parameters of drawing depth, laminate temperature, holding pressure, and punch speed were examined at each three different levels. The effects of these parameters were evaluated on the earing defect and the thickness distribution. It was concluded that the laminate temperature affected both deformations the most. It was determined that all parameters caused a change in flange diameter, but the amount of earing increased with the increase of drawing depth. It was established that inhomogeneous thickness distributions occurred in the part and the highest thickening took place in the curve region.
- 31 December 2020
- Published by Cukurova Universitesi Muhendislik-Mimarlik Fakultesi Dergisi in Çukurova Üniversitesi Mühendislik-Mimarlık Fakültesi Dergisi
- Vol. 35 (4) , 1001-1008
Ç2842, MS58 ve Al 6013 Malzemelerin Elektolitik Ni Kaplanmasında Kaplama Kalınlığı ve Yüzeysel Özelliklerin İncelenmesi
Bu çalışmada elektolitik Ni kaplanmada Ç2842, MS58 ve Al 6013 malzemelerin etkisi ve kaplama sonrası yüzey pürüzlülüğünün değişimi incelenmiştir. Deneylerde Ç2842 çelik, MS58 pirinç ve Al 6013 alüminyum alaşımı malzemeler Ni ile kaplanmıştır. Bu malzemeler, torna tezgahında farklı ilerleme oranlarında (0,065-0,13 mm/dev) işlenerek numuneler üzerinde farklı yüzey pürüzlülükleri elde edilmiştir. Daha sonra numuneler üzerine Ni kaplanmıştır. Kaplama işlemi sonrasında kaplama kalınlığı ve kaplama sonrası yüzey pürüzlülüğü ölçülmüş görüntülü incelmeler yapılarak kaplama kalitesi incelenmiştir. Deneyler sonucunda, diğer malzemelere göre MS 58 malzeme üzerinde daha kalın Ni tabakası (43 µm) elde edilmiştir. Kaplanan malzemenin elektriksel iletkenliğinin yüksek olması kaplama hızını arttırmaktadır. Ancak iletkenlik değerinin düşük olması kaplama yüzeyinin kalitesini iyileştirmektedir. Çelik malzemenin kaplama sayesinde yüzey pürüzlülüğü değeri %33-57 aralığında azalmıştır. Al 6013 malzemede, kaplama sonrası yüzey pürüzlülüğü %94-107 oranında artmakla beraber çukur şeklinde yüzeysel hatalar ortaya çıkmaktadır.
- 31 December 2020
- Published by Cukurova Universitesi Muhendislik-Mimarlik Fakultesi Dergisi in Çukurova Üniversitesi Mühendislik-Mimarlık Fakültesi Dergisi
- Vol. 35 (4) , 1001-1008
Ç2842, MS58 ve Al 6013 Malzemelerin Elektolitik Ni Kaplanmasında Kaplama Kalınlığı ve Yüzeysel Özelliklerin İncelenmesi
Bu çalışmada elektolitik Ni kaplanmada Ç2842, MS58 ve Al 6013 malzemelerin etkisi ve kaplama sonrası yüzey pürüzlülüğünün değişimi incelenmiştir. Deneylerde Ç2842 çelik, MS58 pirinç ve Al 6013 alüminyum alaşımı malzemeler Ni ile kaplanmıştır. Bu malzemeler, torna tezgahında farklı ilerleme oranlarında (0,065-0,13 mm/dev) işlenerek numuneler üzerinde farklı yüzey pürüzlülükleri elde edilmiştir. Daha sonra numuneler üzerine Ni kaplanmıştır. Kaplama işlemi sonrasında kaplama kalınlığı ve kaplama sonrası yüzey pürüzlülüğü ölçülmüş görüntülü incelmeler yapılarak kaplama kalitesi incelenmiştir. Deneyler sonucunda, diğer malzemelere göre MS 58 malzeme üzerinde daha kalın Ni tabakası (43 µm) elde edilmiştir. Kaplanan malzemenin elektriksel iletkenliğinin yüksek olması kaplama hızını arttırmaktadır. Ancak iletkenlik değerinin düşük olması kaplama yüzeyinin kalitesini iyileştirmektedir. Çelik malzemenin kaplama sayesinde yüzey pürüzlülüğü değeri %33-57 aralığında azalmıştır. Al 6013 malzemede, kaplama sonrası yüzey pürüzlülüğü %94-107 oranında artmakla beraber çukur şeklinde yüzeysel hatalar ortaya çıkmaktadır.
