Si Young Chang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Si Young Chang has a total of 58 co-authors. Here are the top co-authors by number of shared publications:
- Poong-Yeon Kim
Nanomaterials Research Center, Korea Institute of Materials Science KIMS, Changwon 51508, Republic of Korea
3 shared publications - Donhee Lee
Department of Material Science and Engineering Korea Aerospace University 10540 Goyang Republic of Korea
2 shared publications - Du Hong Kang
Department of Material Science and Engineering Korea Aerospace University 10540 Goyang Republic of Korea
2 shared publications Hee-Kwon Lee
Changwon Natl Univ, Dept Met & Mat Engn, Chang Won 51140, South Korea
2 shared publications- Hoseong Rhee
Korea Aerospace University, Department of Materials Science and Engineering, Goyang, Korea
2 shared publications - Hyunseung Lee
Korea Aerospace University, Department of Materials Science and Engineering, Goyang, Korea
2 shared publications
Latest Publications
- Open Access
- 22 June 2026
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 71 (2) , 601-604
Effect of Surface Roughness on the Sheet Resistance of CP Titanium Foils
In this study, we investigated the effect of physical surface roughness on the sheet resistance (Rs) of commercially pure titanium (CP-Ti, Grades 1, 2, and 4) foils with varying impurity compositions. Microstructural observations revealed that the grain sizes of Grades 1 and 2 were 24 and 20 μm, respectively, whereas Grade 4 exhibited a very fine microstructure with indistinct grain boundaries. The surface roughness of the as-received CP-Ti foils was approximately 0.05–0.06 μm, showing no significant difference among the grades. However, the sheet resistance was determined to be 4.05, 4.60, and 4.82 mΩ/□, respectively, indicating an increase with higher impurity content. In contrast, when the surface roughness was mechanically controlled, the sheet resistance of all specimens increased with increasing surface roughness for all grades, confirming a linear correlation between surface roughness and sheet resistance.
- 22 June 2026
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 71 (2) , 601-604
Open AccessEffect of Surface Roughness on the Sheet Resistance of CP Titanium Foils
In this study, we investigated the effect of physical surface roughness on the sheet resistance (Rs) of commercially pure titanium (CP-Ti, Grades 1, 2, and 4) foils with varying impurity compositions. Microstructural observations revealed that the grain sizes of Grades 1 and 2 were 24 and 20 μm, respectively, whereas Grade 4 exhibited a very fine microstructure with indistinct grain boundaries. The surface roughness of the as-received CP-Ti foils was approximately 0.05–0.06 μm, showing no significant difference among the grades. However, the sheet resistance was determined to be 4.05, 4.60, and 4.82 mΩ/□, respectively, indicating an increase with higher impurity content. In contrast, when the surface roughness was mechanically controlled, the sheet resistance of all specimens increased with increasing surface roughness for all grades, confirming a linear correlation between surface roughness and sheet resistance.
- Open Access
- 27 May 2026
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 36 (5) , 161-166
Dependence on Surface Roughness of Electrical and Electrochemical Properties of Non-Porous and Porous Titanium Sheets
- 27 May 2026
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 36 (5) , 161-166
Open AccessDependence on Surface Roughness of Electrical and Electrochemical Properties of Non-Porous and Porous Titanium Sheets
- Open Access
- 31 October 2025
- Published by The Korean Powder Metallurgy & Materials Institute in Journal of Powder Materials
- Vol. 32 (5) , 383-389
Preparation of Flake-shape Cobalt Powders by High-Energy Ball Milling for rSOC Current Collectors
Reversible solid oxide cells (rSOCs), which enable two-way conversion between electricity and hydrogen, have gained attention with the rise of hydrogen energy. However, foam-type current collectors in rSOC stacks exhibit poor structural controllability and limited electrode contact area. To address these limitations, this study aimed to convert spherical cobalt powders into flake-type morphology via high-energy ball milling, as a preliminary step toward fabricating flake-based current collectors.Milling parameters—specifically, the ball-to-powder ratio (BPR), milling time, and process control agent (PCA) content—were varied. At an 8:1 BPR, over 90% of the powder became flake-shaped after 8 hours, while extended milling caused cold welding. In contrast, a 10:1 BPR resulted in dominant fragmentation. The Burgio–Rojac model quantified energy input and defined the optimal range for flake formation. Increasing the PCA to 4 wt% delayed flake formation to 16 hours and induced cold welding, as shown by bimodal particle size distributions. These results support the development of Co-based current collectors for use in rSOCs.
