Du Hong Kang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Du Hong Kang has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Donhee Lee
Department of Material Science and Engineering Korea Aerospace University 10540 Goyang Republic of Korea
2 shared publications - Poong-Yeon Kim
Nanomaterials Research Center, Korea Institute of Materials Science KIMS, Changwon 51508, Republic of Korea
2 shared publications - Si Young Chang
Korea Aerospace University, Department of Materials Science and Engineering, Goyang, Korea
2 shared publications - Deokhyun Han
Center for Advanced Materials and Processing Institute for Advanced Engineering 17180 Youngin Republic of Korea
1 shared publication - Man-Sik Kong
Center for Advanced Materials and Processing Institute for Advanced Engineering 17180 Youngin Republic of Korea
1 shared publication
Latest Publications
- Open Access
- 27 October 2025
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 35 (10) , 473-478
Effect of Cl2 Gas Exposure on the Surface Properties of Electropolished STS316L
In this study, the surface characteristics-including roughness, oxide layer thickness, and composition-of the electropolished layer on STS316L steel tubes subjected to double melting via the VIM/VAR process were investigated after exposure to Cl 2 gas. The tubes were exposed to Cl 2 gas for 1 to 13 d to simulate semiconductor conditions. Surface roughness increased with Cl 2 exposure time, showing values of 0.01, 0.04, 0.04 and 0.03 µm after 0, 1, 5 and 9 d, respectively. At the same time, the oxide layer thickness on EPed STS316L, which was initially 8.2 nm, decreased to 3.18, 2.58 after 1, 5 d of Cl 2 exposure, approaching the initial thickness of 2.38 nm observed on non-EPed STS316L. After 9 d, the thickness further decreased to 0.51 nm, with no significant change was observed thereafter. Before Cl 2 exposure, the CrO/FeO ratio was 2.26. After 1, 5, and 9 d of exposure, the ratio decreased to 2.06, 1.75, and 1.27, respectively. In addition, the penetration depth of Cl into the oxide layer increased with longer exposure time. These results suggest that the formation of chromium chlorides led to the breakdown of the stable Cr 2 O 3 layer.
- 27 October 2025
- Published by The Materials Research Society of Korea in Korean Journal of Materials Research
- Vol. 35 (10) , 473-478
Open AccessEffect of Cl2 Gas Exposure on the Surface Properties of Electropolished STS316L
In this study, the surface characteristics-including roughness, oxide layer thickness, and composition-of the electropolished layer on STS316L steel tubes subjected to double melting via the VIM/VAR process were investigated after exposure to Cl 2 gas. The tubes were exposed to Cl 2 gas for 1 to 13 d to simulate semiconductor conditions. Surface roughness increased with Cl 2 exposure time, showing values of 0.01, 0.04, 0.04 and 0.03 µm after 0, 1, 5 and 9 d, respectively. At the same time, the oxide layer thickness on EPed STS316L, which was initially 8.2 nm, decreased to 3.18, 2.58 after 1, 5 d of Cl 2 exposure, approaching the initial thickness of 2.38 nm observed on non-EPed STS316L. After 9 d, the thickness further decreased to 0.51 nm, with no significant change was observed thereafter. Before Cl 2 exposure, the CrO/FeO ratio was 2.26. After 1, 5, and 9 d of exposure, the ratio decreased to 2.06, 1.75, and 1.27, respectively. In addition, the penetration depth of Cl into the oxide layer increased with longer exposure time. These results suggest that the formation of chromium chlorides led to the breakdown of the stable Cr 2 O 3 layer.
- 30 September 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 1165-1168
Surface Properties of Electrolytic Polished Layer on STS316L by Single Melting and Double Melting
In this study, STS316L produced by a single-melting vacuum oxygen decarburization (VOD) process, referred to as SM, and a double-melting process involving vacuum induction melting (VIM) and vacuum arc remelting (VAR), referred to as DM, was subjected to extrusion and drawing to form a tube, followed by electrolytic polishing (EP). The surface roughness of layer on the DMed sample is 0.02 μm, which is much lower than that on the SMed sample of 0.13 μm. The thickness of the EP layer on STS316L by SM and DM revealed the values of approximately 7.1 nm and 8.2 nm, respectively. The Cr/Fe and CrO/FeO ratios in the EP layer on the DMed sample were 1.62 and 2.26, respectively, while, in the SMed sample, 1.22 and 2.03. Consequently, the EPed STS316L by DM showed better corrosion resistance in HCl solution and small amounts of Cr and Fe eluted in HCl solutions.
- 30 September 2025
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- p. 1165-1168
Surface Properties of Electrolytic Polished Layer on STS316L by Single Melting and Double Melting
In this study, STS316L produced by a single-melting vacuum oxygen decarburization (VOD) process, referred to as SM, and a double-melting process involving vacuum induction melting (VIM) and vacuum arc remelting (VAR), referred to as DM, was subjected to extrusion and drawing to form a tube, followed by electrolytic polishing (EP). The surface roughness of layer on the DMed sample is 0.02 μm, which is much lower than that on the SMed sample of 0.13 μm. The thickness of the EP layer on STS316L by SM and DM revealed the values of approximately 7.1 nm and 8.2 nm, respectively. The Cr/Fe and CrO/FeO ratios in the EP layer on the DMed sample were 1.62 and 2.26, respectively, while, in the SMed sample, 1.22 and 2.03. Consequently, the EPed STS316L by DM showed better corrosion resistance in HCl solution and small amounts of Cr and Fe eluted in HCl solutions.