Poong-Yeon Kim
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Poong-Yeon Kim has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Si Young Chang
Korea Aerospace University, Department of Materials Science and Engineering, Goyang, Korea
3 shared publications - Donhee Lee
Department of Material Science and Engineering Korea Aerospace University 10540 Goyang Republic of Korea
2 shared publications - Du Hong Kang
Department of Material Science and Engineering Korea Aerospace University 10540 Goyang Republic of Korea
2 shared publications - Hyeon-Ju Kim
Nanomaterials Research Center, Korea Institute of Materials Science KIMS, Changwon 51508, Republic of Korea
2 shared publications - Jung-Yeul Yun
Nanomaterials Research Center, Korea Institute of Materials Science KIMS, Changwon 51508, Republic of Korea
2 shared publications - Min-Jeong Lee
Nanomaterials Research Center, Korea Institute of Materials Science KIMS, Changwon 51508, Republic of Korea
2 shared publications
Latest Publications
- Open Access
- 31 October 2025
- Published by The Korean Powder Metallurgy & Materials Institute in Journal of Powder Materials
- Vol. 32 (5) , 383-389
Preparation of Flake-shape Cobalt Powders by High-Energy Ball Milling for rSOC Current Collectors
Reversible solid oxide cells (rSOCs), which enable two-way conversion between electricity and hydrogen, have gained attention with the rise of hydrogen energy. However, foam-type current collectors in rSOC stacks exhibit poor structural controllability and limited electrode contact area. To address these limitations, this study aimed to convert spherical cobalt powders into flake-type morphology via high-energy ball milling, as a preliminary step toward fabricating flake-based current collectors.Milling parameters—specifically, the ball-to-powder ratio (BPR), milling time, and process control agent (PCA) content—were varied. At an 8:1 BPR, over 90% of the powder became flake-shaped after 8 hours, while extended milling caused cold welding. In contrast, a 10:1 BPR resulted in dominant fragmentation. The Burgio–Rojac model quantified energy input and defined the optimal range for flake formation. Increasing the PCA to 4 wt% delayed flake formation to 16 hours and induced cold welding, as shown by bimodal particle size distributions. These results support the development of Co-based current collectors for use in rSOCs.
- 31 October 2025
- Published by The Korean Powder Metallurgy & Materials Institute in Journal of Powder Materials
- Vol. 32 (5) , 383-389
Open AccessPreparation of Flake-shape Cobalt Powders by High-Energy Ball Milling for rSOC Current Collectors
Reversible solid oxide cells (rSOCs), which enable two-way conversion between electricity and hydrogen, have gained attention with the rise of hydrogen energy. However, foam-type current collectors in rSOC stacks exhibit poor structural controllability and limited electrode contact area. To address these limitations, this study aimed to convert spherical cobalt powders into flake-type morphology via high-energy ball milling, as a preliminary step toward fabricating flake-based current collectors.Milling parameters—specifically, the ball-to-powder ratio (BPR), milling time, and process control agent (PCA) content—were varied. At an 8:1 BPR, over 90% of the powder became flake-shaped after 8 hours, while extended milling caused cold welding. In contrast, a 10:1 BPR resulted in dominant fragmentation. The Burgio–Rojac model quantified energy input and defined the optimal range for flake formation. Increasing the PCA to 4 wt% delayed flake formation to 16 hours and induced cold welding, as shown by bimodal particle size distributions. These results support the development of Co-based current collectors for use in rSOCs.
- Open Access
- 27 October 2025
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 35 (10) , 473-478
Effect of Cl2 Gas Exposure on the Surface Properties of Electropolished STS316L
In this study, the surface characteristics-including roughness, oxide layer thickness, and composition-of the electropolished layer on STS316L steel tubes subjected to double melting via the VIM/VAR process were investigated after exposure to Cl 2 gas. The tubes were exposed to Cl 2 gas for 1 to 13 d to simulate semiconductor conditions. Surface roughness increased with Cl 2 exposure time, showing values of 0.01, 0.04, 0.04 and 0.03 µm after 0, 1, 5 and 9 d, respectively. At the same time, the oxide layer thickness on EPed STS316L, which was initially 8.2 nm, decreased to 3.18, 2.58 after 1, 5 d of Cl 2 exposure, approaching the initial thickness of 2.38 nm observed on non-EPed STS316L. After 9 d, the thickness further decreased to 0.51 nm, with no significant change was observed thereafter. Before Cl 2 exposure, the CrO/FeO ratio was 2.26. After 1, 5, and 9 d of exposure, the ratio decreased to 2.06, 1.75, and 1.27, respectively. In addition, the penetration depth of Cl into the oxide layer increased with longer exposure time. These results suggest that the formation of chromium chlorides led to the breakdown of the stable Cr 2 O 3 layer.
- 27 October 2025
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 35 (10) , 473-478
Open AccessEffect of Cl2 Gas Exposure on the Surface Properties of Electropolished STS316L
In this study, the surface characteristics-including roughness, oxide layer thickness, and composition-of the electropolished layer on STS316L steel tubes subjected to double melting via the VIM/VAR process were investigated after exposure to Cl 2 gas. The tubes were exposed to Cl 2 gas for 1 to 13 d to simulate semiconductor conditions. Surface roughness increased with Cl 2 exposure time, showing values of 0.01, 0.04, 0.04 and 0.03 µm after 0, 1, 5 and 9 d, respectively. At the same time, the oxide layer thickness on EPed STS316L, which was initially 8.2 nm, decreased to 3.18, 2.58 after 1, 5 d of Cl 2 exposure, approaching the initial thickness of 2.38 nm observed on non-EPed STS316L. After 9 d, the thickness further decreased to 0.51 nm, with no significant change was observed thereafter. Before Cl 2 exposure, the CrO/FeO ratio was 2.26. After 1, 5, and 9 d of exposure, the ratio decreased to 2.06, 1.75, and 1.27, respectively. In addition, the penetration depth of Cl into the oxide layer increased with longer exposure time. These results suggest that the formation of chromium chlorides led to the breakdown of the stable Cr 2 O 3 layer.