- 31 October 2025
- Published by The Korean Powder Metallurgy & Materials Institute in Journal of Powder Materials
- Vol. 32 (5) , 383-389
Open AccessPreparation of Flake-shape Cobalt Powders by High-Energy Ball Milling for rSOC Current Collectors
Reversible solid oxide cells (rSOCs), which enable two-way conversion between electricity and hydrogen, have gained attention with the rise of hydrogen energy. However, foam-type current collectors in rSOC stacks exhibit poor structural controllability and limited electrode contact area. To address these limitations, this study aimed to convert spherical cobalt powders into flake-type morphology via high-energy ball milling, as a preliminary step toward fabricating flake-based current collectors.Milling parameters—specifically, the ball-to-powder ratio (BPR), milling time, and process control agent (PCA) content—were varied. At an 8:1 BPR, over 90% of the powder became flake-shaped after 8 hours, while extended milling caused cold welding. In contrast, a 10:1 BPR resulted in dominant fragmentation. The Burgio–Rojac model quantified energy input and defined the optimal range for flake formation. Increasing the PCA to 4 wt% delayed flake formation to 16 hours and induced cold welding, as shown by bimodal particle size distributions. These results support the development of Co-based current collectors for use in rSOCs.
- Open Access
- 27 October 2025
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 35 (10) , 473-478
Effect of Cl2 Gas Exposure on the Surface Properties of Electropolished STS316L
In this study, the surface characteristics-including roughness, oxide layer thickness, and composition-of the electropolished layer on STS316L steel tubes subjected to double melting via the VIM/VAR process were investigated after exposure to Cl 2 gas. The tubes were exposed to Cl 2 gas for 1 to 13 d to simulate semiconductor conditions. Surface roughness increased with Cl 2 exposure time, showing values of 0.01, 0.04, 0.04 and 0.03 µm after 0, 1, 5 and 9 d, respectively. At the same time, the oxide layer thickness on EPed STS316L, which was initially 8.2 nm, decreased to 3.18, 2.58 after 1, 5 d of Cl 2 exposure, approaching the initial thickness of 2.38 nm observed on non-EPed STS316L. After 9 d, the thickness further decreased to 0.51 nm, with no significant change was observed thereafter. Before Cl 2 exposure, the CrO/FeO ratio was 2.26. After 1, 5, and 9 d of exposure, the ratio decreased to 2.06, 1.75, and 1.27, respectively. In addition, the penetration depth of Cl into the oxide layer increased with longer exposure time. These results suggest that the formation of chromium chlorides led to the breakdown of the stable Cr 2 O 3 layer.
- 27 October 2025
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 35 (10) , 473-478
Open AccessEffect of Cl2 Gas Exposure on the Surface Properties of Electropolished STS316L
In this study, the surface characteristics-including roughness, oxide layer thickness, and composition-of the electropolished layer on STS316L steel tubes subjected to double melting via the VIM/VAR process were investigated after exposure to Cl 2 gas. The tubes were exposed to Cl 2 gas for 1 to 13 d to simulate semiconductor conditions. Surface roughness increased with Cl 2 exposure time, showing values of 0.01, 0.04, 0.04 and 0.03 µm after 0, 1, 5 and 9 d, respectively. At the same time, the oxide layer thickness on EPed STS316L, which was initially 8.2 nm, decreased to 3.18, 2.58 after 1, 5 d of Cl 2 exposure, approaching the initial thickness of 2.38 nm observed on non-EPed STS316L. After 9 d, the thickness further decreased to 0.51 nm, with no significant change was observed thereafter. Before Cl 2 exposure, the CrO/FeO ratio was 2.26. After 1, 5, and 9 d of exposure, the ratio decreased to 2.06, 1.75, and 1.27, respectively. In addition, the penetration depth of Cl into the oxide layer increased with longer exposure time. These results suggest that the formation of chromium chlorides led to the breakdown of the stable Cr 2 O 3 layer.
- 30 September 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 1165-1168
Surface Properties of Electrolytic Polished Layer on STS316L by Single Melting and Double Melting
In this study, STS316L produced by a single-melting vacuum oxygen decarburization (VOD) process, referred to as SM, and a double-melting process involving vacuum induction melting (VIM) and vacuum arc remelting (VAR), referred to as DM, was subjected to extrusion and drawing to form a tube, followed by electrolytic polishing (EP). The surface roughness of layer on the DMed sample is 0.02 μm, which is much lower than that on the SMed sample of 0.13 μm. The thickness of the EP layer on STS316L by SM and DM revealed the values of approximately 7.1 nm and 8.2 nm, respectively. The Cr/Fe and CrO/FeO ratios in the EP layer on the DMed sample were 1.62 and 2.26, respectively, while, in the SMed sample, 1.22 and 2.03. Consequently, the EPed STS316L by DM showed better corrosion resistance in HCl solution and small amounts of Cr and Fe eluted in HCl solutions.