- 29 December 2020
- Published by Gazi Universitesi Fen Bilimleri Dergisi Part C: Tasarim ve Teknoloji in Gazi Üniversitesi Fen Bilimleri Dergisi Part C: Tasarım ve Teknoloji
- Vol. 8 (4) , 972-980
Al 6013 ve MS 58 malzemelere delik içi ezerek parlatma işlemi uygulanmasıyla yüzeysel özelliklerin iyileştirilmesi
Bu çalışmada, Al 6013 ve MS 58 malzemelere delinen deliklerin ezerek parlatma işlemleri araştırılmıştır. Testlerde her iki malzeme için üç farklı ezme payı bırakılarak işlem yapılmıştır. Ezerek parlatma işleminin ardından numuneler, yüzey pürüzlülüğü, mikro setlik ve mikro yapı bakımından incelenmiştir. İşlem sonrasında Al 6013 malzemenin yüzey pürüzlülüğü % 91,5 ve MS 58 malzemenin yüzey pürüzlülüğü % 89,6 oranında azaldığı belirlenmiştir. Testlerde, elde edilen en iyi yüzey pürüzlülüğü değeri Al 6013 malzemede 0,12 µm olduğu belirlenmiştir. MS 58 malzemenin ezilmiş bölgesinde plastik deformasyonla birlikte % 20 sertlik artışı sağlanmıştır. Tane yapısı ve sertlik artışı birlikte düşünüldüğünde MS 58 malzemenin küçük tane yapısına sahip olmasından dolayı bu malzemenin yüzey sertliğinde daha fazla artış meydana geldiği belirlenmiştir.
- 29 December 2020
- Published by Gazi Universitesi Fen Bilimleri Dergisi Part C: Tasarim ve Teknoloji in Gazi Üniversitesi Fen Bilimleri Dergisi Part C: Tasarım ve Teknoloji
- Vol. 8 (4) , 972-980
Al 6013 ve MS 58 malzemelere delik içi ezerek parlatma işlemi uygulanmasıyla yüzeysel özelliklerin iyileştirilmesi
Bu çalışmada, Al 6013 ve MS 58 malzemelere delinen deliklerin ezerek parlatma işlemleri araştırılmıştır. Testlerde her iki malzeme için üç farklı ezme payı bırakılarak işlem yapılmıştır. Ezerek parlatma işleminin ardından numuneler, yüzey pürüzlülüğü, mikro setlik ve mikro yapı bakımından incelenmiştir. İşlem sonrasında Al 6013 malzemenin yüzey pürüzlülüğü % 91,5 ve MS 58 malzemenin yüzey pürüzlülüğü % 89,6 oranında azaldığı belirlenmiştir. Testlerde, elde edilen en iyi yüzey pürüzlülüğü değeri Al 6013 malzemede 0,12 µm olduğu belirlenmiştir. MS 58 malzemenin ezilmiş bölgesinde plastik deformasyonla birlikte % 20 sertlik artışı sağlanmıştır. Tane yapısı ve sertlik artışı birlikte düşünüldüğünde MS 58 malzemenin küçük tane yapısına sahip olmasından dolayı bu malzemenin yüzey sertliğinde daha fazla artış meydana geldiği belirlenmiştir.
- 26 December 2019
- Published by SAGE Publications in Materials Science and Technology
- Vol. 36 (3) , 293-298
Investigation of functional core-rim composite part production by inserted powder injection moulding
In this study, the use of Cu and Ni interlayers have been investigated for functional core-rim composite part production with WC-Co 9 wt-% feedstock/steel. For this purpose, different experiments have been performed and joining condition, shear strength and microstructure of the intermediate region have been examined. It has been found that AISI 4340 insert/WC-Co have been joined and 85.8 MPa shear strength achieved, but high speed steel insert has not joined. Moreover, it has been determined that better results are obtained with Ni interlayer. Under the same conditions, when the 40 µm Ni interlayer has been used between AISI 4340 core and WC-Co rim, shear strength has been increased approximately twice and has been 162.7 MPa.
- 26 December 2019
- Published by SAGE Publications in Materials Science and Technology
- Vol. 36 (3) , 293-298
Investigation of functional core-rim composite part production by inserted powder injection moulding
In this study, the use of Cu and Ni interlayers have been investigated for functional core-rim composite part production with WC-Co 9 wt-% feedstock/steel. For this purpose, different experiments have been performed and joining condition, shear strength and microstructure of the intermediate region have been examined. It has been found that AISI 4340 insert/WC-Co have been joined and 85.8 MPa shear strength achieved, but high speed steel insert has not joined. Moreover, it has been determined that better results are obtained with Ni interlayer. Under the same conditions, when the 40 µm Ni interlayer has been used between AISI 4340 core and WC-Co rim, shear strength has been increased approximately twice and has been 162.7 MPa.