- 30 September 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 1165-1168
Surface Properties of Electrolytic Polished Layer on STS316L by Single Melting and Double Melting
In this study, STS316L produced by a single-melting vacuum oxygen decarburization (VOD) process, referred to as SM, and a double-melting process involving vacuum induction melting (VIM) and vacuum arc remelting (VAR), referred to as DM, was subjected to extrusion and drawing to form a tube, followed by electrolytic polishing (EP). The surface roughness of layer on the DMed sample is 0.02 μm, which is much lower than that on the SMed sample of 0.13 μm. The thickness of the EP layer on STS316L by SM and DM revealed the values of approximately 7.1 nm and 8.2 nm, respectively. The Cr/Fe and CrO/FeO ratios in the EP layer on the DMed sample were 1.62 and 2.26, respectively, while, in the SMed sample, 1.22 and 2.03. Consequently, the EPed STS316L by DM showed better corrosion resistance in HCl solution and small amounts of Cr and Fe eluted in HCl solutions.
- 30 September 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 1165-1168
Surface Properties of Electrolytic Polished Layer on STS316L by Single Melting and Double Melting
In this study, STS316L produced by a single-melting vacuum oxygen decarburization (VOD) process, referred to as SM, and a double-melting process involving vacuum induction melting (VIM) and vacuum arc remelting (VAR), referred to as DM, was subjected to extrusion and drawing to form a tube, followed by electrolytic polishing (EP). The surface roughness of layer on the DMed sample is 0.02 μm, which is much lower than that on the SMed sample of 0.13 μm. The thickness of the EP layer on STS316L by SM and DM revealed the values of approximately 7.1 nm and 8.2 nm, respectively. The Cr/Fe and CrO/FeO ratios in the EP layer on the DMed sample were 1.62 and 2.26, respectively, while, in the SMed sample, 1.22 and 2.03. Consequently, the EPed STS316L by DM showed better corrosion resistance in HCl solution and small amounts of Cr and Fe eluted in HCl solutions.
- Open Access
- 31 August 2025
- Published by The Korean Powder Metallurgy & Materials Institute in Journal of Powder Materials
- Vol. 32 (4) , 299-308
Fabrication and Pore Characteristics of Metal Powder Filters with a Cross-Sealed Honeycomb Shape Using Material Extrusion Additive Manufacturing
The development of high-performance metal filters is essential for maintaining ultra-clean environments in semiconductor manufacturing. In this study, cross-sealed honeycomb filters were fabricated using STS316L powder via material extrusion additive manufacturing (MEAM) for semiconductor gas filtration. The effects of filter geometry (4 or 9 channels) and sintering temperature (850°C, 950°C, or 1,050°C) on performance were examined. First, 4-channel and 9-channel filters sintered at the same temperature (950°C) exhibited similar porosities of 50.08% and 50.57%, but the 9-channel filter showed a higher pressure-drop (0.26 bar) and better filtration-efficiency (3.55 LRV) than the 4-channel filter (0.19 bar and 3.25 LRV, respectively). Second, for filters with the same geometry (4-channel) increasing the sintering temperature reduced porosity from 64.52% to 40.33%, while the pressure-drop increased from 0.13 bar to 0.22 bar and filtration-efficiency improved from 2.53 LRV to 3.51 LRV. These findings demonstrate that filter geometry and sintering temperature are key factors governing the trade-off between air permeability, pressure-drop, and filtration efficiency. This work provides insights and data for optimizing MEAM-based high-performance metal powder filter design.
- 31 August 2025
- Published by The Korean Powder Metallurgy & Materials Institute in Journal of Powder Materials
- Vol. 32 (4) , 299-308
Open AccessFabrication and Pore Characteristics of Metal Powder Filters with a Cross-Sealed Honeycomb Shape Using Material Extrusion Additive Manufacturing
The development of high-performance metal filters is essential for maintaining ultra-clean environments in semiconductor manufacturing. In this study, cross-sealed honeycomb filters were fabricated using STS316L powder via material extrusion additive manufacturing (MEAM) for semiconductor gas filtration. The effects of filter geometry (4 or 9 channels) and sintering temperature (850°C, 950°C, or 1,050°C) on performance were examined. First, 4-channel and 9-channel filters sintered at the same temperature (950°C) exhibited similar porosities of 50.08% and 50.57%, but the 9-channel filter showed a higher pressure-drop (0.26 bar) and better filtration-efficiency (3.55 LRV) than the 4-channel filter (0.19 bar and 3.25 LRV, respectively). Second, for filters with the same geometry (4-channel) increasing the sintering temperature reduced porosity from 64.52% to 40.33%, while the pressure-drop increased from 0.13 bar to 0.22 bar and filtration-efficiency improved from 2.53 LRV to 3.51 LRV. These findings demonstrate that filter geometry and sintering temperature are key factors governing the trade-off between air permeability, pressure-drop, and filtration efficiency. This work provides insights and data for optimizing MEAM-based high-performance metal powder filter design.