- 30 September 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 1165-1168
Surface Properties of Electrolytic Polished Layer on STS316L by Single Melting and Double Melting
In this study, STS316L produced by a single-melting vacuum oxygen decarburization (VOD) process, referred to as SM, and a double-melting process involving vacuum induction melting (VIM) and vacuum arc remelting (VAR), referred to as DM, was subjected to extrusion and drawing to form a tube, followed by electrolytic polishing (EP). The surface roughness of layer on the DMed sample is 0.02 μm, which is much lower than that on the SMed sample of 0.13 μm. The thickness of the EP layer on STS316L by SM and DM revealed the values of approximately 7.1 nm and 8.2 nm, respectively. The Cr/Fe and CrO/FeO ratios in the EP layer on the DMed sample were 1.62 and 2.26, respectively, while, in the SMed sample, 1.22 and 2.03. Consequently, the EPed STS316L by DM showed better corrosion resistance in HCl solution and small amounts of Cr and Fe eluted in HCl solutions.
- Open Access
- 15 March 2025
- Published by Japan Society of Powder and Powder Metallurgy in Journal of the Japan Society of Powder and Powder Metallurgy
- Vol. 72 (Supplement) , S787-S790
Effect of High Temperature on Microstructure and Hardness of Ti-6Al-4Dy Alloy by High Energy Ball Milling and Spark Plasma Sintering
- 15 March 2025
- Published by Japan Society of Powder and Powder Metallurgy in Journal of the Japan Society of Powder and Powder Metallurgy
- Vol. 72 (Supplement) , S787-S790
Open AccessEffect of High Temperature on Microstructure and Hardness of Ti-6Al-4Dy Alloy by High Energy Ball Milling and Spark Plasma Sintering
- 21 June 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (2) , 475-478
Enhancing Microstructural Characteristics and Mechanical Properties of Ti-Al-Dy Alloy through Ball Milling and SPS Consolidation
In this study, pure Ti, Al, Dy powders were ball-milled with zirconia balls in argon atmosphere for 3 h at 800 rpm, producing a Ti- 6 wt.% Al- 4 wt.% Dy alloy powder. The alloy powder was consolidated by SPS technique at 1373 K for 15 min under 50 MPa pressure in vacuum. The sintered body had approximately 99% in density and 6 μm in grain size. XRD and TEM revealed the presence of the second phases such as Ti3Al, Al3Dy and Ti4Al20Dy phases, and their sizes were approximately 50 nm. Microhardness was approximately 960 Hv at room temperature, which decreased as temperature increased. However, there remained the micro-hardness significantly higher compared to the commercial Ti-6Al-4V alloy. After hardness test at 1173 K, XRD analysis did not show any difference in peaks, while the grain size and second phases size increased by ~4 μm and ~2 nm, respectively.
- 21 June 2024
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 69 (2) , 475-478
Enhancing Microstructural Characteristics and Mechanical Properties of Ti-Al-Dy Alloy through Ball Milling and SPS Consolidation
In this study, pure Ti, Al, Dy powders were ball-milled with zirconia balls in argon atmosphere for 3 h at 800 rpm, producing a Ti- 6 wt.% Al- 4 wt.% Dy alloy powder. The alloy powder was consolidated by SPS technique at 1373 K for 15 min under 50 MPa pressure in vacuum. The sintered body had approximately 99% in density and 6 μm in grain size. XRD and TEM revealed the presence of the second phases such as Ti3Al, Al3Dy and Ti4Al20Dy phases, and their sizes were approximately 50 nm. Microhardness was approximately 960 Hv at room temperature, which decreased as temperature increased. However, there remained the micro-hardness significantly higher compared to the commercial Ti-6Al-4V alloy. After hardness test at 1173 K, XRD analysis did not show any difference in peaks, while the grain size and second phases size increased by ~4 μm and ~2 nm, respectively.
- 6 March 2023
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 68 (1) , 81-84
Effect of Ball on SPS Characteristics of Ti-Al-Nd Powders Prepared by High Energy Ball Milling
The effects of different types of balls on spark plasma sintering (SPS) characteristics of high energy ball milled Ti-48wt% Al-4wt% Nd powders were investigated. After ball milling with STS balls and zirconia balls at 800 rpm for 3 h in argon atmosphere, both powders showed shape factors of about 0.8, but their average powder sizes differed respectively at approximately 11 µm and 5 µm. From XRD results, only the peaks of pure Ti, Al and Nd were detected in both powders. The obtained Ti-Al-Nd powders were consolidated by SPS technique at 1373 K for 15 min under a pressure of 50 MPa in vacuum, resulting in high density over 99%. EDS and XRD analyses indicated the formation of binary phases such as TiAl3, TiAl, Ti3Al5, and NdAl3 after SPS in both cases of STS and zirconia balls, while the ternary Ti-Al-Nd phase was detected only in the case of zirconia balls. The size of second phases was slightly smaller in the case of zirconia balls. The microhardness of the sample was 790 Hv with zirconia balls and 540 Hv with STS balls.
