DLDonhee Lee

Donhee Lee

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Donhee Lee has a total of 5 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Effect of Cl2 Gas Exposure on the Surface Properties of Electropolished STS316L

    by Donhee Lee, Du Hong Kang, Poongyeon Kim, Deokhyun Han, Man-Sik Kong, Si Young Chang

    In this study, the surface characteristics-including roughness, oxide layer thickness, and composition-of the electropolished layer on STS316L steel tubes subjected to double melting via the VIM/VAR process were investigated after exposure to Cl 2 gas. The tubes were exposed to Cl 2 gas for 1 to 13 d to simulate semiconductor conditions. Surface roughness increased with Cl 2 exposure time, showing values of 0.01, 0.04, 0.04 and 0.03 µm after 0, 1, 5 and 9 d, respectively. At the same time, the oxide layer thickness on EPed STS316L, which was initially 8.2 nm, decreased to 3.18, 2.58 after 1, 5 d of Cl 2 exposure, approaching the initial thickness of 2.38 nm observed on non-EPed STS316L. After 9 d, the thickness further decreased to 0.51 nm, with no significant change was observed thereafter. Before Cl 2 exposure, the CrO/FeO ratio was 2.26. After 1, 5, and 9 d of exposure, the ratio decreased to 2.06, 1.75, and 1.27, respectively. In addition, the penetration depth of Cl into the oxide layer increased with longer exposure time. These results suggest that the formation of chromium chlorides led to the breakdown of the stable Cr 2 O 3 layer.

  • Surface Properties of Electrolytic Polished Layer on STS316L by Single Melting and Double Melting

    by Donhee Lee, Du Hong Kang, Poongyeon Kim, Si Young Chang

    In this study, STS316L produced by a single-melting vacuum oxygen decarburization (VOD) process, referred to as SM, and a double-melting process involving vacuum induction melting (VIM) and vacuum arc remelting (VAR), referred to as DM, was subjected to extrusion and drawing to form a tube, followed by electrolytic polishing (EP). The surface roughness of layer on the DMed sample is 0.02 μm, which is much lower than that on the SMed sample of 0.13 μm. The thickness of the EP layer on STS316L by SM and DM revealed the values of approximately 7.1 nm and 8.2 nm, respectively. The Cr/Fe and CrO/FeO ratios in the EP layer on the DMed sample were 1.62 and 2.26, respectively, while, in the SMed sample, 1.22 and 2.03. Consequently, the EPed STS316L by DM showed better corrosion resistance in HCl solution and small amounts of Cr and Fe eluted in HCl solutions.