- 6 March 2023
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 68 (1) , 81-84
Effect of Ball on SPS Characteristics of Ti-Al-Nd Powders Prepared by High Energy Ball Milling
The effects of different types of balls on spark plasma sintering (SPS) characteristics of high energy ball milled Ti-48wt% Al-4wt% Nd powders were investigated. After ball milling with STS balls and zirconia balls at 800 rpm for 3 h in argon atmosphere, both powders showed shape factors of about 0.8, but their average powder sizes differed respectively at approximately 11 µm and 5 µm. From XRD results, only the peaks of pure Ti, Al and Nd were detected in both powders. The obtained Ti-Al-Nd powders were consolidated by SPS technique at 1373 K for 15 min under a pressure of 50 MPa in vacuum, resulting in high density over 99%. EDS and XRD analyses indicated the formation of binary phases such as TiAl3, TiAl, Ti3Al5, and NdAl3 after SPS in both cases of STS and zirconia balls, while the ternary Ti-Al-Nd phase was detected only in the case of zirconia balls. The size of second phases was slightly smaller in the case of zirconia balls. The microhardness of the sample was 790 Hv with zirconia balls and 540 Hv with STS balls.
- 6 September 2021
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 66 (3) , 789-793
Microstructural Characteristics of Ti-Al-Dy Alloy Produced by High Energy Ball Milling
In this study, the alloying of Ti, Al and Dy powders by high energy ball milling, and the spark plasma sintering (SPS) characteristics of as milled powders have been investigated based on the observation of microstructure. Pure Ti, 6wt% Al and 4wt% Dy powders were mixed and milled with zirconia balls at 600 ~ 1000 rpm for 3h in an Ar gas. The initial sizes of Ti, Al and Dy powders were approximately 20, 40, and 200 μm, respectively. With increasing the milling speed from 600 to 1000 rpm, the size of mixing powders reduced from 120 to 15 μm. On the other hand, from XRD results of powders milled at higher speeds than 700rpm, the peaks of Ti3Al and AlDy phases were identified, indicating the successful alloying. Therefore, the powders milled at 800 rpm have been employed for the SPS under the applied pressure of 50 MPa at 1373K for 15 min. In the SPSed sample, the Al3Dy and two ternary Ti-Al-Dy phases were newly detected, while the peak of AlDy phase disappeared. The SPSed Ti-6Al-4Dy alloy revealed high relative density and micro-hardness of approximately 99% and 950Hv, respectively.
- 6 September 2021
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 66 (3) , 789-793
Microstructural Characteristics of Ti-Al-Dy Alloy Produced by High Energy Ball Milling
In this study, the alloying of Ti, Al and Dy powders by high energy ball milling, and the spark plasma sintering (SPS) characteristics of as milled powders have been investigated based on the observation of microstructure. Pure Ti, 6wt% Al and 4wt% Dy powders were mixed and milled with zirconia balls at 600 ~ 1000 rpm for 3h in an Ar gas. The initial sizes of Ti, Al and Dy powders were approximately 20, 40, and 200 μm, respectively. With increasing the milling speed from 600 to 1000 rpm, the size of mixing powders reduced from 120 to 15 μm. On the other hand, from XRD results of powders milled at higher speeds than 700rpm, the peaks of Ti3Al and AlDy phases were identified, indicating the successful alloying. Therefore, the powders milled at 800 rpm have been employed for the SPS under the applied pressure of 50 MPa at 1373K for 15 min. In the SPSed sample, the Al3Dy and two ternary Ti-Al-Dy phases were newly detected, while the peak of AlDy phase disappeared. The SPSed Ti-6Al-4Dy alloy revealed high relative density and micro-hardness of approximately 99% and 950Hv, respectively.
- Open Access
- 1 March 2020
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 30 (3) , 111-116
Effect of Casting Speed on Microstructure and Mechanical Properties of Al-Mg-Si/Al Hybrid Material by Duo-Casting
- 1 March 2020
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 30 (3) , 111-116
Open AccessEffect of Casting Speed on Microstructure and Mechanical Properties of Al-Mg-Si/Al Hybrid Material by Duo-Casting